D6 / 1.2436 / X210CrW12 Cold Work Tool Steel | Supplier in UAE & GCC

D6 (1.2436 / X210CrW12) — 12% Cr cold work tool steel with tungsten for high wear resistance and deeper hardening in large blanking and forming dies.

Industries Served

Mould & Die
Manufacturing
Automotive
Construction
Heavy Engineering

Overview

D6 tool steel (AISI D6 / DIN 1.2436 / X210CrW12, UNS T30406) is a ledeburitic high-carbon, high-chromium cold work tool steel containing 2.00–2.30% carbon, 11.0–13.0% chromium and 0.60–0.80% tungsten, specified to EN ISO 4957. It is essentially the 1.2080 / X210Cr12 (D3) analysis with a tungsten addition. Tungsten forms additional hard carbides and raises hardenability, so D6 gives slightly better wear resistance than D3 and holds full hardness through much thicker sections — producer hardenability data show 60 HRC or more through sections of about 100 mm. Toughness stays modest, so D6 is used where abrasion rather than shock limits tool life. It is hardened from 950–980 °C to about 64 HRC, usually in oil or a 500–550 °C hot bath, and tempered at 150–250 °C for 60–63 HRC. D6 is supplied soft annealed to 255 HB maximum. It is specified for large blanking dies, electrical lamination tooling, profile rolls, brick tooling and paper-cutting knives.

Nifty Alloys supplies D6 / 1.2436 / X210CrW12 tool steel through our Dubai, UAE facility in round bar, flat bar and plate / block, soft annealed and ready for machining and heat treatment. D6 is supplied on request against your order; for urgent jobs, D2 / 1.2379 is held in Dubai stock as a tougher 12% Cr alternative. Every order is supplied with an EN 10204 3.1 Mill Test Certificate as standard, confirming chemistry and annealed hardness with full traceability to the producing mill. EN 10204 3.2 third-party inspection is available on request. We deliver across the UAE and the GCC — Saudi Arabia, Kuwait, Qatar, Oman and Bahrain — and export to Europe, India and Africa. As an ISO 9001:2015 certified tool steel supplier in the UAE, our team can help you choose between D6, D3 and D2 for heavy-section dies. Contact our team to request a quote.

Chemical Composition

2.1 %
C

Carbon

2 – 2.3 %

0.25 %
Si

Silicon

0.1 – 0.4 %

0.4 %
Mn

Manganese

0.3 – 0.6 %

P

Phosphorus

≤ 0.03 %

S

Sulfur

≤ 0.03 %

12 %
Cr

Chromium

11 – 13 %

0.7 %
W

Tungsten

0.6 – 0.8 %

Typical value Range (min–max) Minimum (≥) Maximum (≤) Hover / tap for notes

Standard

EN ISO 4957

EN

Revision: EN ISO 4957:2018

Tool steels — specification for chemical composition, heat treatment, and properties of tool steels including cold work, hot work, and high-speed grades.

Published as BS EN ISO 4957; leading BS dropped to match house style. European standard governing 1.2379 (X153CrMoV12) and other DIN tool steel grades. Supersedes former DIN 17350 for tool steels. Referenced in European and Middle Eastern engineering procurement. Equivalent German standard: DIN EN ISO 4957.

Available Forms

Flat Bar

10–200 mm. Thickness. Widths to order; saw-cut from block where needed. Supplied on request.

Plate / Block

10–400 mm. Thickness. Saw-cut to customer dimensions. Supplied on request.

Round Bar

10–500 mm. Diameter. Typical mill range, supplied on request — confirm size and lead time at enquiry.

Stock & delivery

Stock location
Dubai, UAE
In stock
Annealed — D6 / 1.2436 is supplied on request (not held as Dubai stock); lead time confirmed at quotation. D2 / 1.2379 annealed is held in Dubai stock as an alternative. UAE / GCC delivery times apply from dispatch.
Delivery UAE
24–48 hours
Delivery GCC
3–5 working days — Saudi Arabia, Kuwait, Qatar, Oman, Bahrain
Export
Europe, India, Africa on request
Quotation
Same-day quotation
Minimum order
No minimum order quantity for standard sizes

Key standards

EN ISO 4957

Designations & Equivalents

StandardDesignationNotes
AISI / SAED6Primary designation (legacy AISI type)
UNST30406Unified Numbering System
EN / Werkstoff1.2436European material number
DINX210CrW12German designation (formerly DIN 17350)
EN NameX210CrW12EN ISO 4957 steel name
ISOX210CrW12ISO 4957 designation
ASTMA681 (D6) — alias onlyD6 is not a listed type in current ASTM A681 (Table 1 covers D2, D3, D4, D5, D7). Material is supplied to EN ISO 4957.
JISNoneNo direct JIS equivalent. SKD1 is D3 / 1.2080 and SKD11 is D2 / 1.2379 — do not substitute.
AMSNoneNo AMS specification applies to D6 / 1.2436 — not an aerospace procurement grade
Common NameD6 tool steel, 12% chromium tungsten tool steel, HCHCr-W die steel, 2436 steelBuyer search terms used in UAE / GCC and Europe

Compliance & Certification

StandardStatusNotes
EN 10204 3.1SuitableMill Test Certificate provided as standard. Confirms chemistry and annealed hardness to EN ISO 4957.

Specifications

Mechanical Properties

Values per EN ISO 4957. Bar length compares conditions within each row.

PropertyAnnealed | EN ISO 4957
Hardness (annealed)255 HBmaxSurface, as suppliedMax per EN ISO 4957.
Tensile Strength (UTS)–Room tempNot specified by EN ISO 4957 for annealed tool steel — leave blank.
Yield Strength (0.2% Proof Stress)–Room tempNot specified — leave blank.
Elongation–Not specified — leave blank.
Hardness (as quenched)64 HRCtypical950–980 °C, oil / hot bathTypical — producer data. Not a specified value.
Hardness (hardened & tempered)62 HRCtypicalQuenched + 200 °C temperTypical — producer data. Working range 60–63 HRC.

Physical Properties

PropertyAnnealed | EN ISO 4957
Densityat 20°C7.77 g/cm³
Modulus of Elasticityat 20°C210 GPa
Thermal Conductivityat 20°C16.7 W/m·K
Coefficient of Thermal Expansionat 20–100°C10.8 µm/m·°C
Specific Heat Capacityat 20°C460 J/kg·K
Melting Point / Rangeat Solidus–[VERIFY — source not confirmed]. Leave blank until confirmed.

Service Conditions

Service Temperature

Max 200 °C

Notes

D6 is a cold work steel: the tool must work below its final tempering temperature or it softens. At the usual 200 °C temper (about 62 HRC) the working limit is about 200 °C. D6 is not secondary hardening — hardness falls to about 56 HRC after a 500 °C temper and 48 HRC after 600 °C — so it has no useful hot hardness. Use a hot work grade such as H13 / 1.2344 for tooling above this. Avoid impact loading and thermal shock.

Corrosion Performance

General corrosion

Stains less readily than low-alloy tool steels but will rust in humid or coastal UAE and GCC conditions. Store under cover with rust-preventive oil. For corrosion-resistant mould work specify 1.2083 / X40Cr14. Hardened D6 accepts PVD coatings for extra wear life.

Pitting resistance

No meaningful pitting resistance in chloride environments. D6 is not a stainless or corrosion-resistant mould steel.

Additional notes

Not applicable — tool steel. About 12% Cr is present, but most is bound in M7C3 carbides, so the matrix does not passivate.

Heat Treatment

ProcessTemperatureCoolingResult & notes
HEAT TREATMENT GUIDED6 / 1.2436 / X210CrW12: Soft Annealing: 800–840 °C2–5 hslow furnace cooling — max 255 HB. Stress Relieving: 600–650 °C — minimum 4 h (or 1 h after through-heating for small parts) — slow furnace cooling. After heavy rough machining, before finish machining and hardening. Preheating: In stages, for example about 400 °C and 650 °C, then 800–850 °C, to limit distortion and cracking risk. Hardening: Austenitise at 950–980 °C — hold until through-heated plus soak — quench in oil, a 500–550 °C hot bath (lowest distortion), or pressurised gas in vacuum furnaces. Small sections can be cooled in air. As-quenched hardness about 64 HRC. Through-hardening: producer data show about 60 HRC through sections of about 100 mm and 58 HRC at about 250 mm. Tempering: Start as soon as the tool reaches about 80 °C — do not let it cool to room temperature. Typical temper 150–250 °C for 60–63 HRC. Double temper, minimum 2 h each (1 h per 25 mm section). Typical hardness after tempering: 100 °C — 63 HRC; 200 °C — 62 HRC; 300 °C — 60 HRC; 400 °C — 58 HRC; 500 °C — 56 HRC; 600 °C — 48 HRC. No secondary hardening peak. Surface Treatment: PVD coating of hardened tools is common. Nitriding temperatures (500 °C+) reduce core hardness to about 56 HRC or less. Post-weld Stress Relief (annealed material): 600–650 °C — furnace cooling.
ENGINEERING NOTES
Weldability
Poor

D6 / 1.2436 is not used for welded joints. With over 2% carbon and a large carbide volume it cracks readily on cooling. Die repair is possible only with preheat to 250–300 °C, interpass held at or above preheat, low-hydrogen practice and slow cooling under cover. On annealed material, stress relieve at 600–650 °C with furnace cooling after welding. Hardened tools must be re-tempered after repair. Ask us before welding a hardened D6 tool.

Filler metals
  • ER312 · AWS A5.9 / TIG (GTAW)Buffer (buttering) layer on crack-sensitive high-carbon base metal before hard build-up. Not a matching-hardness deposit.
  • Cold work matching rod, 56–62 HRC deposit · Tool-steel repair rod / TIG (GTAW)For edge and surface build-up on dies. [VERIFY — consumable code and classification to be confirmed with consumable supplier]
Machinability
Fair

Machine in the soft-annealed condition (≤255 HB). Producer data put machinability at about 20–25% of a free-cutting 1018 carbon steel, so use coated carbide for turning and milling and cobalt HSS for drilling at low speed. Stress relieve at 600–650 °C (minimum 4 h) after heavy rough machining. Avoid wire EDM of large solid sections — D6 is not secondary hardening and keeps high residual stress at its low tempering temperature; D2 / 1.2379 is the better choice for heavy wire-cut work. Grind hardened tools with soft, open wheels and plenty of coolant.

Applications

  • Large blanking and trimming dies too thick to through-harden in D3
  • Stamping dies for silicon-steel electrical laminations in motor and transformer production
  • Profile rolls for roll-forming lines in GCC steel framing and sandwich-panel plants
  • Brick extrusion die inserts and clay-press tooling for UAE and Saudi brick plants
  • Guillotine and rotary knives for paper, cardboard and corrugated packaging
  • Tube and wire drawing dies, plugs and mandrels for abrasive drawing duty
  • Flat thread-rolling dies for bolt and screw manufacture
  • Press tooling for ceramic tiles, refractories and abrasive powders
  • Planer and profile knives for hardwood and composite-board joinery
  • Wear plates and guide rails for cement and aggregate handling equipment
  • Ring gauges, plug gauges and wear-critical measuring tools

Frequently Asked Questions

Quick answers on our grades, certification, supply and lead times.

Still have questions?

Our team responds fast with specifications, certification and stock availability.

Contact our team

D6 tool steel (1.2436 / X210CrW12) is used for heavy-section cold work tooling that must resist abrasion. Typical parts are large blanking and trimming dies, stamping dies for silicon-steel electrical laminations, profile rolls for roll-forming lines, brick extrusion die inserts, paper and cardboard knives, drawing dies and thread-rolling dies. Hardened and tempered to 60–63 HRC, its chromium and tungsten carbides resist wear from abrasive sheet, clay and fibre. In the UAE and GCC it is specified mainly for brick and block plants, steel-framing roll lines and packaging converters.

Get in touch

Elevateyourprojectswithoursuperiorsteel