440B / 1.4112 / X90CrMoV18 Martensitic Stainless Steel | Supplier in UAE & GCC

440B / 1.4112 / X90CrMoV18 — 18% Cr Mo-V martensitic stainless: 265 HB max annealed, 53–58 HRC hardened; knives, valve parts, bearings and guide shafts.

Industries Served

Food Processing
Manufacturing
Mould & Die
Marine

Overview

440B stainless steel (1.4112 / X90CrMoV18 to EN 10088-3; nearest equivalent AISI 440B / UNS S44003 to ASTM A276; JIS SUS440B) is a high-carbon martensitic stainless steel containing 0.85–0.95% carbon, 17.0–19.0% chromium, 0.90–1.30% molybdenum and 0.07–0.12% vanadium. Its high carbon forms hard chromium carbides for wear resistance and edge retention, molybdenum improves corrosion resistance and temper resistance, and vanadium refines the grain. Supplied soft annealed at 265 HB maximum for machining, it is hardened from about 1000–1050°C in oil, air or a hot bath and tempered to a working hardness of about 53–58 HRC — roughly 57 HRC after tempering at 100°C and 53 HRC at 400–500°C. It sits between 420 and 440C: harder and more wear-resistant than 420, and slightly tougher than 440C, with corrosion resistance suited to fresh water, steam, food acids and mild atmospheres. AISI 440B has slightly wider carbon and chromium limits, lower molybdenum and no vanadium, so 1.4112 is its nearest modern equivalent. Typical uses are cutlery and industrial knives, surgical instruments, valve balls and seats, bearings, guide shafts and wear parts in plastics processing.

Nifty Alloys supplies 440B / 1.4112 stainless steel from Dubai, UAE, in round bar, soft annealed, with precision-ground bar on request. Every supply carries an EN 10204 3.1 Mill Test Certificate as standard, stating the grade supplied, chemistry and annealed hardness; EN 10204 3.2 third-party inspection is available on request. We deliver across the UAE within 24–48 hours, to Saudi Arabia, Kuwait, Qatar, Oman and Bahrain within 3–5 working days, and export to Europe, India and Africa. Send your size list to request a quote — quotations are turned around the same day.

Chemical Composition

0.9 %
C

Carbon

0.85 – 0.95 %

0.4 %
Si

Silicon

≤ 1 %

0.5 %
Mn

Manganese

≤ 1 %

P

Phosphorus

≤ 0.04 %

S

Sulfur

≤ 0.03 %

18 %
Cr

Chromium

17 – 19 %

1.1 %
Mo

Molybdenum

0.9 – 1.3 %

0.1 %
V

Vanadium

0.07 – 0.12 %

Typical value Range (min–max) Minimum (≥) Maximum (≤) Hover / tap for notes

Standard

EN 10088-3

EN

Revision: EN 10088-3:2014

Stainless steels — Technical delivery conditions for semi-finished products, bars, rods, wire, sections and bright products. European standard covering 1.4542 (X5CrNiCuNb16-4).

EN designation: 1.4542, X5CrNiCuNb16-4. Supplied in solution annealed (+AT) condition.

Available Forms

Round Bar

3–150 mm. Diameter, annealed; precision ground on request. [VERIFY — stock range not confirmed]

Stock & delivery

Stock location
Dubai, UAE
In stock
Annealed (+A, 265 HB max) [VERIFY — stock status].
Delivery UAE
24–48 hours
Delivery GCC
3–5 working days — Saudi Arabia, Kuwait, Qatar, Oman, Bahrain
Export
Europe, India, Africa on request
Quotation
Same-day quotation
Minimum order
No minimum order quantity for standard sizes

Key standards

EN 10088-3

Designations & Equivalents

StandardDesignationNotes
AISI / SAE440B / SAE 51440BASTM A276 Type 440B — nearest equivalent
UNSS44003Unified Numbering System
EN / Werkstoff1.4112EN 10088-3 material number — primary chemistry
EN NameX90CrMoV18EN 10088 steel name
JISSUS440BJapanese Industrial Standard
Common Name90Cr18MoV(GB) Chinese designation
Common Name440B stainless / 18% chrome knife steel / stainless shaft steel / X90CrMoV18Buyer search terms

Compliance & Certification

StandardStatusNotes
EN 10204 3.1SuitableProvided as standard — grade supplied, chemistry and annealed hardness.
EN 10204 3.2ConditionalAvailable on request with independent third-party inspection — specify at order stage.
NACE MR0175 / ISO 15156Not Applicable — High-carbon 440-series martensitic grade — not used for sour service.

Specifications

Mechanical Properties

Values per EN 10088-3. Bar length compares conditions within each row.

PropertyAnnealed (+A) | EN 10088-3
Hardness265 HBmaxAnnealed (+A)EN 10088-3 maximum.
Hardness53–58 HRCHardened 1000–1050°C, tempered 100–500°CTypical working hardness — guidance.
Tensile Strength (UTS)800 MPatypicalAnnealedTypical — not specified.

Physical Properties

PropertyAnnealed (+A) | EN 10088-3
Densityat 20°C7.7 g/cm³
Modulus of Elasticityat 20°C210 GPa
Thermal Conductivityat 20°C25 W/m·K
Coefficient of Thermal Expansionat 20–100°C10.4 µm/m·°C
Electrical Resistivityat 20°C0.65 µΩ·m

Service Conditions

Service Temperature

Max 400 °C

Notes

Hardness is largely retained to about 400–500°C (secondary-hardening plateau about 53 HRC) but falls sharply above about 550°C. Toughness is low at sub-zero temperatures; not for shock-loaded service.

Corrosion Performance

PREN 21

General corrosion

Best corrosion resistance in the hardened, low-tempered and polished condition. Tempering at about 400–600°C reduces corrosion resistance. Keep surfaces clean and polished in the humid, coastal UAE climate.

Pitting resistance

Moderate — resists fresh water, steam, food acids and mild atmospheres; not for seawater or chloride-rich media.

PREN notes

PREN ≈ 20–22 calculated (Cr + 3.3Mo); effective resistance lower because much chromium is in carbides.

Heat Treatment

HEAT TREATMENT GUIDE — 440B / 1.4112 / X90CrMoV18

Hot working: preheat to 760–815°C, then heat to about 1040–1150°C; do not work below about 900°C; cool slowly (furnace). Soft annealing: 840–870°C, very slow furnace cooling — 265 HB max (+A). Stress relieving: about 650–700°C after rough machining. Hardening: preheat to about 760–800°C, austenitise at about 1000–1050°C; quench in preheated oil, air, hot bath (about 500–550°C) or pressurised gas. Tempering (typical, Lucefin data): 100°C ≈ 57 HRC; 200°C ≈ 55 HRC; 300°C ≈ 54 HRC; 400–500°C ≈ 53 HRC; 600°C ≈ 40 HRC. Low-temperature tempering (about 150°C) gives maximum hardness (about 58 HRC) and best corrosion resistance. Sub-zero treatment optional to reduce retained austenite.

ENGINEERING NOTES
Weldability
Poor

Not suitable for welding — the high carbon content makes the weld zone air-harden and crack. If an unavoidable repair is attempted, use high preheat (about 250–300°C), an austenitic filler such as E312 and anneal immediately afterwards. Design parts to avoid welding.

Filler metals
  • E312-16 · AWS A5.4 / SMAWAustenitic electrode for non-load-bearing repairs only; anneal after welding
  • ER309L · AWS A5.9 / TIGAustenitic filler for dissimilar attachments where unavoidable
Machinability
Poor

Machine only in the annealed condition, with carbide or ceramic tooling, rigid set-ups and chip breakers — chips are tough and stringy and the carbides wear tools. After hardening, finish by grinding; can be polished to a high gloss.

Frequently Asked Questions

Quick answers on our grades, certification, supply and lead times.

Still have questions?

Our team responds fast with specifications, certification and stock availability.

Contact our team

440B stainless steel is used for parts that need high hardness and wear resistance with moderate corrosion resistance: cutlery and industrial knives, surgical instruments, valve balls and seats, bearings, linear guide shafts, plastics-processing wear parts and pump components. In the UAE and GCC it is used in food processing, valve and machine-shop applications.

Get in touch

Elevateyourprojectswithoursuperiorsteel