Tool Steel dealers in UAE

O2 / 1.2842 / 90MnCrV8 Oil Hardening Tool Steel | Supplier in UAE & GCC

O2 / 1.2842 / 90MnCrV8 — Mn-Cr-V oil-hardening cold-work tool steel: 229 HB max annealed, 58–64 HRC hardened; gauges, knives, punches and thread tools.

Industries Served

Manufacturing
Mould & Die
Automotive

Overview

O2 / 1.2842 (90MnCrV8 to EN ISO 4957; near-equivalent AISI O2 to ASTM A681; formerly BS 4659 BO2; French 90MV8) is a light-alloyed, oil-hardening cold-work tool steel with nearly 1% carbon. 1.2842 contains 0.85–0.95% carbon, 1.80–2.20% manganese, 0.20–0.50% chromium and 0.05–0.20% vanadium. Its high manganese content provides the hardenability for an oil or hot-bath quench, keeping distortion and cracking risk low, while vanadium refines the grain and improves toughness and edge retention. Unlike O1 / 1.2510 it contains no tungsten, relying on manganese and vanadium instead. Supplied soft annealed at 229 HB maximum, it machines easily and is hardened from 790–820°C to about 64 HRC; EN ISO 4957 requires at least 60 HRC after quenching from 790°C in oil and tempering at 180°C. Tempered at 100–300°C it gives a working hardness of roughly 56–63 HRC with good dimensional stability. Hardenability through large sections is limited, so it suits small and medium tools. Typical uses are gauges and measuring tools, cutting and punching tools, shear and paper knives, thread-cutting tools, reamers, guide strips and small plastic moulds.

Nifty Alloys supplies O2 / 1.2842 tool steel from stock in Dubai, UAE, in round bar and flat bar, soft annealed, with precision ground flats available through our ground flat stock service. Every supply is dispatched with EN 10204 3.1 Mill Test Certificates as standard, certifying EN ISO 4957 chemistry and annealed hardness with full traceability to the mill; EN 10204 3.2 third-party inspection is available on request. We deliver across the UAE within 24–48 hours, to Saudi Arabia, Kuwait, Qatar, Oman and Bahrain within 3–5 working days, and export to Europe, India and Africa. Send your size list or drawing to request a quote — quotations are turned around the same day.

Chemical Composition

0.9 %
C

Carbon

0.85 – 0.95 %

0.25 %
Si

Silicon

0.1 – 0.4 %

2 %
Mn

Manganese

1.8 – 2.2 %

0.4 %
Cr

Chromium

0.2 – 0.5 %

0.1 %
V

Vanadium

0.05 – 0.2 %

P

Phosphorus

≤ 0.03 %

S

Sulfur

≤ 0.03 %

Typical value Range (min–max) Minimum (≥) Maximum (≤) Hover / tap for notes

Standard

EN ISO 4957

EN

Revision: EN ISO 4957 — current edition

Tool steels — specification for chemical composition, heat treatment, and properties of tool steels including cold work, hot work, and high-speed grades.

Published as BS EN ISO 4957; leading BS dropped to match house style. European standard governing 1.2379 (X153CrMoV12) and other DIN tool steel grades. Supersedes former DIN 17350 for tool steels. Referenced in European and Middle Eastern engineering procurement. Equivalent German standard: DIN EN ISO 4957.

Available Forms

Flat Bar

5–100 mm. Thickness; width to order; ground flats via /services/ground-flat-stock.

Round Bar

5–250 mm. Diameter, annealed.

Stock & delivery

Stock location
Dubai, UAE
In stock
Annealed (+A, 229 HB max) — standard stocked condition.
Delivery UAE
24–48 hours
Delivery GCC
3–5 working days — Saudi Arabia, Kuwait, Qatar, Oman, Bahrain
Export
Europe, India, Africa on request
Quotation
Same-day quotation
Minimum order
No minimum order quantity for standard sizes

Key standards

EN ISO 4957

Designations & Equivalents

StandardDesignationNotes
EN / Werkstoff1.2842Material number — primary chemistry on this page
EN Name90MnCrV8EN ISO 4957 steel name
AISI / SAEO2 — near equivalentASTM A681 (alias per register)
UNST31502Unified Numbering System (O2)
ASTMA681Alias — US alloy tool steel standard
BSBO2Former BS 4659 designation — superseded by BS EN ISO 4957
Common Name90MV8(AFNOR) French designation
Common Name9Mn2V — nearest(GB) Chinese designation
Common NameO2 tool steel / oil hardening steel / gauge plate / ground flat stockBuyer search terms

Compliance & Certification

StandardStatusNotes
EN 10204 3.1SuitableProvided as standard — EN ISO 4957 chemistry and annealed hardness.

Specifications

Mechanical Properties

Values per EN ISO 4957. Bar length compares conditions within each row.

PropertyAnnealed (+A) | EN ISO 4957
Hardness229 HBmaxSoft annealed (+A)EN ISO 4957 maximum.
Hardness60 HRCminTest: 790°C oil, tempered 180°CEN ISO 4957 minimum hardening response.
Hardness57–62 HRCWorking hardness after temperingTypical — guidance.
Tensile Strength (UTS)770 MPatypicalAnnealedTypical — not specified.

Physical Properties

PropertyAnnealed (+A) | EN ISO 4957
Densityat 20°C7.85 g/cm³
Thermal Conductivityat 20°C32.8 W/m·K
Coefficient of Thermal Expansionat 20–100°C12.2 µm/m·°C

Service Conditions

Service Temperature

Notes

Cold-work tool steel tempered at 100–300°C; hardness falls if tools run above the tempering temperature (≈ 50 HRC at 400°C). Not for hot-work service.

Corrosion Performance

General corrosion

Store dry; protect ground surfaces with rust-preventive oil.

Pitting resistance

Not corrosion resistant; finished tools rust quickly in humid, coastal UAE and GCC conditions — keep oiled.

Additional notes

Not applicable — not a stainless steel.

Heat Treatment

HEAT TREATMENT GUIDE — O2 / 1.2842 / 90MnCrV8

Hot forming: 1050–850°C. Soft annealing: about 680–730°C, slow furnace cooling — 229 HB max (+A). Stress relieving: about 600–650°C, slow furnace cooling, after heavy machining. Hardening: preheat to about 500–600°C, austenitise at 790–820°C; quench in oil or hot bath at 180–220°C — about 64 HRC as quenched. EN ISO 4957 test: 790 ± 10°C oil, tempered 180 ± 10°C → 60 HRC min. Tempering: immediately after quenching, at least 1–2 h — typical: 100°C ≈ 63 HRC, 200°C ≈ 60 HRC, 300°C ≈ 56 HRC, 400°C ≈ 50 HRC. Working hardness usually 57–62 HRC. Note: limited through-hardenability — best for small and medium sections; protect against decarburisation.

ENGINEERING NOTES
Weldability
Poor

Tool repair welding only, with a qualified procedure: preheat to about 300–500°C, weld at that temperature with a suitable tool-steel or hard-facing filler, and stress relieve or temper immediately afterwards. High carbon makes the weld zone prone to cracking.

Filler metals
  • Matching O-type filler rod · Tool-steel repair / TIGEdge repair of hardened tools with preheat and post-weld temper
  • Cr-Mo alloy electrode · Cr-Mo repair electrodeRepairs on annealed material before hardening
Machinability
Good

Good machinability in the annealed condition (229 HB max). Stress relieve at about 600–650°C after heavy machining, finish-machine, then harden. After hardening, finish by grinding. Protect against decarburisation during hardening.

Frequently Asked Questions

Quick answers on our grades, certification, supply and lead times.

Still have questions?

Our team responds fast with specifications, certification and stock availability.

Contact our team

O2 / 1.2842 is used for gauges and measuring tools, cutting and punching tools for thin sheet, shear and paper knives, thread-cutting tools, reamers, guide strips, cams and small plastic moulds. It hardens in oil to about 64 HRC with low distortion and machines easily when annealed. In the UAE and GCC it is a common toolroom and maintenance steel.

Get in touch

Elevateyourprojectswithoursuperiorsteel