Alloy Steel dealers in UAE

AISI 4340 / EN24 / 817M40 / 34CrNiMo6 Alloy Steel | Supplier in UAE & GCC

AISI 4340 / EN24 (817M40, 34CrNiMo6) — 1.5% Ni-Cr-Mo through-hardening steel: EN24T 850–1000 MPa in sections to 250 mm; shafts, gears and oilfield tools.

Industries Served

Oil & Gas
Aerospace & Defence
Automotive
Heavy Engineering
Power Generation
Manufacturing
Mining

Overview

AISI 4340 / EN24 (BS 970 817M40, DIN 34CrNiMo6 / 1.6582, UNS G43400) is a nickel-chromium-molybdenum through-hardening alloy steel, supplied in Europe to EN ISO 683-2 (formerly EN 10083-3), in the US to ASTM A29 chemistry and, for aerospace, as genuine 4340 to AMS 6415. EN24 contains about 0.40% carbon, 1.3–1.7% nickel, 1.0–1.4% chromium and 0.2–0.35% molybdenum: nickel raises toughness and lowers the impact transition temperature, chromium and molybdenum give deep hardenability, and molybdenum suppresses temper embrittlement. As a result EN24 holds high strength through heavy sections — Condition T (EN24T, 850–1000 MPa, 248–302 HB) is guaranteed up to a 250 mm limiting ruling section, and higher conditions reach 1000–1150 MPa in sections up to 63 mm. The three designations are close but not identical in carbon, nickel and chromium, so the mill certificate states which was supplied. EN24 is the default choice for heavily loaded shafts, gears, crankshafts, high-tensile studs and oilfield tool bodies where 4140 / EN19 lacks section capability or toughness.

Nifty Alloys supplies AISI 4340 / EN24 / 817M40 alloy steel from stock in Dubai, UAE, in round bar, flat bar, plate / block and forgings, in the hardened and tempered EN24T condition as standard, with Condition U / V and annealed material on request. Material is cut to length and dispatched with EN 10204 3.1 Mill Test Certificates as standard, stating chemistry, condition, tensile, impact and hardness results with full traceability to the mill; EN 10204 3.2 third-party inspection and AMS 6415 aircraft-quality 4340 are available on request. We deliver across the UAE within 24–48 hours, to Saudi Arabia, Kuwait, Qatar, Oman and Bahrain within 3–5 working days, and export to Europe, India and Africa. Send your size list or drawing to request a quote — quotations are turned around the same day.

Chemical Composition

0.4 %
C

Carbon

0.36 – 0.44 %

Si

Silicon

0.1 – 0.4 %

Mn

Manganese

0.45 – 0.7 %

1.5 %
Ni

Nickel

1.3 – 1.7 %

1.2 %
Cr

Chromium

1 – 1.4 %

0.25 %
Mo

Molybdenum

0.2 – 0.35 %

P

Phosphorus

≤ 0.035 %

S

Sulfur

≤ 0.04 %

Typical value Range (min–max) Minimum (≥) Maximum (≤) Hover / tap for notes

Standard

EN ISO 683-2

EN

Revision: EN ISO 683-2:2018

Heat-treatable steels, alloy steels and free-cutting steels — Part 2: Alloy steels for quenching and tempering.

European standard governing 25CrMo4 (1.7218). Defines chemical composition, mechanical properties per condition, and delivery requirements. Replaces former EN 10083-1.

Available Forms

Flat Bar

10–150 mm. Thickness; width × thickness to order. [VERIFY — stock range not confirmed]

Forging

200–1000 mm. Forged bars, rings and blocks to order. [VERIFY — stock range not confirmed]

Plate / Block

10–200 mm. Thickness; blocks saw-cut to size. [VERIFY — stock range not confirmed]

Round Bar

16–500 mm. Diameter, EN24T. Condition T guaranteed to 250 mm ruling section; larger sizes at reduced core properties. [VERIFY — stock range not confirmed]

Stock & delivery

Stock location
Dubai, UAE
In stock
Q&T Condition T (EN24T) — standard stocked condition. Condition U / V and annealed (+A) on request. AMS 6415 aircraft-quality 4340 on request.
Delivery UAE
24–48 hours
Delivery GCC
3–5 working days — Saudi Arabia, Kuwait, Qatar, Oman, Bahrain
Export
Europe, India, Africa on request
Quotation
Same-day quotation
Minimum order
No minimum order quantity for standard sizes

Key standards

EN ISO 683-2

Designations & Equivalents

StandardDesignationNotes
AISI / SAE4340US designation — ASTM A29 chemistry (0.38–0.43 C, 1.65–2.00 Ni, 0.70–0.90 Cr)
UNSG43400Unified Numbering System
BSEN24 / EN24TOriginal BS 970:1955 designation; "T" = Condition T (850–1000 MPa)
BS817M40 / 817M40TBS 970 designation (withdrawn standard) — primary chemistry on this page
DIN34CrNiMo6EN ISO 683-2 (formerly EN 10083-3) — 0.30–0.38 C, 1.30–1.70 Cr
EN / Werkstoff1.658234CrNiMo6 material number
DIN36CrNiMo4 / 1.6511Lower-nickel related grade — aliases only, not an equivalent
Common Name35NCD6(AFNOR) French designation
JISSNCM439 / SNCM447Japanese Industrial Standard
Common Name40CrNiMo(GB) Chinese designation
AMSAMS 6415SAE 4340 aircraft-quality bars, forgings and tubing — requires 4340 chemistry
ASTMA29 / A29MChemistry standard for 4340 bar
Common NameEN24T / high tensile steel / NiCrMo steel / 4340 round bar / aircraft steelBuyer search terms

Compliance & Certification

StandardStatusNotes
EN 10204 3.1SuitableProvided as standard — chemistry (817M40, 4340 or 34CrNiMo6 as supplied), condition, tensile, impact and hardness.
EN 10204 3.2ConditionalAvailable on request with independent third-party inspection — specify at order stage.
NACE MR0175 / ISO 15156Not Applicable — Not acceptable under ISO 15156-2 general requirements: carbon and low-alloy steels must contain less than 1% nickel, and EN24 / 4340 contain 1.3–2.0%. Use only if separately qualified for the project (ISO 15156-2 Annex B); for sour service consider 4130 / 4140 at ≤ 22 HRC.
NACE MR0103Requires ConfirmationConfirm against the project refinery sour-service requirements at order stage.
AMS 6415ConditionalAvailable only as genuine SAE 4340 aircraft-quality material on request — not met by EN24 / 34CrNiMo6 stock.

Specifications

Mechanical Properties

Values per EN ISO 683-2. Bar length compares conditions within each row.

PropertyQ&T Condition T (EN24T) | EN ISO 683-2Annealed (+A) | EN ISO 683-2Q&T Condition U / V | EN ISO 683-2
Tensile Strength (UTS)850–1000 MPa817M40T — up to 250 mmBS 970 Condition T range (reference).–925–1075 MPa817M40U — over 29 to 100 mmBS 970 reference.
Tensile Strength (UTS)900–1100 MPa34CrNiMo6 +QT — 100 to 160 mmEN ISO 683-2 range; 800–950 MPa at 160–250 mm.–1000–1150 MPa817M40V — over 13 to 63 mmBS 970 reference.
Tensile Strength (UTS)––1100–1300 MPa34CrNiMo6 +QT — 16 to 40 mmEN ISO 683-2; 1200–1400 MPa up to 16 mm, 1000–1200 MPa at 40–100 mm.
Yield Strength (ReH)680 MPamin817M40T — over 63 to 150 mmBS 970 reference; 650 MPa min over 150–250 mm.–755 MPamin817M40UBS 970 reference; Condition V: 850 MPa min.
Yield Strength (0.2% Proof Stress)700 MPamin34CrNiMo6 +QT — 100 to 160 mmEN ISO 683-2 minimum; 600 MPa at 160–250 mm.–900 MPamin34CrNiMo6 +QT — 16 to 40 mmEN ISO 683-2; 1000 MPa up to 16 mm, 800 MPa at 40–100 mm.
Elongation13 %min817M40T — A (5.65√So)BS 970 reference. 34CrNiMo6: 12% (100–160 mm), 13% (160–250 mm).–12 %min817M40U / V — A (5.65√So)BS 970 reference. 34CrNiMo6: 9–11% by size.
Reduction of Area55 %min34CrNiMo6 +QT — 100 to 250 mmEN ISO 683-2 minimum.––
Impact Energy (Charpy V-notch)50 Jmin817M40T — over 63 to 150 mm, room tempBS 970 reference KCV; 35 J over 150–250 mm. 34CrNiMo6: 45 J (KV, +20°C).–42 Jmin817M40U / V — room tempBS 970 reference KCV. 34CrNiMo6: 45 J (16–100 mm).
Hardness248–302 HB817M40TBS 970 reference (about 25–32 HRC).248 HBmaxSoft annealed (+A)EN ISO 683-2 maximum for 34CrNiMo6.269–331 HB817M40UBS 970 reference; Condition V: 293–352 HB.

Physical Properties

PropertyQ&T Condition T (EN24T) | EN ISO 683-2Annealed (+A) | EN ISO 683-2Q&T Condition U / V | EN ISO 683-2
Densityat 20°C7.85 g/cm³7.85 g/cm³7.85 g/cm³
Modulus of Elasticityat 20°C210 GPa210 GPa210 GPa
Thermal Conductivityat 20°C42.6 W/m·K42.6 W/m·K42.6 W/m·K
Coefficient of Thermal Expansionat 20°C12.3 µm/m·°C12.3 µm/m·°C12.3 µm/m·°C
Specific Heat Capacityat 20°C470 J/kg·K470 J/kg·K470 J/kg·K
Electrical Resistivityat 20°C0.19 µΩ·m0.19 µΩ·m0.19 µΩ·m

Service Conditions

Service Temperature

Min -40 °CMax 400 °C

Notes

[VERIFY — maxServiceTempC 400: continuous load-bearing limit not confirmed in a code source] Nickel gives good low-temperature toughness: 34CrNiMo6 +QT is typically certified at 40 J min at -40°C (KV) when specified — state the impact temperature on the order. Do not use quenched-and-tempered material at or near its tempering temperature, and avoid prolonged service in the 350–550°C temper-embrittlement range. Not a creep-resisting grade.

Corrosion Performance

General corrosion

Chromium and nickel give only slightly better atmospheric resistance than carbon steel. Unsuitable for seawater, chloride or acidic service without coating. High-strength conditions (U / V and above) are susceptible to hydrogen embrittlement from plating or cathodic protection — bake after electroplating.

Pitting resistance

No pitting resistance. Rusts in humid and coastal atmospheres typical of the UAE and GCC; protect with oil, paint, phosphate, nitriding or hard chrome plating.

Additional notes

Not applicable — low-alloy steel.

Heat Treatment

HEAT TREATMENT GUIDE — AISI 4340 / 34CrNiMo6 / EN24

Forging: start about 1150–1200°C, finish above about 850°C; cool slowly in the furnace or in ash. Soft annealing: 650–700°C — furnace cool — max 248 HB (+A). Hardening: 830–860°C — soak to uniform temperature — quench in oil or polymer. Temper immediately. Tempering: 540–680°C — 1 h per 25 mm minimum — air cool; tempering temperature selects the condition (lower for V, higher for T). Avoid tempering in the 250–400°C range (tempered-martensite embrittlement). Strength by section: Condition T (850–1000 MPa) to 250 mm; U (925–1075 MPa) to 100 mm; V (1000–1150 MPa) to 63 mm — BS 970 limiting ruling sections. EN ISO 683-2 34CrNiMo6 +QT: 1200–1400 MPa up to 16 mm falling to 800–950 MPa at 160–250 mm. Surface hardening: induction or flame hardening to at least 50 HRC; gas or salt-bath nitriding of EN24T gives a hard, wear-resistant case — temper the core above the nitriding temperature first. Stress relieving: about 50°C below the last tempering temperature after heavy machining.

ENGINEERING NOTES
Weldability
Poor

Difficult to weld — high carbon equivalent and deep hardenability make the heat-affected zone prone to martensite and hydrogen cracking. Avoid welding wherever possible. If unavoidable: weld in the annealed condition, preheat to about 300–350°C [VERIFY — preheat range not confirmed] and hold interpass at preheat, use dry low-hydrogen consumables, cool slowly, and immediately stress relieve or re-harden and temper. Welding EN24T reduces the HAZ to an uncontrolled hardness and strength.

Filler metals
  • E11018-M · AWS A5.5 / SMAWLow-hydrogen high-strength electrode for near-matching strength; bake per manufacturer
  • ER120S-1 · AWS A5.28 / TIG / MIGHigh-strength wire for near-matching joints; preheat and PWHT essential
  • E8018-B2 · AWS A5.5 / SMAWUnder-matching repair electrode where joint strength below parent is acceptable
Machinability
Good

Machines well in Condition T (248–302 HB) with carbide tooling — one reason EN24T is stocked pre-hardened. Annealed material (max 248 HB) is easier for heavy roughing before heat treatment. Condition U / V (up to 352 HB) needs rigid set-ups, carbide grades for hardened steel and reduced speeds. Allow for distortion and scale removal if hardening after machining.

Applications

  • Heavy-duty drive shafts, propeller shafts and pinion shafts in large sections
  • Gears, gear blanks and crown wheels for mining and industrial gearboxes
  • Crankshafts, connecting rods and axles for engines and heavy vehicles
  • High-tensile studs, bolts and tie rods for GCC process plant and structures
  • Oilfield tool bodies, subs, crossovers and non-sour downhole components
  • Hydraulic cylinder rods, rams and pistons under high load
  • Aircraft landing-gear parts and structural fittings (AMS 6415 4340)
  • Spindles, arbors and machine-tool components needing toughness
  • Die holders, bolsters and pressure plates in forging and press shops
  • Nitrided or induction-hardened wear parts with a tough core
  • Couplings and torque-transmitting parts for power generation equipment

Related grades in Alloy Steel

Frequently Asked Questions

Quick answers on our grades, certification, supply and lead times.

Still have questions?

Our team responds fast with specifications, certification and stock availability.

Contact our team

EN24 / AISI 4340 is used for heavily loaded parts that need high strength and toughness through large sections: drive and pinion shafts, gears, crankshafts, axles, high-tensile studs, hydraulic rods and oilfield tool bodies. In the EN24T condition it gives 850–1000 MPa tensile strength in sections up to 250 mm. In the UAE and GCC it is widely ordered for gearbox and pump shafts, heavy machinery repairs and non-sour oilfield components.

Get in touch

Elevateyourprojectswithoursuperiorsteel