Alloy Steel dealers in UAE

AISI 4330V / 4330 Mod Alloy Steel | Supplier in UAE & GCC

AISI 4330V / 4330 Mod — vanadium-modified Ni-Cr-Mo steel with deep hardenability and low-temperature toughness; API 6A 75K bodies, AMS 6427 aerospace parts.

Industries Served

Oil & Gas
Aerospace & Defence
Heavy Engineering
Manufacturing

Overview

AISI 4330V (4330 Mod, UNS K23080) is a vanadium-modified nickel-chromium-molybdenum alloy steel supplied quenched and tempered to API Spec 6A material designations for wellhead and tree equipment, and to AMS 6427 (aircraft quality) or AMS 6411 (vacuum remelted) for aerospace. Its about 0.30% carbon keeps toughness and weldability ahead of higher-carbon grades, 1.65–2.00% nickel lowers the impact transition temperature, chromium and 0.40–0.50% molybdenum give deep hardenability, and a 0.05–0.10% vanadium addition refines grain and resists softening during tempering. The result is a steel that through-hardens large forgings and holds Charpy toughness at sub-zero temperatures — quenched and tempered to API 6A 75K it meets 517 MPa minimum yield and 655 MPa minimum tensile, and it can be heat treated far higher for oil tools and aircraft parts. Because it contains more than 1% nickel, 4330V is not pre-qualified for sour service under NACE MR0175 / ISO 15156-2 and needs Annex B qualification for H2S duty. There is no exact European equivalent.

Nifty Alloys supplies AISI 4330V / 4330 Mod from stock in Dubai, UAE, in round bar and forgings, quenched and tempered to API 6A 75K as standard, with 80K non-standard, higher-strength oil-tool conditions and normalised and tempered material on request. Bars are ultrasonically tested, cut to length and dispatched with EN 10204 3.1 Mill Test Certificates as standard, reporting chemistry, tensile, Charpy impact and hardness results with full traceability to the mill; EN 10204 3.2 third-party inspection, API 6A PSL 3 / 4 testing and AMS 6427 / AMS 6411 supply are available on request. We deliver across the UAE within 24–48 hours, to Saudi Arabia, Kuwait, Qatar, Oman and Bahrain within 3–5 working days, and export to Europe, India and Africa. Send your size, PSL and temperature class to request a quote — quotations are turned around the same day.

Chemical Composition

0.32 %
C

Carbon

0.3 – 0.34 %

Si

Silicon

0.15 – 0.35 %

Mn

Manganese

0.75 – 1 %

1.8 %
Ni

Nickel

1.65 – 2 %

0.88 %
Cr

Chromium

0.75 – 1 %

0.42 %
Mo

Molybdenum

0.4 – 0.5 %

0.08 %
V

Vanadium

0.05 – 0.1 %

P

Phosphorus

≤ 0.025 %

S

Sulfur

≤ 0.01 %

Typical value Range (min–max) Minimum (≥) Maximum (≤) Hover / tap for notes

Standard

API Spec 6A

Other

Revision: API Spec 6A — current edition

Specification for Wellhead and Tree Equipment — defines material designations (36K, 45K, 60K, 75K), product specification levels (PSL 1–4) and temperature classes for pressure-containing bodies.

4130 Q&T at ≤22 HRC is widely supplied against the 75K material designation (YS ≥517 MPa, UTS ≥655 MPa, El ≥17%, RA ≥35%). 80K material exceeds 75K tensile requirements; PSL and temperature class must be stated on the order. Also published as ISO 10423.

Available Forms

Forging

200–1000 mm. Forged bars, blocks and rings to order. [VERIFY — stock range not confirmed]

Round Bar

50–400 mm. Diameter, Q&T API 6A 75K, UT tested. [VERIFY — stock range not confirmed]

Stock & delivery

Stock location
Dubai, UAE
In stock
Quenched & Tempered to API 6A 75K — standard stocked condition. 80K non-standard, higher-strength oil-tool conditions, normalised and tempered, AMS 6427 / AMS 6411 and NACE Annex B-qualified material on request.
Delivery UAE
24–48 hours
Delivery GCC
3–5 working days — Saudi Arabia, Kuwait, Qatar, Oman, Bahrain
Export
Europe, India, Africa on request
Quotation
Same-day quotation
Minimum order
No minimum order quantity for standard sizes

Key standards

API Spec 6A

Designations & Equivalents

StandardDesignationNotes
AISI / SAE4330V / 4330 Mod / 4330MPrimary designations — vanadium-modified 4330
UNSK23080Unified Numbering System
AMSAMS 6427Aircraft-quality bars, forgings and tubing (4330 Mod)
AMSAMS 6411Vacuum-remelted bars, forgings and tubing (4330 Mod)
Common NameAPI Spec 6A 75K(API) Standard wellhead material designation; 80K = non-standard per purchaser
ASTMA29 / A29MGeneral bar requirements only
DIN30CrNiMo8 / 1.6580 — nearest onlyHigher Cr and Ni, no V — not an equivalent
DIN34CrNiMo6 / 1.6582 — nearest onlyHigher Cr, lower Mo, no V — not an equivalent
Common Name4330V Q&T / 4330 Mod 75K / NiCrMoV steel / wellhead steel / oil tool steelBuyer search terms

Compliance & Certification

StandardStatusNotes
EN 10204 3.1SuitableProvided as standard — chemistry, tensile, Charpy impact and hardness.
EN 10204 3.2ConditionalAvailable on request with independent third-party inspection — specify at order stage.
NACE MR0175 / ISO 15156Requires ConfirmationNot pre-qualified: ISO 15156-2 A.2.1.2 limits carbon and low-alloy steels to < 1% Ni, and 4330V contains 1.65–2.00% Ni. Sour-service supply requires SSC qualification under ISO 15156-2 Annex B for the heat and application, plus 22 HRC maximum hardness. Confirm qualification data at enquiry.
NACE MR0103Requires ConfirmationMR0103 does not apply the 1% Ni restriction; hardness and condition compliance to be confirmed at order stage.
API Spec 6A PSL 3 / 4Conditional75K standard designation (or 80K NS per purchaser) with PSL 3 / 4 impact, hardness and NDE testing on request — state PSL, material class and temperature class.
AMS 6427 / AMS 6411ConditionalSupplied on request as aircraft-quality or vacuum-remelted 4330 Mod — confirm revision and condition.

Specifications

Mechanical Properties

Values per API Spec 6A. Bar length compares conditions within each row.

PropertyQ&T 75K | API Spec 6ANormalised & Tempered | AMS 6427
Tensile Strength (UTS)655 MPamin75K — QTC per API 6AAPI 6A minimum (95 ksi).–
Yield Strength (0.2% Proof Stress)517 MPamin75K — QTC per API 6AAPI 6A minimum (75 ksi).–
Yield Strength (0.2% Proof Stress)552 MPamin80K non-standard (NS)Purchaser / manufacturer specification (80 ksi) — not an API standard designation.–
Elongation17 %min75K — 50 mm gaugeAPI 6A minimum; NS materials 15% min.–
Reduction of Area35 %min75KAPI 6A minimum; NS materials 20% min.–
Impact Energy (Charpy V-notch)20 JminAt temperature class, averageAPI 6A PSL 2–4 typical requirement (20 J average / 15 J single) — confirm per PSL and class.–
Hardness197–237 HB75K197 HB API 6A minimum for 75K [VERIFY — not confirmed]; 237 HB (22 HRC) maximum applies only to sour-service supply.–As suppliedMaximum per AMS 6427 / mill specification, reported on MTC [VERIFY — AMS supply-condition limit not confirmed].

Physical Properties

PropertyQ&T 75K | API Spec 6ANormalised & Tempered | AMS 6427
Densityat 20°C7.85 g/cm³7.85 g/cm³
Modulus of Elasticityat 20°C205 GPa205 GPa
Thermal Conductivityat 20°C38 W/m·K38 W/m·K
Coefficient of Thermal Expansionat 20–100°C12.3 µm/m·°C12.3 µm/m·°C

Service Conditions

Service Temperature

Min -46 °CMax 400 °C

Notes

[VERIFY — maxServiceTempC 400: continuous load-bearing limit not confirmed in a code source] Nickel gives good sub-zero toughness: 4330V is routinely Charpy-tested for API 6A temperature classes down to K (-60°C) and L (-46°C) when specified; the minimum shown assumes impact testing at the required class. API 6A equipment temperature classes run up to 121°C (classes U / V). Avoid prolonged service in the 350–550°C temper-embrittlement range and never exceed the tempering temperature.

Corrosion Performance

General corrosion

Corrodes in brine, CO2 and humid coastal atmospheres without protection. Higher-strength conditions are susceptible to hydrogen embrittlement and, in H2S, to sulphide stress cracking — sour-service use requires NACE Annex B qualification and hardness control.

Pitting resistance

No pitting resistance. Wellhead and valve components are protected by coatings, corrosion-resistant overlays (for example Alloy 625 weld cladding) or inhibitors where wetted by produced fluids.

Additional notes

Not applicable — low-alloy steel.

Heat Treatment

HEAT TREATMENT GUIDE — AISI 4330V / 4330 Mod / UNS K23080

Forging: start about 1150–1200°C, finish above about 850°C; cool slowly. Normalising: about 870–925°C — air cool — refines grain before hardening [VERIFY — range not confirmed]. Hardening: 850–880°C — soak through section — quench in water, polymer or oil depending on section and distortion risk. Tempering: 600–650°C for API 6A 75K / 80K strength — air cool; lower tempering temperatures give higher-strength oil-tool and aerospace conditions. Temper immediately after quenching. Sour-service parts: final hardness 22 HRC maximum, verified per ISO 15156-2, plus Annex B qualification. Stress relieving: below the final tempering temperature after heavy machining; PWHT at 620°C minimum for sour-service weldments. API 6A PSL 3 / 4: heat-treat and test using a qualification test coupon (QTC) representative of the part section.

ENGINEERING NOTES
Weldability
Fair

Weldable with strict controls — lower carbon than 4340 or 4145 helps, but nickel, chromium and molybdenum give high hardenability and a crack-prone HAZ. Use a qualified procedure: preheat to about 200–315°C [VERIFY — preheat range not confirmed], maintain interpass, use dry low-hydrogen consumables, cool slowly and post-weld heat treat below the tempering temperature. For sour-service parts, ISO 15156-2 requires PWHT at 620°C minimum for low-alloy steels and weld deposits with less than 1% nickel unless separately qualified.

Filler metals
  • E10018-M · AWS A5.5 / SMAWLow-hydrogen high-strength electrode for near-matching joints; Ni content > 1% — not for sour service without qualification
  • ER100S-1 · AWS A5.28 / TIG / MIGHigh-strength wire for near-matching joints; preheat and PWHT required
  • E8018-B2 · AWS A5.5 / SMAWCr-Mo electrode with < 1% Ni — under-matching option where sour-service weld chemistry is required
Machinability
Fair

Machines best in the normalised and tempered condition. Q&T 75K material (about 197–237 HB) machines readily with carbide tooling; higher-strength oil-tool conditions need rigid set-ups and hardened-steel carbide grades at reduced speeds. Allow for distortion and scale removal if hardening after rough machining.

Applications

  • API 6A valve bodies, bonnets and end connections for GCC wellhead and tree equipment
  • Tubing and casing hangers, mandrels and tubing-head adaptors
  • Valve stems, gate and seat components in high-pressure wellhead valves
  • Drilling jars, MWD collars, subs and downhole tool bodies needing high toughness
  • Frac-pump fluid-end and high-pressure manifold components
  • BOP and pressure-control equipment parts for onshore and offshore rigs
  • Aircraft landing-gear parts, actuators and structural fittings (AMS 6427 / 6411)
  • High-strength aerospace bolting and airframe components
  • Low-temperature service shafts and couplings needing sub-zero impact toughness
  • Heavy-duty forgings and tool bodies for heavy engineering

Frequently Asked Questions

Quick answers on our grades, certification, supply and lead times.

Still have questions?

Our team responds fast with specifications, certification and stock availability.

Contact our team

AISI 4330V is used for API 6A wellhead and tree equipment — valve bodies, bonnets, hangers and end connections — and for high-toughness oil tools such as drilling jars, MWD collars and frac-pump components. In aerospace it is supplied to AMS 6427 and AMS 6411 for landing-gear parts and structural fittings. In the UAE and GCC, wellhead manufacturers and oil-tool shops buy 4330V Q&T bar and forgings to API 6A 75K.

Get in touch