7075-T6 / 3.4365 (UNS A97075) - the highest-strength commercially available aluminium alloy. UTS min 503 MPa T6. Outstanding strength-to-weight ratio for aerospace structural components, plastic injection mould tooling, and high-performance engineering applications.

Industries Served

Aerospace & Defense
Mould & Die
Automotive
Manufacturing
Oil & Gas
Marine
Electronics

Overview

7075 (DIN 3.4365, EN AW-7075, UNS A97075) is a zinc-magnesium-copper aluminium alloy - the highest-strength commercially available wrought aluminium alloy. In the T6 (peak aged) condition, 7075 achieves a minimum tensile strength of 503 MPa with a density of only 2.81 g/cm3, giving it a specific strength (strength-to-weight ratio) that significantly exceeds medium carbon steel and approaches some low-alloy steels. The alloy's strength comes from its high zinc (5.1-6.1%), magnesium (2.1-2.9%), and copper (1.2-2.0%) additions, which form coherent MgZn2 (eta phase) precipitates during artificial ageing that create very fine-scale precipitation hardening. 7075 in T6 and T651 conditions is the industry standard for aircraft structural components, high-performance mould tooling for plastic injection moulding, and precision engineering applications where minimum weight at maximum strength is the design objective. The T651 designation confirms controlled stretching after quenching to relieve residual stress - always specify T651 for plate and thick bar where dimensional stability during heavy machining is required.

Nifty Alloys supplies 7075-T6 / 3.4365 aluminium from stock in Dubai, UAE, in round bar, flat bar, plate/sheet, square bar, and hollow bar. T651 stress-relieved plate and bar are available for mould tooling and aerospace structural applications requiring maximum dimensional stability. All material is supplied with EN 10204 3.1 Mill Test Certificates as standard, confirming chemical composition, mechanical properties, and temper designation. AMS 4122 (bar/rod) and AMS 4045 (plate) aerospace-certified material is available from our qualified mill sources - specify at enquiry stage. We deliver across the UAE within 24-48 hours and export to Saudi Arabia, Kuwait, Qatar, Oman, and Bahrain. Contact our team for same-day quotation.

Chemical Composition

Al

Aluminium

5.6 %
Zn

Zinc

5.1 – 6.1 %

2.5 %
Mg

Magnesium

2.1 – 2.9 %

1.6 %
Cu

Copper

1.2 – 2 %

0.23 %
Cr

Chromium

0.18 – 0.28 %

0.2 %
Fe

Iron

≤ 0.5 %

0.1 %
Si

Silicon

≤ 0.4 %

0.05 %
Mn

Manganese

≤ 0.3 %

0.05 %
Ti

Titanium

≤ 0.2 %

Other

each

≤ 0.05 %

Other

total

≤ 0.15 %

Typical value Range (min–max) Minimum (≥) Maximum (≤) Hover / tap for notes

Standard

ASTM B221 - current edition

Available Forms

Round Bar

Diameter 6-500 mm. Extruded and drawn. Per ASTM B221 / AMS 4122. T6 and T651 conditions. For mould cores, pins, and machined precision components. T6 condition standard; T651 available on request for large diameters.

Flat Bar

Thickness 5-150 mm, width up to 500 mm. Extruded per ASTM B221. For structural components, spacers, and machined flat parts.

Plate

Plate thickness 6-200 mm. Per ASTM B209 / AMS 4045. T651 (stress relieved) condition standard for plate. For mould bases, tooling plates, and aerospace structural panels. Cut-to-size available.

Sheet

Sheet thickness 0.5-6 mm. Per ASTM B209. For aerospace structural panels and machined flat parts. Cut-to-size available.

Square Bar

Cross-section 10-200 mm. Extruded per ASTM B221. For machined block components, jig details, and structural elements.

Hollow Bar

Extruded hollow section. OD 50-300 mm, various wall thicknesses. For lightweight structural tubes, pneumatic cylinder liners, and precision hollow components. Specify OD x ID x length. Available on request.

Designations & Equivalents

StandardDesignationNotes
Common Name7075Alloy number
EN NameAlZn5.5MgCuDIN / EN chemical name
EN / Werkstoff3.4365DIN material number (Werkstoff-Nr.)
UNSA97075—
EN NameEN AW-7075EN designation
ASTMB221 Alloy 7075ASTM bar/rod/extrusion
ASTMB209 Alloy 7075ASTM plate/sheet
AMSAMS 41227075-T6 bar and rod - aerospace procurement reference
AMSAMS 40457075-T651 plate - aerospace procurement reference
BSBS EN 573-3 EN AW-7075BS / ISO designation
Common NameAircraft aluminium / Aerospace aluminiumCommon name
Common Name7075-T6Common designation (T6 temper)
Common Name7075-T651Common designation (T651 temper)

Compliance & Certification

StandardStatusNotes
EN 10204 3.1SuitableMill Test Certificate standard with all Nifty Alloys supply, confirming chemical composition, mechanical properties, and temper designation.
EN 10204 3.2ConditionalIndependent third-party Mill Test Certificate available on request.
AMS 4122ConditionalAerospace bar/rod (7075-T6) certification available from qualified mill sources - specify at enquiry stage.
AMS 4045ConditionalAerospace plate (7075-T651) certification available from qualified mill sources - specify at enquiry stage. NACE MR0175 not applicable as primary specification.

Specifications

Mechanical Properties

Bar length compares conditions within each row.

PropertyT6 (Artificially Aged)ASTM B221T651 (Stress Relieved)ASTM B209
Tensile Strength (UTS)503 MPaminTypical 572 MPaRoom temp, longitudinalPer ASTM B221 7075-T6 bar. Min 503 MPa for bar; plate min 483 MPa (see T651 SpecSheet).483 MPaminTypical 558 MPaRoom temp, longitudinalPer ASTM B209 7075-T651 plate. Slightly lower minimum than T6 bar (503 MPa) - plate vs bar form difference, not temper difference.
Yield Strength (0.2% Proof Stress)434 MPaminTypical 503 MPaRoom temp0.2% offset.414 MPaminTypical 490 MPaRoom temp
Elongation8 %minTypical 11 %50 mm gauge length8 %minTypical 11 %50 mm gauge length
Hardness87 HRBmaxRockwell BApproximately 150-155 HB equivalent.87 HRBmaxRockwell BEquivalent to T6.
Fatigue Strength (endurance limit)159 MPamax10^8 cycles, R=-1, rotating beamFatigue strength of aluminium is lower than steel at equivalent UTS. [VERIFY]159 MPamax10^8 cycles, R=-1Same as T6. [VERIFY]
Fracture Toughness (KIc)27 MPa*m0.5maxL-T orientationLower than 7050 and 2024. SCC susceptible in ST direction. [VERIFY]–
Residual Stress–Near zero MPatypicalPost-stretchKey T651 advantage - controlled stretching eliminates residual quench stress. Distortion-free machining.

Physical Properties

PropertyT6 (Artificially Aged)ASTM B221T651 (Stress Relieved)ASTM B209
Densityat 20 degrees C2.81 g/cm32.81 g/cm3
Modulus of Elasticityat 25 degrees C71.7 GPa71.7 GPa
Thermal Conductivityat 25 degrees C130 W/m.K130 W/m.K
Coefficient of Thermal Expansionat 20-100 degrees C23.6 um/m.C23.6 um/m.C
Specific Heat Capacityat 20 degrees C960 J/kg.K960 J/kg.K
Melting Point / Rangeat Solidus477 degrees C477 degrees C

Service Conditions

Service Temperature

Min -269 °CMax 125 °C

Notes

7075-T6 is unsuitable for elevated temperature service above approximately 125 degrees C - the MgZn2 precipitates coarsen and dissolve progressively (over-ageing), causing significant strength reduction. For service above 125 degrees C, consider 7075-T73 or T7351 (over-aged - better elevated temperature stability) or switch to a different alloy system. Excellent cryogenic properties - maintains ductility and toughness to liquid helium temperature (-269 degrees C), making 7075 suitable for LNG, cryogenic piping, and aerospace cryogenic fuel system components.

Corrosion Performance

General corrosion

Moderate. 7075 is significantly less corrosion-resistant than 5083 or 6061 aluminium alloys due to its high copper content (1.2-2.0%). The copper creates galvanic couples with the aluminium matrix leading to localised pitting in marine and industrial environments. Anodising (per AMS 2571 or equivalent) is strongly recommended for any outdoor, marine, or humid service. Without surface protection, 7075 corrodes visibly in UAE coastal environments within months.

Pitting resistance

Moderate. Susceptible to pitting corrosion in chloride environments without surface protection. Anodise or chromate conversion coat for corrosion protection.

Additional notes

PREN is not applicable to aluminium alloys (PREN is a stainless-steel pitting index). Crevice corrosion: Moderate - susceptible in stagnant salt environments without coating. Stress corrosion cracking (SCC): IMPORTANT LIMITATION - 7075-T6 is susceptible to SCC in the short transverse (through-thickness) direction in marine and high-humidity environments under sustained tensile stress. This is a well-known limitation. For SCC-critical applications in marine or humid environments, specify 7075-T73 or T7351 (over-aged temper) which has significantly better SCC resistance at the cost of approximately 10-15% lower UTS. For mould tooling and aerospace dry-service applications in UAE, SCC is not typically a service concern. NACE: Not applicable as a primary specification - 7075 aluminium is not normally specified for sour service oil & gas applications under NACE MR0175. For specific downhole instrument and tool body applications, verify acceptability with the applicable standard.

Heat Treatment

7075 heat treatment is a two-step precipitation hardening process. Nifty Alloys supplies T6 and T651 in the fully heat-treated condition from the mill. The guide below is for customer reference only - re-heat treatment after machining is rarely required.

Solution Heat Treatment (SHT) - 460-480 degrees C - Water quench (rapid - mandatory) - Result: W condition (soft, highly ductile, not suitable for service). Dissolves all alloying elements into solid solution. Water quench mandatory - any delay or slow quench reduces subsequent ageing response and final strength. Perform within 5 seconds of removing from furnace.

Controlled Stretching (T651 - plate and bar only) - Room temperature - Mechanical (no cooling) - Result: T651 (residual stress eliminated, flat and distortion-free). Applied to plate and thick bar after quench. 1.5-3% permanent elongation. Eliminates residual stress that would cause distortion during machining. Nifty Alloys T651 plate is supplied pre-stretched by the mill - do not re-stretch.

Artificial Ageing (peak T6) - 120-125 degrees C - Air cool - Result: T6 (UTS min 503 MPa bar, min 483 MPa plate). 24 hours at 120-125 degrees C. MgZn2 precipitates form and provide maximum strength. Do not over-age (higher temperature or longer time) - this reduces strength and is irreversible without full re-SHT. Keep furnace temperature within +/-3 degrees C.

Over-ageing to T73 / T7351 (SCC resistance) - 160-175 degrees C (two-step) - Air cool - Result: T73/T7351 (UTS min 435 MPa - lower than T6 but much better SCC resistance). Two-step ageing: stage 1 at 120 degrees C (3-6 hrs) then stage 2 at 160-175 degrees C (14-18 hrs). Produces over-aged condition with significantly better stress corrosion resistance but approximately 10-15% lower strength than T6. Specify T73 for marine or humid outdoor service.

Annealing (O temper - full soft) - 415 degrees C - Slow furnace cool - Result: O temper (fully annealed, max ductility for cold forming). For cold forming operations requiring maximum ductility. Full anneal at 415 degrees C, cool at max 28 degrees C/hr to 260 degrees C, then air cool. Material must be re-SHT and aged to restore T6 properties after forming.

ENGINEERING NOTES
Weldability
Not_recommended

7075 in T6 / T651 condition has poor weldability by conventional arc welding processes. The high zinc and copper content makes it susceptible to solidification cracking (hot cracking) in the weld zone, and the HAZ undergoes significant strength reduction due to dissolution of the MgZn2 precipitates. For this reason, conventional MIG/TIG welding of 7075 is strongly discouraged for structural applications. Friction stir welding (FSW) is the preferred joining method for 7075 where welding is essential - FSW is a solid-state process that avoids solidification cracking and produces joints with strength approaching parent metal. For non-structural joining, adhesive bonding (aerospace-grade structural adhesives) and mechanical fastening are preferred. Where conventional welding cannot be avoided: preheat to 150-175 degrees C, use 4145 or 4043 filler, accept reduced joint strength, and apply full post-weld solution treatment and ageing if critical. Joining/filler options: Friction Stir Welding (FSW, solid state, no filler) is the preferred method for structural assemblies; AWS/MIG (GMAW) with 4145 or 4043 filler is for non-structural joints only with 150-175 degrees C preheat and full re-T6 if critical; aerospace-grade structural epoxy (Hysol EA9394 or equivalent) adhesive bonding is the preferred alternative to welding and eliminates HAZ softening.

Machinability
Excellent

7075-T6/T651 has excellent machinability - one of the best-machining structural alloys available. Machinability rating approximately 70% of free-machining brass. High cutting speeds (5-10x steel), sharp HSS or carbide tooling, flood coolant or mist. Low cutting forces reduce tool wear and allow high material removal rates. 7075 is the preferred aluminium alloy for CNC milling of mould cavities and precision components due to its combination of high strength, excellent surface finish, and fast machining speeds. T651 plate gives better dimensional stability during machining than T6 due to absence of residual stress.

Applications

  • Plastic injection mould plates, cavity blocks, and core inserts where high strength and machinability must be combined for rapid prototyping and medium-volume production tooling
  • Aircraft structural components including fuselage frames, wing ribs, skins, and bulkheads requiring maximum strength at minimum weight per AMS 4122 / AMS 4045
  • Aerospace fasteners, structural fittings, and machined brackets for aircraft and missile structural assemblies
  • High-performance automotive racing components including suspension uprights, gear housings, and structural brackets requiring steel-competitive strength at aluminium weight
  • CNC machined precision components and housings for semiconductor and electronics manufacturing equipment in UAE hi-tech manufacturing sector
  • Offshore and marine structural components where corrosion resistance and weight savings are both important - deck fittings, housings, and structural panels
  • Military and defence equipment components including weapon system housings, vehicle structural panels, and portable equipment frames per defence procurement specifications
  • Bicycle and sports equipment frames, bicycle componentry, and recreational equipment requiring the highest strength aluminium alloy available
  • Pneumatic and hydraulic cylinder liners from hollow bar, valve bodies, and precision fluid power components requiring lightweight high-strength properties
  • Oil & gas downhole instrument housings, wireline tool bodies, and subsea equipment components requiring non-magnetic, high-strength lightweight materials

Frequently Asked Questions

Quick answers on our grades, certification, supply and lead times.

Still have questions?

Our team responds fast with specifications, certification and stock availability.

Contact our team

7075-T6 is the highest-strength commercial aluminium alloy, specified wherever maximum strength at minimum weight is required. Key applications in UAE and globally include: plastic injection mould plates, cavity blocks, and core inserts for rapid tooling production; aircraft structural components including fuselage frames, wing ribs, and skin panels per AMS 4122 / AMS 4045; aerospace fasteners, fittings, and structural brackets; high-performance automotive racing suspension and structural components; CNC machined precision housings and equipment frames for semiconductor and hi-tech manufacturing; offshore and marine structural components; military and defence equipment housing and structural panels; and downhole oil & gas instrument tool bodies requiring non-magnetic lightweight high-strength properties. Its specific strength (UTS/density) significantly exceeds medium carbon steel, making it the aluminium of choice when steel is too heavy.