Alloy Steel dealers in UAE

X120Mn12 / 1.3401 / Hadfield Manganese Steel | Supplier in UAE & GCC

X120Mn12 / 1.3401 Hadfield — austenitic 12% Mn wear steel: about 200 HB as quenched, work-hardens to about 500 HB under impact; tough and non-magnetic.

Industries Served

Mining
Construction
Heavy Engineering
Manufacturing
Power Generation

Overview

X120Mn12 (material number 1.3401), universally known as Hadfield or 12–14% manganese steel, is an austenitic wear-resistant steel containing 1.10–1.30% carbon and 12.0–13.0% manganese. Manganese stabilises austenite at room temperature, so after solution annealing at about 1000–1050°C and water quenching the steel is fully austenitic, tough and ductile at roughly 200 HB. Its defining property is work hardening: under repeated impact and high-stress abrasion the surface transforms and hardens to around 500 HB while the core stays tough, so worn surfaces continually renew their hardness and the part resists cracking under shock. It is essentially non-magnetic. Hadfield steel performs best where impact accompanies wear — crusher jaws and hammers, mill liners, excavator and dragline buckets, grizzly bars, rail crossings and security bars — and is less effective under low-stress sliding abrasion without impact. Wrought X120Mn12 has no product standard specifying mechanical properties; it is supplied to 1.3401 chemistry, and ASTM A128 is a castings standard used only as a chemistry reference.

Nifty Alloys supplies X120Mn12 / 1.3401 Hadfield manganese steel from stock in Dubai, UAE, in plate, flat bar and round bar, solution annealed and water quenched, with profile cutting on request. Every supply is dispatched with EN 10204 3.1 Mill Test Certificates as standard, certifying chemistry, delivery condition and hardness with full traceability to the mill; EN 10204 3.2 third-party inspection is available on request. We deliver across the UAE within 24–48 hours, to Saudi Arabia, Kuwait, Qatar, Oman and Bahrain within 3–5 working days, and export to Europe, India and Africa for quarry, mining, cement and recycling operations. Send your plate sizes, profiles or drawings to request a quote — quotations are turned around the same day.

Chemical Composition

1.2 %
C

Carbon

1.1 – 1.3 %

12.5 %
Mn

Manganese

12 – 13 %

Si

Silicon

0.3 – 0.5 %

P

Phosphorus

≤ 0.1 %

S

Sulfur

≤ 0.04 %

Cr

Chromium

≤ 1.5 %

Ni

Nickel

≤ 1 %

Typical value Range (min–max) Minimum (≥) Maximum (≤) Hover / tap for notes

Standard

Stahl-Eisen-Liste (SEL)

Other

Revision: Stahl-Eisen-Liste — current edition

German register of steel designations and material numbers. Lists X120Mn12 under material number 1.3401 (austenitic high-manganese steel) with its chemical composition.

Designation reference — not a product standard with mechanical requirements. Wrought X120Mn12 plate and bar are supplied to 1.3401 chemistry, solution annealed and water quenched, with properties per producer data.

Available Forms

Plate / Block

6–50 mm. Thickness; profile cut to drawing. [VERIFY — stock range not confirmed]

Flat Bar

6–50 mm. Thickness; cut from plate or rolled flats. [VERIFY — stock range not confirmed]

Round Bar

20–150 mm. Diameter, forged or rolled. [VERIFY — stock range not confirmed]

Stock & delivery

Stock location
Dubai, UAE
In stock
Solution Annealed & Water Quenched — only supply condition. Profile cutting on request.
Delivery UAE
24–48 hours
Delivery GCC
3–5 working days — Saudi Arabia, Kuwait, Qatar, Oman, Bahrain
Export
Europe, India, Africa on request
Quotation
Same-day quotation
Minimum order
No minimum order quantity for standard sizes; cut pieces available

Key standards

Stahl-Eisen-Liste (SEL)

Designations & Equivalents

StandardDesignationNotes
DINX120Mn12Steel name — primary designation
EN / Werkstoff1.3401Material number (Stahl-Eisen-Liste)
Common NameHadfield steel / Mn13 / 12–14% manganese steel / mangalloy / austenitic manganese steelBuyer search terms
ASTMA128 Grade A / B-2Austenitic manganese steel castings — chemistry reference only
EN NameEN 10349 GX120Mn12 / GX120Mn13(EN (cast)) Cast counterparts — castings standard, not wrought plate
BSBW10Former BS 3100 cast grade
Common NameZ120M12(AFNOR) French designation
JISSCMnH11Japanese cast high-manganese steel
Common NameMn13(GB) Chinese designation

Compliance & Certification

StandardStatusNotes
EN 10204 3.1SuitableProvided as standard — chemistry, delivery condition and hardness.
EN 10204 3.2ConditionalAvailable on request with independent third-party inspection — specify at order stage.

Specifications

Mechanical Properties

Values per Stahl-Eisen-Liste (SEL). Bar length compares conditions within each row.

PropertySolution Annealed & Water Quenched | SEL 1.3401
Tensile Strength (UTS)880–1130 MPatypicalAs quenched, about 10 mm plateTypical — not specified.
Yield Strength (0.2% Proof Stress)410 MPatypicalAs quenched, about 10 mm plateTypical minimum quoted by producers — not specified.
Elongation40 %typicalAs quenchedTypical — not specified.
Impact Energy (Charpy V-notch)124 JtypicalRoom tempTypical — not specified.
Hardness200 HBtypicalAs quenchedTypical (about 190–250 HB).
Hardness500 HBtypicalWork-hardened surface in serviceTypical achievable after impact work hardening.

Physical Properties

PropertySolution Annealed & Water Quenched | SEL 1.3401
Densityat 20°C7.71 g/cm³
Relative Magnetic Permeabilityat 20°C1.01 -
Coefficient of Thermal Expansionat 20–100°C18 µm/m·°C

Service Conditions

Service Temperature

Max 260 °C

Notes

[VERIFY — maxServiceTempC 260: embrittlement threshold per producer] Prolonged service or reheating above about 260–300°C causes carbide precipitation and embrittlement — keep wear parts and welds below this. As an austenitic steel it has no ductile-to-brittle transition and retains toughness at low temperatures.

Corrosion Performance

General corrosion

Corrosion behaviour similar to carbon steel. Combined corrosion and abrasion (wet slurries) accelerates wear — consider alternative materials for wet, low-impact abrasion.

Pitting resistance

No pitting resistance. Rusts in humid and coastal UAE and GCC atmospheres; corrosion is usually secondary to wear in service.

Additional notes

Not applicable — austenitic manganese steel, not stainless.

Heat Treatment

HEAT TREATMENT GUIDE — X120Mn12 / 1.3401 / Hadfield

Supply condition: solution annealed at about 1000–1050°C and water quenched — fully austenitic, about 200 HB. Hot forming / forging: 1050–850°C, followed by renewed solution annealing and water quench. Re-solution annealing: 1000–1050°C, water quench — restores toughness if the material has been embrittled by overheating. No hardening or tempering: hardness is developed in service by work hardening (impact / high-stress abrasion), to about 500 HB at the surface. Avoid reheating: do not expose above about 260–300°C during cutting, welding or service — slow cooling or holding in the 300–800°C range precipitates embrittling carbides [VERIFY — threshold per producer]. Thermal cutting: plasma or laser preferred; keep heat input low and avoid preheating. Pre-hardening option: surfaces can be pre-work-hardened by shot peening or explosive hardening where immediate wear resistance is needed.

ENGINEERING NOTES
Weldability
Fair

Weldable with austenitic consumables, but heat must be kept low: prolonged exposure above about 260–300°C precipitates carbides at grain boundaries and embrittles the steel [VERIFY — exact threshold per producer]. Do not preheat; use low heat input, short stringer beads, skip welding and keep interpass temperature below about 150°C — quench or air cool between passes. Use manganese-nickel electrodes for build-up and repair, and austenitic stainless (E307 / E309) for joining to carbon steel. Peen weld beads to reduce shrinkage stresses.

Filler metals
  • EFeMn-A · AWS A5.13 / SMAWManganese-nickel electrode for build-up and repair of manganese steel
  • E307-16 · AWS A5.4 / SMAWHigh-Mn austenitic stainless — joining manganese steel to itself or to carbon steel
  • E309L-16 · AWS A5.4 / SMAWAustenitic stainless for dissimilar joints to carbon / low-alloy steel
Machinability
Poor

Very difficult to machine: the steel work-hardens immediately under the tool. Avoid machining where possible — produce shapes by plasma, laser or waterjet cutting, and grind for final fit. If machining is unavoidable, use rigid set-ups, carbide or ceramic tooling, low speeds and heavy, continuous feeds below the work-hardened layer. Drilling is impractical; use thermal cutting or EDM for holes.

Applications

  • Jaw crusher plates, cone crusher liners and impact crusher hammers
  • Ball and SAG mill liners and lifter bars
  • Excavator, loader and dragline bucket liners, lips and side cutters
  • Grizzly bars, screen decks and chute liners in GCC quarries and cement plants
  • Shredder and scrap-processing wear parts in recycling plants
  • Railway crossings, frogs and switch components
  • Security bars, safe plates and anti-drill protection
  • Dredge pump and cutter-head wear components
  • Coal pulveriser and power-plant crusher parts
  • Hopper liners and transfer points subject to impact wear

Frequently Asked Questions

Quick answers on our grades, certification, supply and lead times.

Still have questions?

Our team responds fast with specifications, certification and stock availability.

Contact our team

X120Mn12 / 1.3401 Hadfield steel is used for wear parts that take impact as well as abrasion: jaw and cone crusher liners, impact hammers, mill liners, excavator and dragline bucket liners, grizzly bars, chute liners, shredder parts, railway crossings and security bars. Under impact its surface work-hardens to about 500 HB while the core stays tough. In the UAE and GCC it is widely used in quarries, cement plants, mining and recycling.

Get in touch

Elevateyourprojectswithoursuperiorsteel