Nickel Alloys dealers in UAE

Monel K500 / Alloy K-500 / 2.4375 Nickel-Copper Alloy | Supplier in UAE & GCC

Alloy K-500 / 2.4375 / UNS N05500 — age-hardened nickel-copper alloy: about 3× the yield of Alloy 400, seawater resistant, non-magnetic; marine shafting.

Industries Served

Marine
Oil & Gas
Aerospace & Defence
Petrochemical
Food Processing

Overview

Alloy K-500 (UNS N05500, EN 2.4375 / NiCu30Al, ASTM B865, QQ-N-286, AMS 4676; widely known by the trade names Monel K-500 and K-Monel) is a precipitation-hardenable nickel-copper alloy containing 63.0–70.0% nickel, about 27–33% copper, 2.30–3.15% aluminium and 0.35–0.85% titanium. The aluminium and titanium form fine Ni3(Al,Ti) precipitates during age hardening, giving roughly three times the yield strength and twice the tensile strength of Alloy 400 while keeping essentially the same corrosion resistance. Annealed and age-hardened bar to ASTM B865 provides 895 MPa minimum tensile and 585–620 MPa minimum yield strength with 20% elongation, and cold working before ageing raises this to 965–1000 MPa tensile and 690–760 MPa yield. It resists flowing seawater, high-velocity seawater erosion and cavitation, alkalis, hydrofluoric acid and de-aerated reducing acids, and is acceptable for sour service under NACE MR0175 / ISO 15156-3 at 35 HRC maximum. Unlike Alloy 400 it is virtually non-magnetic even at low temperatures. In the aged condition it has a greater tendency to stress corrosion cracking than Alloy 400 in some media, and like other nickel-copper alloys it should not be used in nitric acid or oxidising salts. Typical uses are pump and propeller shafts, impellers, valve trim, marine fasteners, oil-well drill collars and non-magnetic instrument housings.

Nifty Alloys supplies Alloy K-500 / 2.4375 from Dubai, UAE, in round bar and forgings — annealed and age hardened as standard, with annealed material and QQ-N-286, AMS 4676 and NACE MR0175 supply on request. Every supply carries an EN 10204 3.1 Mill Test Certificate as standard; EN 10204 3.2 third-party inspection is available on request. We deliver across the UAE within 24–48 hours, to Saudi Arabia, Kuwait, Qatar, Oman and Bahrain within 3–5 working days, and export to Europe, India and Africa. Send your size list and condition to request a quote — quotations are turned around the same day. Monel® is a registered trademark of its owner.

Chemical Composition

65 %
Ni

Nickel

63 – 70 %

30 %
Cu

Copper

27 – 33 %

2.8 %
Al

Aluminium

2.3 – 3.15 %

0.6 %
Ti

Titanium

0.35 – 0.85 %

1 %
Fe

Iron

≤ 2 %

0.8 %
Mn

Manganese

≤ 1.5 %

0.1 %
C

Carbon

≤ 0.25 %

Si

Silicon

≤ 0.5 %

S

Sulfur

≤ 0.01 %

Typical value Range (min–max) Minimum (≥) Maximum (≤) Hover / tap for notes

Standard

ASTM B865

Other

Revision: ASTM B865 — current edition

Available Forms

Forging

100–800 mm. Forged discs, rings and blocks to order. [VERIFY — supply range not confirmed]

Round Bar

12–300 mm. Diameter, annealed + age hardened. [VERIFY — stock range not confirmed]

Stock & delivery

Stock location
Dubai, UAE
In stock
Annealed + age hardened bar [VERIFY — stocked forms]; annealed, QQ-N-286, AMS 4676 and NACE MR0175 material on request.
Delivery UAE
24–48 hours
Delivery GCC
3–5 working days — Saudi Arabia, Kuwait, Qatar, Oman, Bahrain
Export
Europe, India, Africa on request
Quotation
Same-day quotation
Minimum order
No minimum order quantity for standard sizes; cut pieces available

Key standards

ASTM B865

Designations & Equivalents

StandardDesignationNotes
UNSN05500Unified Numbering System — primary chemistry
EN / Werkstoff2.4375European material number
EN NameNiCu30AlEuropean alloy designation (DIN 17743)
DIN17752German bar specification — aliases only
BS3076 NA18British bar designation — aliases only
Common NameQQ-N-286(Federal) US federal / naval specification (Module 2)
AMSAMS 4676Bars and forgings (Module 2)
ASMESB-865 / Code Case 1192ASME equivalent; Code Case 1192 for bolting — aliases only
Common NameMIL-N-24549(MIL) Legacy military specification — aliases only [VERIFY]
Common NameAlloy K500 / Nickel K-500 / age-hardened nickel-copper / non-magnetic nickel alloyBuyer search terms (trademarks used only in SEO / description / FAQ fields)

Compliance & Certification

StandardStatusNotes
EN 10204 3.1SuitableProvided as standard — chemistry, condition, tensile and hardness.
EN 10204 3.2ConditionalAvailable on request with independent third-party inspection — specify at order stage.
NACE MR0175 / ISO 15156SuitableAge-hardened K-500 at 35 HRC max acceptable under ISO 15156-3 within the applicable environmental limits [VERIFY — current edition].
QQ-N-286ConditionalSupplied to QQ-N-286 on request — confirm revision.
AMS 4676ConditionalSupplied to AMS 4676 on request — confirm revision.
ASME Code Case 1192ConditionalBolting applications only — not pre-qualified for ASME pressure-vessel parts.

Specifications

Mechanical Properties

Values per ASTM B865. Bar length compares conditions within each row.

PropertyAnnealed + Age Hardened | ASTM B865Annealed | ASTM B865
Tensile Strength (UTS)895 MPaminAll sizesASTM B865 minimum (130 ksi).690 MPatypicalAnnealedTypical — not specified.
Yield Strength (0.2% Proof Stress)620 MPamin< 25.4 mmASTM B865 minimum (90 ksi).–
Yield Strength (0.2% Proof Stress)585 MPamin≥ 25.4 mmASTM B865 minimum (85 ksi).–
Elongation20 %min50 mm / 4DASTM B865 minimum.–
Hardness24–35 HRCAgedTypical; NACE maximum 35 HRC.185 HBmaxAnnealedASTM B865 maximum (B90 HRB).

Physical Properties

PropertyAnnealed + Age Hardened | ASTM B865Annealed | ASTM B865
Densityat 20°C8.44 g/cm³8.44 g/cm³
Modulus of Elasticityat 20°C179 GPa179 GPa
Thermal Conductivityat 20°C17.5 W/m·K17.5 W/m·K
Coefficient of Thermal Expansionat 20–100°C13.4 µm/m·°C13.4 µm/m·°C
Specific Heat Capacityat 20°C418 J/kg·K418 J/kg·K
Electrical Resistivityat 20°C0.62 µΩ·m0.62 µΩ·m

Service Conditions

Service Temperature

Min -196 °CMax 480 °C

Notes

Good mechanical properties from subzero temperatures (strength increases, no ductile-to-brittle transition) to about 480°C. Oil and gas grades commonly impact tested at −29°C or lower (27 J average / 20 J minimum).

Corrosion Performance

General corrosion

Corrosion resistance substantially equivalent to Alloy 400 — seawater, alkalis, HF and de-aerated reducing acids. In the aged condition, greater SCC tendency than Alloy 400 in some media (for example moist aerated HF vapour). Not for nitric acid or oxidising salts. Acceptable in sour service within NACE MR0175 / ISO 15156-3 limits.

Pitting resistance

Excellent in flowing and high-velocity seawater (erosion and cavitation resistant); fouling and pitting can occur in stagnant seawater.

Additional notes

Not applicable — PREN is not meaningful for nickel-copper alloys.

Heat Treatment

HEAT TREATMENT GUIDE — Alloy K-500 / 2.4375 / UNS N05500

Annealing (solution): about 980°C, rapid quench — dissolves the hardening phase; 185 HB max. Age hardening (annealed or hot-worked material): about 593–610°C (1100–1125°F) for 16 h, then furnace cool at about 8–15°C/h to 480°C (900°F); below 480°C cooling rate is not critical (furnace, air or quench) — 895 MPa UTS minimum, typically 24–35 HRC. Cold-worked material: shorter ageing (about 8–16 h depending on cold work) for higher strength. Stress relieving: weldments stress relieved before age hardening. Hot working: about 870–1150°C; avoid prolonged soaking at the upper end. Dimensional change: slight uniform contraction on ageing — machine oversize, age, then finish.

ENGINEERING NOTES
Weldability
Good

Best welded by GTAW in the annealed condition using ERNiCu-7 / ENiCu-7 fillers; weldments should be stress relieved before age hardening. Matching filler does not age harden, so welds are weaker than aged base metal. Joints must be clean of sulphur, lead and other low-melting contaminants.

Filler metals
  • ERNiCu-7 · AWS A5.14 / TIG (GTAW)Nickel-copper filler — welds do not age harden
  • ENiCu-7 · AWS A5.11 / SMAWNickel-copper covered electrode
Machinability
Fair

Heavy machining is best done annealed or hot-worked and quenched; common practice is to machine slightly oversize, age harden, then finish to size. Age-hardened material can be finish-machined to close tolerances. Ageing causes a slight uniform contraction (about 2.5 × 10⁻⁴ mm/mm).

Applications

  • Marine propeller and pump shafts for GCC vessels and offshore units
  • Pump impellers and centrifugal-pump components in seawater
  • Valve trim, stems and seats for oil and gas and marine service
  • Marine fasteners, bolting and studs (ASME Code Case 1192)
  • Oil-well drill collars and MWD / LWD non-magnetic housings
  • Subsea connectors and sour-service components (NACE MR0175)
  • Doctor blades and scrapers for pulp and paper
  • Springs, chains and mixing shafts in corrosive service
  • Sensors and electronic components requiring low magnetic permeability
  • Naval and defence components to QQ-N-286

Related grades in Nickel Alloys

Frequently Asked Questions

Quick answers on our grades, certification, supply and lead times.

Still have questions?

Our team responds fast with specifications, certification and stock availability.

Contact our team

Alloy K-500 is used for marine propeller and pump shafts, impellers, valve trim, marine fasteners and bolting, oil-well drill collars and non-magnetic MWD housings, subsea connectors, doctor blades, springs and sensors. In the UAE and GCC it is a standard material for marine shafting and oil and gas valve and pump components.

Get in touch