Overview

Aluminium 7075 (3.4365, EN AW-7075 / AlZn5.5MgCu, UNS A97075) is a heat-treatable aluminium-zinc-magnesium-copper alloy and the standard high-strength aerospace aluminium, supplied to ASTM B209 and EN 485-2 for plate, ASTM B211 and EN 754-2 for bar, and to AMS 4123 for aerospace T651 bar. Its 5.1–6.1% zinc and 2.1–2.9% magnesium form dense MgZn2 precipitates during ageing, while 1.2–2.0% copper adds strength and 0.18–0.28% chromium controls grain structure and improves stress-corrosion behaviour. In the peak-aged T6 / T651 condition, bar reaches 530 MPa minimum tensile and 455 MPa minimum yield up to 102 mm — strength comparable to many medium-carbon steels at 2.81 g/cm³, about one-third of steel's density. The over-aged T73 / T7351 tempers trade roughly 10–15% of that strength for high resistance to stress corrosion cracking. 7075 machines to a fine finish with excellent dimensional stability in stretched T651 plate, but it is not fusion weldable — which is why it is chosen for machined aircraft fittings, structural parts and precision mould plates rather than welded fabrications.

Nifty Alloys supplies aluminium 7075 / 3.4365 from stock in Dubai, UAE, in round bar and plate / block, in the T6 / T651 condition as standard and in T73 / T7351 on request, to ASTM B209, ASTM B211, EN 485-2 and EN 754-2, with AMS 4123 supply available on request. Plate is saw cut to block size and bar to length, and every supply is dispatched with EN 10204 3.1 Mill Test Certificates as standard, giving certified, traceable chemistry, temper and mechanical results; EN 10204 3.2 third-party inspection is available on request. We deliver across the UAE within 24–48 hours, to Saudi Arabia, Kuwait, Qatar, Oman and Bahrain within 3–5 working days, and export to Europe, India and Africa for aerospace MRO, toolmaking and precision engineering. Send your size list or drawing to request a quote — quotations are turned around the same day.

Chemical Composition

Al

Aluminium

5.6 %
Zn

Zinc

5.1 – 6.1 %

2.5 %
Mg

Magnesium

2.1 – 2.9 %

1.6 %
Cu

Copper

1.2 – 2 %

0.23 %
Cr

Chromium

0.18 – 0.28 %

Fe

Iron

≤ 0.5 %

Si

Silicon

≤ 0.4 %

Mn

Manganese

≤ 0.3 %

Ti

Titanium

≤ 0.2 %

Others

each / total

≤ 0.05 %

Typical value Range (min–max) Minimum (≥) Maximum (≤) Hover / tap for notes

Standard

ASTM B209

ASTM

Revision: B209 / B211 — current editions

Standard specification for aluminium and aluminium-alloy sheet and plate. Covers 7075 in T6, T651, T73, T7351, and other temper conditions.

Primary ASTM standard for 7075 plate and sheet. Companion to ASTM B221 (bar/rod). Most widely referenced ASTM standard for aluminium plate in UAE mould, die, and aerospace applications.

Available Forms

Plate / Block

6–200 mm. Thickness, T651; blocks saw cut to size. Strength falls with thickness — see SpecSheet. [VERIFY — stock range not confirmed]

Round Bar

10–200 mm. Diameter, T651. ASTM B211 T651 to 178 mm; larger diameters on request. [VERIFY — stock range not confirmed]

Stock & delivery

Stock location
Dubai, UAE
In stock
T6 / T651 — standard stocked condition (plate and bar). T73 / T7351 on request. AMS 4123 certification on request.
Delivery UAE
24–48 hours
Delivery GCC
3–5 working days — Saudi Arabia, Kuwait, Qatar, Oman, Bahrain
Export
Europe, India, Africa on request
Quotation
Same-day quotation
Minimum order
No minimum order quantity for standard sizes

Key standards

ASTM B209

Designations & Equivalents

StandardDesignationNotes
Common Name7075(AA) Aluminum Association designation — primary
UNSA97075Unified Numbering System
EN NameEN AW-7075 / EN AW-AlZn5.5MgCuEN 573-3 designation
EN / Werkstoff3.4365Former DIN 1725-1 material number (AlZnMgCu1.5)
ISOAlZn5.5MgCuISO 209 chemical designation
ASTMB209 / B211Plate / rolled or cold-finished bar
Common NameEN 485-2 / EN 754-2(EN Standard) Plate / cold-drawn bar mechanical properties
AMSAMS 41237075-T651 rolled or cold-finished bars and rods
AMSAMS 40457075-T6 sheet and T651 plate — aliases only
AMSAMS 41227075-T6 / T651 rolled or cold-finished bars, rods, wire and rings — aliases only
AMSAMS 41247075-T73 / T7351 rolled or cold-finished bars, rods and wire — aliases only
Common NameQQ-A-225/9 / QQ-A-250/12(Federal (legacy)) Legacy federal bar / plate specifications, now AMS-QQ-A — still seen on drawings
JISA7075Japanese Industrial Standard
Common Name7075-T6 / 7075-T651 / aircraft aluminium / aerospace aluminiumBuyer search terms

Compliance & Certification

StandardStatusNotes
EN 10204 3.1SuitableProvided as standard — chemistry, temper and tensile results to ASTM B209 / B211 or EN 485-2 / EN 754-2.
EN 10204 3.2ConditionalAvailable on request with independent third-party inspection — specify at order stage.
AMS 4123ConditionalSupplied on request for T651 bar and rod — confirm specification revision at enquiry.

Specifications

Mechanical Properties

Values per ASTM B209. Bar length compares conditions within each row.

PropertyT6 / T651 | ASTM B209 / B211T73 / T7351 | ASTM B209 / B211
Tensile Strength (UTS)530 MPaminTypical 572 MPaBar — 3.2 to 102 mmASTM B211 minimum (77 ksi). Typical value marked typical.469 MPaminTypical 505 MPaBar — 3.2 to 102 mmASTM B211 minimum (68 ksi). Typical value marked typical.
Tensile Strength (UTS)517 MPaminBar (T651) — over 102 to 152 mmASTM B211 minimum (75 ksi); 503 MPa over 152–178 mm.455 MPaminBar — over 102 to 127 mmASTM B211 minimum (66 ksi); 441 MPa over 127–152 mm.
Tensile Strength (UTS)540 MPaminPlate T651 — 6.3 to 25 mmASTM B209 metric / EN 485-2 minimum.475 MPaminPlate T7351 — 6.3 to 50 mmASTM B209 metric minimum.
Tensile Strength (UTS)530 MPaminPlate T651 — over 25 to 50 mmASTM B209 / EN 485-2 minimum.440 MPaminPlate T7351 — over 60 to 80 mmASTM B209 metric minimum; 420 MPa over 90–100 mm.
Tensile Strength (UTS)495 MPaminPlate T651 — over 60 to 80 mmASTM B209 / EN 485-2 minimum; 460 MPa over 90–100 mm.–
Yield Strength (0.2% Proof Stress)455 MPaminTypical 503 MPaBar — 3.2 to 102 mmASTM B211 minimum (66 ksi). Typical value marked typical.386 MPaminTypical 435 MPaBar — 3.2 to 102 mmASTM B211 minimum (56 ksi). Typical value marked typical.
Yield Strength (0.2% Proof Stress)460 MPaminPlate T651 — over 25 to 50 mmEN 485-2 minimum; 420 MPa over 60–80 mm, 360 MPa over 90–100 mm.390 MPaminPlate T7351 — 25 to 50 mmASTM B209 metric minimum; 360 MPa over 50–60 mm.
Elongation7 %minTypical 11 %Bar — 4D gaugeASTM B211 minimum. Plate: 5% at 25–50 mm, 4% over 50 mm (EN 485-2).10 %minTypical 13 %Bar — 4D gauge, up to 102 mmASTM B211 minimum; 8% over 102 mm.
Hardness150 HBtypical500 kg / 10 mm ballTypical — not a specification requirement.135 HBtypical500 kg / 10 mm ballTypical — not a specification requirement.

Physical Properties

PropertyT6 / T651 | ASTM B209 / B211T73 / T7351 | ASTM B209 / B211
Densityat 20°C2.81 g/cm³2.81 g/cm³
Modulus of Elasticityat 20°C71.7 GPa71.7 GPa
Thermal Conductivityat 25°C130 W/m·K130 W/m·K
Coefficient of Thermal Expansionat 20–100°C23.4 µm/m·°C23.4 µm/m·°C
Specific Heat Capacityat 100°C960 J/kg·K960 J/kg·K
Electrical Conductivityat 20°C33 % IACS33 % IACS
Melting Point / Rangeat Solidus–Liquidus477 °C477 °C

Service Conditions

Service Temperature

Max 120 °C

Notes

[VERIFY — maxServiceTempC 120: continuous load-bearing limit not confirmed in a producer or code source] T6 / T651 is aged at about 120°C; prolonged exposure at or above this temperature over-ages the alloy and strength falls progressively, so long-term structural service should stay below it. Short exposures to higher temperatures (for example paint curing) cause measurable strength loss. Like other aluminium alloys, 7075 has no ductile-to-brittle transition and retains or gains strength at cryogenic temperatures.

Corrosion Performance

General corrosion

Not suitable for seawater immersion or unprotected outdoor use in the Gulf climate. Protect with hard or sulphuric anodising, chromate or trivalent conversion coating, primer or paint. Isolate from steel, stainless steel and copper alloys to prevent galvanic attack. Sour service: aluminium alloys are not certified to NACE MR0175 — not applicable.

Pitting resistance

Moderate general corrosion resistance — lower than 5xxx and 6xxx alloys because of its copper content. Pits in chloride and coastal atmospheres if unprotected. T6 / T651 is susceptible to stress corrosion cracking in the short-transverse direction under sustained tensile stress; T73 / T7351 is highly resistant (ASTM B211 T73 lot acceptance includes a minimum electrical conductivity check).

Additional notes

Not applicable — PREN applies to stainless steels and nickel alloys.

Heat Treatment

HEAT TREATMENT GUIDE — 7075 / 3.4365 / AlZn5.5MgCu

Solution heat treatment: about 465–480°C — soak per section thickness — rapid water quench (delay kept to seconds). Stress relief by stretching (T651 / T7351): controlled permanent stretch of about 1.5–3% after quenching and before ageing — removes quench stresses and minimises machining distortion. Artificial ageing to T6 / T651: about 120°C for 24 h — peak strength. Over-ageing to T73 / T7351: two-step ageing, a low-temperature step followed by a higher-temperature step near 160–175°C [VERIFY — exact cycle per AMS 2770 not confirmed] — about 10–15% lower strength with high stress-corrosion resistance. Annealing (O temper): about 415°C with controlled slow cooling [VERIFY — cycle not confirmed]; used only for severe forming before re-heat treatment. Post-machining: no heat treatment is needed on T651 / T7351 stock. Do not re-heat finished parts above about 120°C — this over-ages T6 material. Surface finishing: hard anodising (Type III) adds wear resistance for mould and tooling surfaces.

ENGINEERING NOTES
Weldability
Poor

7075 is not suitable for fusion welding: its zinc and copper content cause solidification (hot) cracking in the weld and liquation cracking in the heat-affected zone, and the HAZ loses most of its T6 strength. Join by mechanical fastening, riveting or adhesive bonding. Friction stir welding (solid-state) can join 7075 with acceptable properties where qualified. If a non-structural repair weld is unavoidable, the joint strength will be far below the parent metal and must not be relied on.

Filler metals
  • ER5356 · AWS A5.10 / TIG (GTAW)Non-structural repair only — joint strength far below parent; not for load-bearing welds
  • Friction stir welding (no filler) · Solid-state processPreferred joining route where welding is required — qualify procedure for the application
Machinability
Good

Machines very well in T6 / T651 (about 150 HB), producing short chips and a fine surface finish. Use sharp carbide or polished HSS tools with high positive rake, high spindle speeds and flood coolant or mist. T651 / T7351 stretched material has low residual stress and minimal distortion when pocketing deep cavities in mould plates — specify T651 rather than T6 for heavily machined parts. Hard anodising after machining is recommended for wear and corrosion protection.

Applications

  • Aircraft wing and fuselage fittings, brackets and machined structural parts
  • Plastic injection prototype and short-run mould plates, cores and cavities
  • Blow moulds, vacuum-forming and rubber moulds needing fast cycle times
  • Jigs, fixtures and tooling plates for CNC machining cells in UAE workshops
  • Aerospace MRO replacement parts machined from AMS 4123 bar in the GCC
  • Defence and missile components where high strength-to-weight is critical
  • Motorsport uprights, brackets and suspension components
  • High-strength gears, shafts and rods in lightweight machinery
  • Bicycle, climbing and sporting equipment components
  • Robotic arms, end-effectors and automation hardware
  • SCC-resistant T7351 structural fittings for humid or coastal environments

Frequently Asked Questions

Quick answers on our grades, certification, supply and lead times.

Still have questions?

Our team responds fast with specifications, certification and stock availability.

Contact our team

Aluminium 7075 is used for highly stressed machined parts where low weight matters: aircraft fittings and structural parts, defence components, motorsport and sporting equipment, robotic hardware, and precision mould plates and tooling. In T6 / T651 it reaches 530 MPa minimum tensile strength in bar at about one-third of steel's density. In the UAE and GCC, toolmakers machining injection and blow moulds and aerospace MRO workshops are major users of 7075-T651 plate and bar.