Bronze dealers in UAE

C51000 / CuSn5 / CW451K / PB102 Phosphor Bronze | Supplier in UAE & GCC

C51000 / CuSn5 / CW451K (PB102) — 5% phosphor bronze: high fatigue strength, spring and wear properties, marine corrosion resistance; bushes, springs.

Industries Served

Marine
Electrical
Heavy Engineering
Aerospace & Defence
Petrochemical

Overview

C51000 phosphor bronze (EN CuSn5 / CW451K; BS PB102; JIS C5102; DEF STAN 02-838; AMS 4625) is the most widely used wrought phosphor bronze, containing 4.2–5.8% tin (4.5–5.5% to EN) and 0.03–0.35% phosphorus, with copper the remainder. Tin raises strength by solid solution and improves corrosion resistance, while phosphorus deoxidises the alloy and increases stiffness and wear resistance. The result is an excellent combination of strength and ductility, high fatigue strength, superb spring qualities and a low coefficient of friction against steel, with corrosion resistance in marine and industrial atmospheres close to that of aluminium bronzes. It responds very well to cold working — strength comes entirely from drawing — and brazes, solders and butt-welds readily, although its hot formability is poor and machinability is modest (about 20% of free-cutting brass). It is supplied cold drawn to ASTM B139 half-hard (H02) or hard (H04); hard-drawn PB102 bar typically reaches about 570 MPa tensile and 520 MPa proof stress, while EN 12163 R330 rod gives at least 330 MPa tensile with 35–45% elongation. It is non-magnetic with electrical conductivity of about 15–17% IACS. Typical uses are bushes and bearings, thrust washers, springs and diaphragms, fasteners, pump and valve spindles, gears and worm gears, electrical connectors and switches, and bridge bearing plates.

Nifty Alloys supplies C51000 / CuSn5 / PB102 phosphor bronze from Dubai, UAE, in round bar, flat bar and plate — H02 half hard as standard and H04 hard on request — with AMS 4625 supply on request. Every supply carries an EN 10204 3.1 Mill Test Certificate as standard; EN 10204 3.2 third-party inspection is available on request. We deliver across the UAE within 24–48 hours, to Saudi Arabia, Kuwait, Qatar, Oman and Bahrain within 3–5 working days, and export to Europe, India and Africa. Send your size list and temper to request a quote — quotations are turned around the same day.

Chemical Composition

94.8 %
Cu

Copper

5 %
Sn

Tin

4.2 – 5.8 %

0.2 %
P

Phosphorus

0.03 – 0.35 %

Zn

Zinc

≤ 0.3 %

Fe

Iron

≤ 0.1 %

Pb

Lead

≤ 0.05 %

Ni

Nickel

Typical value Range (min–max) Minimum (≥) Maximum (≤) Hover / tap for notes

Standard

ASTM B139 / B139M

Other

Revision: ASTM B139 / B139M — current edition

Available Forms

Flat Bar

4–50 mm. Thickness; width to order. [VERIFY — stock range not confirmed]

Plate / Block

3–50 mm. Thickness; cut to size. [VERIFY — stock range not confirmed]

Round Bar

6–80 mm. Diameter, H02 / H04 (EN R330 to 80 mm). [VERIFY — stock range not confirmed]

Stock & delivery

Stock location
Dubai, UAE
In stock
H02 half-hard bar [VERIFY — stocked forms]; H04 hard and AMS 4625 on request.
Delivery UAE
24–48 hours
Delivery GCC
3–5 working days — Saudi Arabia, Kuwait, Qatar, Oman, Bahrain
Export
Europe, India, Africa on request
Quotation
Same-day quotation
Minimum order
No minimum order quantity for standard sizes; cut pieces available

Key standards

ASTM B139 / B139M

Designations & Equivalents

StandardDesignationNotes
UNSC51000Primary chemistry (ASTM B139 / B103)
EN NameCuSn5EN 12163 / EN 1652 designation
EN / WerkstoffCW451K(EN Number) EN numerical designation
BSPB102BS 2874 / 2870 designation (5% tin) — NOT PB101
Common NameDEF STAN 02-838(UK Defence) Naval rod specification — aliases only
AMSAMS 4625Hard-drawn product (Module 2) [VERIFY scope]
Common NameAMS 4510 / AMS 4720 / MIL-T-3595(AMS / MIL) Sheet-strip / wire / tube — aliases only
Common NameQQ-B-750 / J461 / J463 / SB-171(Federal / SAE / ASME) Legacy federal and related specifications — aliases only
Common NameC5102 / ISO 427 CuSn5 / IS 7811(JIS / ISO / IS) National and ISO equivalents — aliases only
Common Name5% phosphor bronze / PB102 / Phosphor Bronze A / CDA 510 / C510 bronze barBuyer search terms

Compliance & Certification

StandardStatusNotes
EN 10204 3.1SuitableProvided as standard — chemistry, temper and mechanical properties.
AMS 4625ConditionalSupplied to AMS 4625 on request — confirm revision and product scope.

Specifications

Mechanical Properties

Values per ASTM B139 / B139M. Bar length compares conditions within each row.

PropertyH02 Half Hard | ASTM B139H04 Hard | ASTM B139
Tensile Strength (UTS)330 MPaminTypical 485 MPaH02 / EN R330EN R330 minimum; typical half-hard about 485 MPa [VERIFY B139].550–880 MPaTypical 570 MPaH04 rod ≤ 6 mmASTM B139 range for small rod; typical 570 MPa [VERIFY larger sizes].
Yield Strength (0.2% Proof Stress)380 MPatypicalH02Typical [VERIFY].520 MPatypicalH04Typical.
Elongation25 %typicalH02Typical [VERIFY].10 %typicalH04Typical [VERIFY].
Hardness120–160 HVHalf hardTypical range — guidance.180 HVtypicalHardTypical.

Physical Properties

PropertyH02 Half Hard | ASTM B139H04 Hard | ASTM B139
Densityat 20°C8.86 g/cm³8.86 g/cm³
Modulus of Elasticityat 20°C110 GPa110 GPa
Thermal Conductivityat 20°C69 W/m·K69 W/m·K
Coefficient of Thermal Expansionat 20–300°C17.8 µm/m·°C17.8 µm/m·°C
Specific Heat Capacityat 20°C377 J/kg·K377 J/kg·K
Electrical Conductivityat 20°C15 % IACS15 % IACS

Service Conditions

Service Temperature

Min -196 °CMax 200 °C

Notes

Cold-worked tempers soften above about 200°C (annealing 500–700°C). Retains toughness at cryogenic temperatures. Melting range about 950–1050°C.

Corrosion Performance

General corrosion

Corrosion resistance almost equivalent to aluminium bronzes in many atmospheres; good stress corrosion cracking resistance. Attacked by oxidising acids, ammonia and sulphides.

Pitting resistance

Good resistance to seawater, marine and industrial atmospheres; no dezincification (zinc-free).

Additional notes

Not applicable — PREN is not used for copper alloys.

Heat Treatment

HEAT TREATMENT GUIDE — C51000 / CuSn5 / CW451K

Not hardenable by heat treatment — strength from cold work (H02 / H04 / R-tempers). Annealing: about 500–700°C (900–1250°F), rapid cooling. Stress relieving: about 190–260°C for 1–2 h — improves spring stability. Hot working: poor — primarily a cold-worked alloy. Cold working: excellent.

ENGINEERING NOTES
Weldability
Good

Soldering, brazing and butt welding are rated excellent; gas-shielded arc welding is possible with phosphor-bronze filler. Avoid excessive heat input on heavy sections (hot-cracking risk).

Filler metals
  • ERCuSn-A · AWS A5.7 / TIG (GTAW) / MIG (GMAW)Phosphor bronze filler wire
  • ECuSn-A · AWS A5.6 / SMAWPhosphor bronze covered electrode (5% Sn type)
  • BAg series · AWS A5.8 / BrazingSilver brazing alloys
Machinability
Fair

Machinability about 20% of free-cutting brass — tough continuous chips. Use sharp tooling with positive rake and coolant; for high-volume turned parts, leaded phosphor bronzes are the free-machining alternative.

Applications

  • Bushes, bearings and thrust washers
  • Springs, diaphragms and bellows
  • Fasteners, bolts, nuts and cotter pins
  • Pump and valve spindles and shafts
  • Gears, worm gears and pinions
  • Electrical connectors, switches and contacts
  • Bridge bearing plates
  • Marine hardware and fittings for GCC vessels
  • Chemical-plant and instrument components
  • Screw-machine and general engineering parts

Frequently Asked Questions

Quick answers on our grades, certification, supply and lead times.

Still have questions?

Our team responds fast with specifications, certification and stock availability.

Contact our team

C51000 / CuSn5 / PB102 is used for bushes and bearings, thrust washers, springs and diaphragms, fasteners, pump and valve spindles, gears and worm gears, electrical connectors and switches, bridge bearing plates and marine hardware. It is the most widely used wrought phosphor bronze, including across the UAE and GCC.

Get in touch

Elevateyourprojectswithoursuperiorsteel