Tool Steel dealers in UAE

H13 / 1.2344 / X40CrMoV5-1 Hot Work Tool Steel | Supplier in UAE & GCC

H13 (1.2344 / X40CrMoV5-1) — 5% Cr-Mo-V hot work tool steel with high hot strength, heat-check resistance and toughness for die casting and forging dies.

Industries Served

Automotive
Manufacturing
Mould & Die
Aerospace & Defence
Oil & Gas
Heavy Engineering

Overview

H13 hot work tool steel (DIN 1.2344, EN ISO 4957 X40CrMoV5-1, UNS T20813, JIS SKD61, BS BH13) is a 5% chromium–molybdenum–vanadium air-hardening tool steel standardised under ASTM A681 and EN ISO 4957. Its nominal 0.40% C, 5.2% Cr, 1.4% Mo and 1.0% V balance gives a strong secondary-hardening response: fine vanadium- and molybdenum-rich carbides precipitate during tempering at 550–620°C, so the steel resists softening when tool surfaces cycle to around 540–600°C, temperatures at which conventional CrMo alloy steels lose strength rapidly. Around 1% silicon adds tempering and scaling resistance, while the moderate carbon level keeps toughness high enough for dies that are water-cooled in service. H13 is supplied soft annealed to a maximum of 229 HB (EN ISO 4957) or 235 HB (ASTM A681) for machining, then hardened from 1020–1030°C and multiple-tempered to a working hardness of typically 44–52 HRC. It is the reference grade for aluminium, zinc and magnesium die casting dies, aluminium extrusion dies, hot forging dies and hot-shear tooling.

Nifty Alloys supplies H13 / 1.2344 hot work tool steel from stock in Dubai, UAE, in round bar, flat bar, plate / block and forgings — annealed for machining, or pre-hardened to 44–48 HRC for finish-machined tooling. Material is offered to ASTM A681 or EN ISO 4957 X40CrMoV5-1 to suit American or European drawings, and every piece is supplied with an EN 10204 3.1 Mill Test Certificate confirming chemistry, hardness and full traceability to the producing mill; EN 10204 3.2 third-party inspection is available on request. Saw-cut bars and blocks are delivered across the UAE within 24–48 hours and to Saudi Arabia, Kuwait, Qatar, Oman and Bahrain in 3–5 working days, with export to Europe, India and Africa on request. Send your sizes and condition to our team to request a quote — same-day quotation as standard.

Chemical Composition

0.4 %
C

Carbon

0.32 – 0.45 %

1 %
Si

Silicon

0.8 – 1.25 %

0.4 %
Mn

Manganese

0.2 – 0.6 %

5.2 %
Cr

Chromium

4.75 – 5.5 %

1.4 %
Mo

Molybdenum

1.1 – 1.75 %

1 %
V

Vanadium

0.8 – 1.2 %

Ni

Nickel

≤ 0.3 %

Cu

Copper

≤ 0.25 %

P

Phosphorus

≤ 0.03 %

S

Sulfur

≤ 0.03 %

Typical value Range (min–max) Minimum (≥) Maximum (≤) Hover / tap for notes

Standard

ASTM A681

ASTM

Revision: ASTM A681 — current edition [VERIFY — confirm edition year]

Standard specification for alloy tool steels — covers cold work, hot work, shock-resistant, and special purpose tool steel grades including D2.

Primary North American standard for D2 / D3 / D6 cold work tool steels. Defines chemical composition requirements. Widely referenced in UAE and GCC mould and die procurement. Companion: ASTM A685 (high-speed steels).

Available Forms

Flat Bar

10–200 mm. Thickness. Saw-cut from plate / block to customer width — custom sizes on request. [VERIFY]

Forging

200–1000 mm. Typical forged block / disc section, made to drawing. Maximum section subject to mill capability. [VERIFY]

Plate / Block

10–400 mm. Thickness. Widths cut to order; black or rough-milled. UT to EN 10228-3 on request. [VERIFY]

Round Bar

16–500 mm. Diameter. Black or peeled. Larger diameters as forged bar on request. [VERIFY — confirm stocked range with purchasing]

Stock & delivery

Stock location
Dubai, UAE
In stock
Annealed (≤229 HB) round bar and plate / block — from stock. Pre-hardened 44–48 HRC, flat bar to size, forgings, ESR / premium quality and AMS 6408 material — supplied to order. [VERIFY — confirm against current stock]
Delivery UAE
24–48 hours
Delivery GCC
3–5 working days — Saudi Arabia, Kuwait, Qatar, Oman, Bahrain
Export
Europe, India, Africa on request
Quotation
Same-day quotation
Minimum order
No minimum order quantity for standard sizes

Key standards

ASTM A681

Designations & Equivalents

StandardDesignationNotes
AISI / SAEH13Primary designation — AISI/SAE hot work, chromium type
UNST20813Unified Numbering System — wrought H13
EN / Werkstoff1.2344European material number
DINX40CrMoV5-1DIN EN ISO 4957 designation
EN NameX40CrMoV5-1EN ISO 4957 steel name
ISOX40CrMoV5-1ISO 4957
BSBH13BS 4659 (withdrawn) — still quoted on legacy drawings
JISSKD61JIS G4404
ASTMA681ASTM product standard for alloy tool steels
AMSAMS 6408ESR / VAR premium aircraft-quality H13 only
Common NameZ40CDV5AFNOR (France) legacy designation
Common Name4Cr5MoSiV1GB/T (China) designation
Common Name2344, H13 die steel, 5% Cr hot work steelBuyer search terms

Compliance & Certification

StandardStatusNotes
EN 10204 3.1SuitableMill Test Certificate provided as standard — heat number, chemistry, hardness, conformity to ASTM A681 and/or EN ISO 4957.
EN 10204 3.2ConditionalAvailable on request — specify at order stage.
NACE MR0175 / ISO 15156Not Applicable — Tool steel — not listed for sour-service pressure-containing equipment. Not to be used for oil & gas wetted components in H2S service.
NACE MR0103Not Applicable — Tool steel — not applicable to refinery sour-service equipment.
EN 10228-3 Ultrasonic TestingRequires ConfirmationUT of blocks and forgings to an agreed EN 10228-3 quality class (or SEP 1921 class) available on request — recommended for large die blocks.

Specifications

Mechanical Properties

Values per ASTM A681. Bar length compares conditions within each row.

PropertyAnnealed | ASTM A681Pre-hardened 44–48 HRC | EN ISO 4957
Hardness235 HBmaxTypical 200–220 HBSurface, as deliveredASTM A681 max 235 HB; EN ISO 4957 max 229 HB. Typical value — producer data.44–48 HRCTypical 46 HRCSurfaceRange agreed on purchase order — not a standard-defined condition.
Tensile Strength (UTS)≤780 MPatypicalRoom tempNot specified by standard. Typical — approximate conversion from 229–230 HB.1430–1610 MPatypicalRoom tempTypical — approximate conversion from 44–48 HRC (ASTM E140). Not a guaranteed value.
Yield Strength (0.2% Proof Stress)–Room tempNot specified by ASTM A681 / EN ISO 4957 — report from mill certificate if tested. [VERIFY — source not confirmed]1200–1400 MPatypicalRoom tempTypical [VERIFY — source not confirmed]
Elongation–Not specified by ASTM A681 / EN ISO 4957. [VERIFY — source not confirmed]10–13 %typicalRoom tempTypical [VERIFY — source not confirmed]
Hardness (heat-treatment response)52–56 HRCtypicalAs quenched from 1020–1030°CTypical — confirms hardening response; not a delivery-condition property.–

Physical Properties

PropertyAnnealed | ASTM A681Pre-hardened 44–48 HRC | EN ISO 4957
Densityat 20°C7.8 g/cm³–
Modulus of Elasticityat 20°C210 GPa–
Thermal Conductivityat 20°C25 W/m·K–
Coefficient of Thermal Expansionat 20–100°C10.5 µm/m·°C–
Specific Heat Capacityat 20°C460 J/kg·K–
Electrical Resistivityat 20°C0.52 Ω·mm²/m–
ISO 9001:2015at Quality Management System — procurement, stock management, supply.––[Current registrar — maintained in this Certification record only]
AEO (Authorised Economic Operator)at Customs compliance for UAE and GCC trade.––UAE Federal Customs Authority
1–13 Not a confirmed form — omitted.
2––Live page claims export to "the Americas".
3––Live metaTitle / metaDescription have no UAE or DIN designation and canonical uses /products/.
4––Live chemistry / mechanical / heat-treatment tabs did not render.
5–13 Add 301: /products/h13-tool-steel → /tool-steel/h13-1-2344-hot-work-tool-steel. Update approved-slugs.md.
6–6408 Listed as procurement reference only; standard air-melted stock does not comply.
7–681 Confirm against the current ASTM A681 edition — [VERIFY] flags in 7.9.
8––Size ranges and in-stock conditions are typical industry values.
9–44 Consider adding pre-hardened-44-48 to product-structure-template-v3.md.

Service Conditions

Service Temperature

Max 540 °C

Notes

Typical continuous working limit for the tool surface; intermittent surface peaks to about 600°C are normal in die casting and forging. Keep working temperature at least 25–50°C below the final tempering temperature, otherwise the tool softens in service. Preheat dies to 250–300°C before first shot or forging stroke — hardened H13 has reduced toughness when cold and cracks under thermal shock. Re-temper (stress-relieve) dies periodically in service at 25–50°C below the last tempering temperature.

Corrosion Performance

General corrosion

Nitriding or nitrocarburising improves resistance to erosion and to soldering by molten aluminium, and modestly improves atmospheric corrosion resistance. Unprotected H13 surfaces are attacked by molten aluminium. For moulds processing corrosive resins (e.g. PVC), specify a stainless mould steel such as 1.2083.

Pitting resistance

Not resistant to chloride pitting. Rusts in humid coastal atmospheres such as the Gulf — protect stock and finished tools with oil or VCI wrapping. Condensation and untreated cooling water cause pitting in die cooling channels.

Additional notes

Not applicable — tool steel. About 5% Cr is insufficient for stainless passivity.

Heat Treatment

ProcessTemperatureCoolingResult & notes
HEAT TREATMENT GUIDEH13 / 1.2344 / X40CrMoV5-1 Critical points (typical): Ac1 ≈ 860°C, Ac3 ≈ 940°C, Ms ≈ 340°C. Forging: Preheat slowly and uniformly to about 750°C, then heat to 1050–1150°C. Do not forge below 850°C. Cool slowly in a furnace or insulating mediaH13 is air-hardening and will crack if cooled in open air. Soft annealing: 750–800°C, through-heat and hold 2–4 h. Furnace cool at 10–20°C/h to about 600°C, then air cool. Result: ≤229 HB. Stress relieving: 600–650°C, hold at least 2 h after through-heating. Slow furnace cool to 500°C, then air. Carry out after rough machining and before hardening to minimise distortion. Hardening: Preheat in two steps600–650°C and 800–850°C. Austenitise at 1020–1030°C (1000–1050°C range depending on toughness vs hot-strength requirement); soak 30 min after the core reaches temperature. Use vacuum, protective atmosphere or neutral salt bath to prevent decarburisation. Quench in pressurised gas, oil, hot salt bath (500–550°C) or still air for small sections. As-quenched hardness: typically 52–56 HRC. Tempering: Temper immediately when the tool reaches 50–70°C. Minimum two tempers (three for die-casting dies), at least 2 h at temperature each, cooling to room temperature between tempers. Temper at 550–620°C for working hardness 44–52 HRC; avoid finishing at the secondary-hardening peak (~500°C) where toughness is lowest. Typical response: 550°C ≈ 52–54 HRC; 600°C ≈ 48–50 HRC (typical — confirm against the mill tempering curve). Pre-hardened supply: Produced by hardening and tempering at approximately 600–620°C to 44–48 HRC. Nitriding: Gas or plasma nitriding at 510–530°C, or nitrocarburising (salt bath or gas) at about 570°C for 1–2 h. Surface hardness approximately 950–1000 HV. Nitride after final tempering and at least 25°C below the last tempering temperature to protect core hardness. In-service stress relief: Re-temper die-casting dies periodically at 25–50°C below the last tempering temperature to relieve accumulated thermal stresses and delay heat checking.
ENGINEERING NOTES
Weldability
Poor

H13 is crack-sensitive and welding is normally limited to die and tool repair by experienced tool welders. Preheat to 325–375°C (annealed or hardened material) and hold interpass temperature at or above preheat. Use TIG (GTAW) with an H13-type matching filler for working surfaces; grind out cracks and heat-checked layers completely before welding. Hardened tools: after welding cool to about 70°C, then temper immediately at 25–50°C below the original tempering temperature. Annealed material: cool slowly in the furnace or insulating media, then stress-relieve at 600–650°C or re-anneal before hardening. Not a structural welding grade.

Filler metals
  • H13-type 5%Cr-Mo-V rod · Matching composition / TIG (GTAW)Preferred for die working surfaces — matches base hardness after tempering. No AWS classification; confirm product designation with consumable supplier. [VERIFY]
  • ERNiCrMo-3 · AWS A5.14 / TIG (GTAW)Buffer layer or repair of heat-checked die-casting surfaces; lower hardness than base metal. Confirm with die-repair specialist. [VERIFY]
  • ER312 · AWS A5.9 / TIG (GTAW)Crack repair and buttering on non-working, non-wear areas only — not for die faces.
Machinability
Fair

Best machined in the annealed condition (≤229 HB): coated carbide (ISO P20–P30) for turning and milling, HSS-Co or carbide drills. Leave allowance to remove the decarburised skin on black bar and to correct heat-treatment distortion; stress-relieve at 600–650°C after heavy roughing and before hardening. Pre-hardened 44–48 HRC material requires rigid set-ups, coated carbide or CBN and reduced cutting speeds. EDM is suitable — after EDM, re-temper at 15–25°C below the last tempering temperature to relieve the recast layer.

Applications

  • Die casting dies, inserts, cores and slides for aluminium, zinc and magnesium alloys
  • Aluminium extrusion dies, die holders, bolsters and backers for GCC profile extruders
  • Extrusion press liners, mandrels, dummy blocks and stems for non-ferrous extrusion
  • Hot forging dies and die inserts for oil & gas flanges, fittings and valve bodies
  • Hot upsetting and hot heading tools for bolts, nuts and fasteners
  • Hot shear blades and trimming dies for forging lines and steel mills
  • Shot sleeves, plunger tips and ejector pins in high-pressure die casting machines
  • Plastic injection mould inserts and cores for glass-filled and high-temperature resins
  • Piercing mandrels and punches for seamless tube and hot-forming operations
  • Nitrided extruder screws, barrel liners and hot-work guide components

Frequently Asked Questions

Quick answers on our grades, certification, supply and lead times.

Still have questions?

Our team responds fast with specifications, certification and stock availability.

Contact our team

H13 tool steel is used for hot work tooling that must keep its hardness and resist heat checking under repeated heating and cooling — mainly die casting dies, aluminium extrusion dies and hot forging dies. Typical components include die-casting inserts, cores and shot sleeves for aluminium, zinc and magnesium; extrusion dies, bolsters, liners and mandrels; forging dies for flanges, fittings and valve bodies; hot shear blades; and hot heading tools. Its toughness and polishability also make it a common choice for plastic injection mould inserts running glass-filled or high-temperature resins. In the UAE and GCC, H13 is widely used by aluminium extruders, die casters and forging shops serving the oil & gas sector.

Get in touch