Tool Steel dealers in UAE

1.2714 / 55NiCrMoV7 Hot Work Tool Steel | Supplier in UAE & GCC

1.2714 (55NiCrMoV7) — Ni-Cr-Mo-V hot work die steel with high toughness and deep hardening for hammer and press forging dies, die holders and hot shears.

Industries Served

Mould & Die
Heavy Engineering
Automotive
Manufacturing

Overview

1.2714 hot work tool steel (DIN 1.2714 / 55NiCrMoV7, nearest AISI L6) is a nickel-chromium-molybdenum-vanadium die steel containing 0.50–0.60% carbon, 1.50–1.80% nickel, 0.80–1.20% chromium, 0.35–0.55% molybdenum and 0.05–0.15% vanadium, specified to EN ISO 4957. Nickel gives the toughness and deep hardenability that large forging dies need, while molybdenum resists temper embrittlement and vanadium refines the grain. The result is a steel that takes the repeated impact and thermal cycling of hammer and press forging without cracking. 1.2714 is hardened from 840–880 °C in oil, a warm bath or air and reaches 55–58 HRC as quenched. For forging dies it is normally used at 36–42 HRC, either pre-hardened at the mill or tempered to that range by the toolmaker. It is supplied soft annealed to 248 HB maximum or pre-hardened, for forging dies, die holders, bolsters, hot shear blades and hot punches.

Nifty Alloys supplies 1.2714 / 55NiCrMoV7 hot work die steel from stock in Dubai, UAE, in forged block, round bar and forgings to drawing, annealed or pre-hardened to 36–42 HRC. Blocks are saw-cut to die size, and sizes on hand are confirmed with every quotation. Every order carries an EN 10204 3.1 Mill Test Certificate as standard, confirming chemistry and hardness with full traceability to the producing mill. EN 10204 3.2 third-party inspection is available on request. We deliver across the UAE within 24–48 hours and to Saudi Arabia, Kuwait, Qatar, Oman and Bahrain, and export to Europe, India and Africa. As an ISO 9001:2015 certified tool steel supplier in the UAE, our team supports forging shops choosing between 1.2714, 1.2767 and H13 for their dies. Contact our team to request a quote.

Chemical Composition

0.55 %
C

Carbon

0.5 – 0.6 %

Si

Silicon

0.1 – 0.4 %

Mn

Manganese

0.6 – 0.9 %

P

Phosphorus

≤ 0.03 %

S

Sulfur

≤ 0.03 %

1.1 %
Cr

Chromium

0.8 – 1.2 %

0.5 %
Mo

Molybdenum

0.35 – 0.55 %

1.7 %
Ni

Nickel

1.5 – 1.8 %

0.1 %
V

Vanadium

0.05 – 0.15 %

Typical value Range (min–max) Minimum (≥) Maximum (≤) Hover / tap for notes

Standard

EN ISO 4957

EN

Revision: EN ISO 4957:2018

Tool steels — specification for chemical composition, heat treatment, and properties of tool steels including cold work, hot work, and high-speed grades.

Published as BS EN ISO 4957; leading BS dropped to match house style. European standard governing 1.2379 (X153CrMoV12) and other DIN tool steel grades. Supersedes former DIN 17350 for tool steels. Referenced in European and Middle Eastern engineering procurement. Equivalent German standard: DIN EN ISO 4957.

Available Forms

Forging

Open-die forgings to customer drawing; size and lead time on request.

Plate / Block

20–50 mm. Thickness. Forged block saw-cut to die size. Stocked in Dubai.

Round Bar

20–300 mm. Diameter. Stocked in Dubai — sizes on hand confirmed at enquiry.

Stock & delivery

Stock location
Dubai, UAE
In stock
1.2714 held in Dubai stock in Annealed and Pre-Hardened 36–42 HRC conditions (block and round bar); forgings to drawing on request. Sizes and condition on hand confirmed with each quotation. [VERIFY with sales — which conditions and forms are on the shelf]
Delivery UAE
24–48 hours
Delivery GCC
3–5 working days — Saudi Arabia, Kuwait, Qatar, Oman, Bahrain
Export
Europe, India, Africa on request
Quotation
Same-day quotation
Minimum order
No minimum order quantity for standard sizes

Key standards

EN ISO 4957

Designations & Equivalents

StandardDesignationNotes
EN / Werkstoff1.2714European material number — primary designation
DIN55NiCrMoV7German / EN designation
EN Name55NiCrMoV7EN ISO 4957 steel name
ISO55NiCrMoV7ISO 4957 designation
AISI / SAEL6 (nearest)Nearest AISI type only — L6 has higher carbon (0.65–0.75%) and no specified vanadium
UNST61206 (L6, nearest)UNS number of AISI L6 — nearest type, not identical
ASTMA681 (L6 nearest) — alias onlyMaterial is supplied to EN ISO 4957, not ASTM A681
AMSNoneNo AMS specification applies to 1.2714 — not an aerospace procurement grade
Common NameForging die steel, hammer die steel, 2714 steel, 55NCD7 (AFNOR), 56NiCrMoV7 KU (UNI)Buyer search terms used in UAE / GCC and Europe

Compliance & Certification

StandardStatusNotes
EN 10204 3.1SuitableMill Test Certificate provided as standard. Confirms chemistry and hardness (annealed or pre-hardened) to EN ISO 4957.

Specifications

Mechanical Properties

Values per EN ISO 4957. Bar length compares conditions within each row.

PropertyAnnealed | EN ISO 4957Pre-Hardened 36–42 HRC | EN ISO 4957
Hardness (annealed)248 HBmaxSurface, as suppliedMax per EN ISO 4957.–
Tensile Strength (UTS)–Room tempNot specified for annealed tool steel — leave blank.1230 MPatypicalRoom tempApproximate conversion from 36–42 HRC (about 1130–1330 MPa); one producer quotes 1200–1400 MPa for 355–415 HB. Typical, not specified.
Yield Strength (0.2% Proof Stress)–Room tempNot specified — leave blank.–Room temp[VERIFY — source not confirmed]. Leave blank until mill data available.
Elongation–Not specified — leave blank.–[VERIFY — source not confirmed]. Leave blank until mill data available.
Hardness (as quenched)55–58 HRC840–880 °C, oil / warm bath / airTypical range — producer data, depends on section and quench. Not a specified value.–
Hardness–36–42 HRCTypical 39 HRCSurface, as suppliedSupply condition per metallurgist brief. Typical value mid-range.
Impact Energy (Charpy)––[VERIFY — source not confirmed]. Producers describe toughness qualitatively only.

Physical Properties

PropertyAnnealed | EN ISO 4957Pre-Hardened 36–42 HRC | EN ISO 4957
Densityat 20°C–[VERIFY — source not confirmed]. Leave blank until confirmed.–[VERIFY — source not confirmed]. Leave blank until confirmed.
Modulus of Elasticityat 20°C–[VERIFY — source not confirmed]. Leave blank until confirmed.–[VERIFY — source not confirmed]. Leave blank until confirmed.
Thermal Conductivityat 20°C35.9 W/m·K35.9 W/m·K
Coefficient of Thermal Expansionat 20–100°C12.3 µm/m·°C12.3 µm/m·°C
Specific Heat Capacityat 20°C–[VERIFY — source not confirmed]. Leave blank until confirmed.–[VERIFY — source not confirmed]. Leave blank until confirmed.
Melting Point / Rangeat Solidus–[VERIFY — source not confirmed]. Leave blank until confirmed.–[VERIFY — source not confirmed]. Leave blank until confirmed.

Service Conditions

Service Temperature

Notes

Forging dies must be preheated before use and must stay below their final tempering temperature in service, or they will soften. 1.2714 has high toughness but only moderate hot hardness and temper resistance — it suits hammer and press dies with short contact times. For long contact times, high die temperatures, die casting or extrusion dies, choose H13 / 1.2344 or H11 / 1.2343. Die preheat temperature to be agreed with the forge [VERIFY — source not confirmed].

Corrosion Performance

General corrosion

No corrosion resistance. Dies and blocks rust in humid UAE and GCC conditions and when water or graphite-water lubricants are used. Oil dies between campaigns and store blocks under cover.

Pitting resistance

No pitting resistance.

Additional notes

Not applicable — low-alloy hot work die steel.

Heat Treatment

ProcessTemperatureCoolingResult & notes
HEAT TREATMENT GUIDE1.2714 / 55NiCrMoV7: Forging: Preheat slowly to about 700 °C, then heat to 1050 °C. Do not forge below 800 °C. Cool slowly in a furnace or insulating medium, then anneal. Soft Annealing: 650–710 °Cabout 4 hslow furnace cooling — max 248 HB. (One source gives 740–760 °C with cooling at max 10 °C/h to 600 °C.) Stress Relieving: 600–650 °C — about 2 h per 25 mm ruling section — furnace cool to 500 °C, then air. After rough machining, before finish machining and hardening. Preheating: 600–700 °C before hardening. Hardening: Austenitise at 840–880 °C (850 °C normal) — quench in oil, a 160–250 °C warm bath, pressurised gas or air. As-quenched hardness 55–58 HRC depending on section and quench. Tempering: Temper immediately. About 2 h per 25 mm ruling section; double temper recommended. Typical hardness after tempering: 200 °C — 55 HRC; 250 °C — 54 HRC; 300 °C — 53 HRC; 400 °C — 49 HRC; 500 °C — 45 HRC. Forging dies are tempered higher to 36–42 HRC for toughness — use the mill tempering diagram for the exact temperature. Pre-Hardened 36–42 HRC: Supplied hardened and tempered at the mill. Machine directly; no further hardening needed. Nitriding: Temper about 50 °C above the nitriding temperature first. Typical case depths at 525 °C: 20 h — 0.25 mm; 30 h — 0.30 mm; 60 h — 0.40 mm. Post-weld: Re-temper below the original tempering temperature.
ENGINEERING NOTES
Weldability
Fair

Repair welding of forging dies in 1.2714 is common practice, but it needs strict control: preheat the whole die, hold interpass at or above preheat, use low-hydrogen practice and cool slowly in an insulating medium [VERIFY — preheat range to be confirmed from producer welding data]. Pre-hardened dies should be re-tempered after welding at a temperature below the original tempering temperature. Annealed material should be stress relieved at 600–650 °C. Ask us before welding a hardened die.

Filler metals
  • ER312 · AWS A5.9 / TIG (GTAW)Buffer (buttering) layer on the die before hard build-up. Not a matching-hardness deposit.
  • Ni-Cr-Mo hot work matching consumable, 38–45 HRC deposit · Hot work die repair rod / TIG or SMAWFor impression and edge build-up on forging dies. [VERIFY — consumable code and classification to be confirmed with consumable supplier]
Machinability
Good

Annealed (≤248 HB): machines well with carbide or HSS. Pre-hardened (36–42 HRC): die-sinking and milling with coated carbide at reduced speed — the main advantage of pre-hardened supply is that no hardening or distortion follows machining. Stress relieve annealed blocks at 600–650 °C after heavy rough machining. EDM is used for die impressions; remove the white layer and re-temper after heavy EDM.

Applications

  • Hammer forging dies for drop forging of steel components
  • Press forging dies for flanges, fittings and valve bodies for GCC oil & gas
  • Die holders, bolsters and backers for aluminium extrusion presses in UAE plants
  • Hot shear blades for cutting billets and bars in forging shops
  • Hot punches, piercing tools and trimming dies for forgings
  • Upsetting and heading dies for bolts and studs
  • Embossing, coining and forming dies under heavy impact
  • Die inserts and anvils nitrided after high-temperature tempering
  • Large forged die blocks where through-hardening and toughness are needed
  • Plastic mould bases and frames where surface demands are low

Related grades in Tool Steel

Frequently Asked Questions

Quick answers on our grades, certification, supply and lead times.

Still have questions?

Our team responds fast with specifications, certification and stock availability.

Contact our team

1.2714 steel (55NiCrMoV7) is used mainly for hot forging dies that must survive repeated impact and thermal cycling. Typical uses are hammer and press forging dies, die holders, bolsters and backers, hot shear blades for billets, hot punches and trimming dies, upsetting dies and heavy embossing tools. Used at 36–42 HRC, its nickel-chromium-molybdenum chemistry gives high toughness through large die blocks. In the UAE and GCC it is widely used by forging shops producing flanges, fittings and valve bodies, and by aluminium extrusion plants for die holders and bolsters.

Get in touch