316Ti / 1.4571 / X6CrNiMoTi17-12-2 — Ti-stabilised 316: Mo pitting resistance plus intergranular-corrosion resistance after welding and heat exposure.

Industries Served

Petrochemical
Oil & Gas
Marine
Food Processing
Power Generation

Overview

316Ti stainless steel (EN 1.4571 / X6CrNiMoTi17-12-2, UNS S31635, ASTM A240 / A276; known in Europe as the classic "V4A") is a titanium-stabilised, molybdenum-bearing austenitic chromium-nickel stainless steel containing 16.5–18.5% chromium, 10.5–13.5% nickel, 2.0–2.5% molybdenum and titanium of at least five times the carbon content, up to 0.70%. Molybdenum gives the pitting and crevice-corrosion resistance of 316 in chlorides, acids and quiet seawater, while titanium binds carbon as stable titanium carbides, preventing chromium carbide precipitation and intergranular corrosion after welding or exposure in the sensitisation range — and giving better strength at elevated temperature than 316 / 316L. It is the standard Mo-bearing stainless specified to EN in Europe, particularly in Germany, for heavy-section welds and higher-temperature equipment. In the solution-annealed condition (+AT) to EN 10088-3 it gives 500–700 MPa tensile strength, 200 MPa minimum proof stress, 40% elongation and 100 J impact energy, retaining 127 MPa proof stress at 550°C; ASTM A276 / A240 require 515 / 205 MPa. It is non-magnetic when annealed and tough at sub-zero temperatures. Typical uses are chemical, petrochemical and pharmaceutical equipment, heat exchangers, marine hardware, pressure vessels and welded process piping.

Nifty Alloys supplies 316Ti / 1.4571 stainless steel from Dubai, UAE, in round bar, plate and sheet, solution annealed to EN 10088-3 / EN 10088-2, with ASTM A276 / A240 dual certification on request. Every supply carries an EN 10204 3.1 Mill Test Certificate as standard, with chemistry and mechanical properties; EN 10204 3.2 third-party inspection is available on request. We deliver across the UAE within 24–48 hours, to Saudi Arabia, Kuwait, Qatar, Oman and Bahrain within 3–5 working days, and export to Europe, India and Africa. Send your size list to request a quote — quotations are turned around the same day.

Chemical Composition

0.04 %
C

Carbon

≤ 0.08 %

0.5 %
Si

Silicon

≤ 1 %

1.5 %
Mn

Manganese

≤ 2 %

P

Phosphorus

≤ 0.045 %

S

Sulfur

≤ 0.03 %

17.2 %
Cr

Chromium

16.5 – 18.5 %

11.5 %
Ni

Nickel

10.5 – 13.5 %

2.2 %
Mo

Molybdenum

2 – 2.5 %

0.4 %
Ti

Titanium

5 – 0.7 %

N

Nitrogen

Typical value Range (min–max) Minimum (≥) Maximum (≤) Hover / tap for notes

Standard

EN 10088-3

EN

Revision: EN 10088-3:2014

Stainless steels — Technical delivery conditions for semi-finished products, bars, rods, wire, sections and bright products. European standard covering 1.4542 (X5CrNiCuNb16-4).

EN designation: 1.4542, X5CrNiCuNb16-4. Supplied in solution annealed (+AT) condition.

Available Forms

Plate / Block

3–80 mm. Thickness; cut to size. [VERIFY — stock range not confirmed]

Round Bar

4–300 mm. Diameter, solution annealed (EN properties to 250 mm). [VERIFY — stock range not confirmed]

Sheet

0.5–3 mm. Thickness; 2B finish. [VERIFY — stock range not confirmed]

Stock & delivery

Stock location
Dubai, UAE
In stock
Solution Annealed (+AT) [VERIFY — stock status]; ASTM dual certification on request.
Delivery UAE
24–48 hours
Delivery GCC
3–5 working days — Saudi Arabia, Kuwait, Qatar, Oman, Bahrain
Export
Europe, India, Africa on request
Quotation
Same-day quotation
Minimum order
No minimum order quantity for standard sizes

Key standards

EN 10088-3

Designations & Equivalents

StandardDesignationNotes
EN / Werkstoff1.4571EN 10088 material number — primary chemistry
EN NameX6CrNiMoTi17-12-2EN 10088 steel name
AISI / SAE316TiASTM A240 / A276 Type 316Ti
UNSS31635Unified Numbering System
Common NameNone(AMS / MIL) No AMS or MIL specification applies to 316Ti
BS320S31 / 320S18Former British designations
JISSUS316TiJapanese Industrial Standard
Common NameZ6CNDT17-12(AFNOR) French designation
Common Name10Kh17N13M2T(GOST) Russian designation
Common Name06Cr17Ni12Mo2Ti(GB) Chinese designation
Common Name316Ti / V4A / 1.4571 stainless / Ti-stabilised 316 / marine grade stainlessBuyer search terms (V4A common in Europe)

Compliance & Certification

StandardStatusNotes
EN 10204 3.1SuitableProvided as standard — chemistry and mechanical properties.
EN 10204 3.2ConditionalAvailable on request with independent third-party inspection — specify at order stage.
NACE MR0175 / ISO 15156SuitableAustenitic stainless steel in the solution-annealed condition, 22 HRC max, acceptable under ISO 15156-3 within the environmental limits of the applicable table [VERIFY — current edition].
PED 2014/68/EU (EN 10028-7)ConditionalPressure-purpose plate to EN 10028-7 on request.

Specifications

Mechanical Properties

Values per EN 10088-3. Bar length compares conditions within each row.

PropertySolution Annealed (+AT) | EN 10088-3
Tensile Strength (UTS)500–700 MPaEN 10088-3 +AT, ≤ 160 mmEN range (ASTM: 515 MPa min).
Yield Strength (0.2% Proof Stress)200 MPaminEN 10088-3 +ATEN minimum (ASTM: 205 MPa); Rp1.0 235 MPa min.
Yield Strength (0.2% Proof Stress)127 MPaminAt 550°CEN 10088-3 minimum at temperature (185 MPa at 100°C).
Elongation40 %minA (5.65√So), longitudinalEN minimum.
Impact Energy (Charpy V-notch)100 Jmin+20°C, longitudinalEN minimum.
Hardness215 HBmax+ATEN maximum (guidance).

Physical Properties

PropertySolution Annealed (+AT) | EN 10088-3
Densityat 20°C8 g/cm³
Modulus of Elasticityat 20°C200 GPa
Thermal Conductivityat 20°C15 W/m·K
Coefficient of Thermal Expansionat 20–100°C16.5 µm/m·°C
Specific Heat Capacityat 20°C500 J/kg·K
Electrical Resistivityat 20°C0.75 µΩ·m

Service Conditions

Service Temperature

Min -196 °CMax 550 °C

Notes

EN 10088-3 gives minimum proof stress at temperature to 550°C (Rp0.2 127 MPa at 550°C). Stabilisation prevents intergranular corrosion after exposure in the sensitisation range. Oxidation resistance to about 850°C in air, but for scaling service use 321 / 310S. Retains toughness at sub-zero temperatures.

Corrosion Performance

PREN 24

General corrosion

Corrosion resistance similar to 316 in acids, alkalis and chlorides, with added resistance to intergranular corrosion after welding or heat exposure. Susceptible to chloride stress corrosion cracking above about 60°C like other austenitic grades.

Pitting resistance

Good pitting and crevice-corrosion resistance in chlorides of medium concentration and quiet seawater; for warm or flowing seawater and high-chloride service, use duplex or super-austenitic grades.

PREN notes

PREN = Cr + 3.3Mo ≈ 23–26 — similar to 316 / 316L.

Heat Treatment

HEAT TREATMENT GUIDE — 316Ti / 1.4571 / X6CrNiMoTi17-12-2

Supply condition: solution annealed (+AT) at 1020–1120°C, water or air cooled — fully austenitic. Not hardenable by heat treatment — strength increased only by cold work (for example +AT+C700: Rm 700–850 MPa, Rp0.2 350 MPa, ≤ 35 mm). Hot forming: about 1150–850°C, followed by solution annealing. Stabilising anneal (optional): about 870–900°C for severe intergranular-corrosion service. Welding: no preheat or PWHT required.

ENGINEERING NOTES
Weldability
Excellent

Readily welded by GTAW, GMAW, SMAW and SAW without preheat or PWHT. Use Nb-stabilised 318 / 19 12 3 Nb filler (titanium does not transfer reliably across the arc) or 316L(Si) filler. Welds resist intergranular corrosion in the as-welded condition; well suited to heavy-section welds.

Filler metals
  • 19 12 3 Nb (318) · EN ISO 14343 / TIG / MIGNb-stabilised filler — standard choice for 1.4571
  • ER318 · AWS A5.9 / TIG / MIGUS equivalent of 19 12 3 Nb
  • ER316LSi · AWS A5.9 / TIG / MIGLow-carbon alternative where stabilised filler is not required
  • E318-16 · AWS A5.4 / SMAWNb-stabilised covered electrode
Machinability
Fair

Medium-to-poor machinability — titanium carbonitrides are abrasive and the grade work hardens. Use rigid set-ups, sharp carbide tools, positive rake, steady feed and generous coolant.

Applications

  • Chemical and petrochemical process equipment and vessels
  • Heat exchangers and condensers
  • Heavy-section welded fabrications where post-weld annealing is impractical
  • Pharmaceutical and medical-engineering equipment
  • Marine hardware and fittings in quiet seawater
  • Pressure vessels and piping to European specifications
  • Pulp and paper and textile-dyeing equipment
  • Food and beverage processing plant
  • Desalination and water-treatment components in the GCC
  • Higher-temperature equipment needing 316 corrosion resistance

Related grades in Stainless Steel

Frequently Asked Questions

Quick answers on our grades, certification, supply and lead times.

Still have questions?

Our team responds fast with specifications, certification and stock availability.

Contact our team

316Ti / 1.4571 is used for chemical, petrochemical and pharmaceutical equipment, heat exchangers, pressure vessels, heavy-section welded fabrications, marine hardware, pulp and paper and food-processing plant. It is the standard Mo-bearing stainless steel in many European specifications. In the UAE and GCC it is used on projects designed to EN / DIN standards and in desalination and process plants.