Alloy Steel dealers in UAE

16MnCr5 / 1.7131 / 527M17 Case Hardening Steel | Supplier in UAE & GCC

16MnCr5 / 1.7131 / 527M17 — Mn-Cr case hardening steel: 207 HB max annealed, about 58–62 HRC carburised case over an 800–1100 MPa core; gears, shafts.

Industries Served

Automotive
Manufacturing
Heavy Engineering
Mould & Die

Overview

16MnCr5 (1.7131, EN ISO 683-3 — formerly EN 10084; BS 527M17 / 590M17; AISI ~5115) is a manganese-chromium case-hardening steel containing 0.14–0.19% carbon, 1.00–1.30% manganese and 0.80–1.10% chromium. Its low carbon keeps the core tough and machinable, while manganese and chromium give good hardenability and a strong response to carburising. Carburised at about 880–980°C and hardened, it develops a hard, wear-resistant case of about 58–62 HRC over a core of roughly 800–1100 MPa, with good fatigue and impact resistance. Double hardening — core hardening at 860–900°C followed by case hardening at 780–820°C — refines both case and core. Supplied soft annealed at 207 HB maximum, or normalised / ferrite-pearlite treated at 138–187 HB, it machines readily before heat treatment and is weldable before carburising. 16MnCr5 is Europe's standard case-hardening steel for automotive and industrial gears, gear shafts, camshafts, gudgeon pins, spindles and cardan joints; for larger, more heavily loaded gears, a nickel-bearing grade such as EN36 gives a stronger core.

Nifty Alloys supplies 16MnCr5 / 1.7131 case-hardening steel from stock in Dubai, UAE, in round bar and flat bar, annealed as standard, with normalised or ferrite-pearlite treated material on request. Bars are cut to length and dispatched with EN 10204 3.1 Mill Test Certificates as standard, certifying EN ISO 683-3 chemistry, delivery condition, hardness and, where specified, Jominy hardenability; EN 10204 3.2 third-party inspection is available on request. We deliver across the UAE within 24–48 hours, to Saudi Arabia, Kuwait, Qatar, Oman and Bahrain within 3–5 working days, and export to Europe, India and Africa. Send your size list or drawing to request a quote — quotations are turned around the same day.

Chemical Composition

0.16 %
C

Carbon

0.14 – 0.19 %

0.25 %
Si

Silicon

≤ 0.4 %

1.15 %
Mn

Manganese

1 – 1.3 %

0.95 %
Cr

Chromium

0.8 – 1.1 %

P

Phosphorus

≤ 0.025 %

S

Sulfur

≤ 0.035 %

Cu

Copper

≤ 0.4 %

Typical value Range (min–max) Minimum (≥) Maximum (≤) Hover / tap for notes

Standard

EN ISO 683-3

EN

Revision: EN ISO 683-3:2019 — current edition

Heat-treatable steels, alloy steels and free-cutting steels — Part 3: Case-hardening steels. Covers 16MnCr5 (1.7131) and 16MnCrS5 (1.7139) in delivery conditions +A, +N, +FP, +TH and +AC.

Current European standard for case-hardening steels; replaced EN 10084. Specifies chemistry, delivery-condition hardness and Jominy hardenability bands (+H, +HH, +HL).

Available Forms

Flat Bar

10–100 mm. Thickness; width × thickness to order.

Round Bar

10–250 mm. Diameter, annealed; bright drawn / centreless ground in smaller sizes.

Stock & delivery

Stock location
Dubai, UAE
In stock
Annealed (+A, 207 HB max) — standard stocked condition. Normalised / +FP on request. Case hardening by the customer.
Delivery UAE
24–48 hours
Delivery GCC
3–5 working days — Saudi Arabia, Kuwait, Qatar, Oman, Bahrain
Export
Europe, India, Africa on request
Quotation
Same-day quotation
Minimum order
No minimum order quantity for standard sizes

Key standards

EN ISO 683-3

Designations & Equivalents

StandardDesignationNotes
EN Name16MnCr5EN ISO 683-3 (formerly EN 10084) — primary designation
EN / Werkstoff1.7131Material number
EN Name16MnCrS5 / 1.7139Controlled-sulphur variant for improved machinability
BS527M17 / 590M17 / 590H17BS 970 designations (withdrawn standard)
AISI / SAE5115 — nearestUS designation
Common Name16MC5 / 16MC4(AFNOR) French designations
Common Name15CrMn / 20CrMn(GB) Chinese designations (nearest)
Common NameSS 2173 / UNE F.1516 / GOST 18KhG(Other) Swedish, Spanish and Russian designations
Common Name16MnCr5 case hardening steel / carburising steel / gear steelBuyer search terms

Compliance & Certification

StandardStatusNotes
EN 10204 3.1SuitableProvided as standard — EN ISO 683-3 chemistry, delivery condition, hardness and, on request, Jominy hardenability.
EN 10204 3.2ConditionalAvailable on request with independent third-party inspection — specify at order stage.
NACE MR0175 / ISO 15156Not Applicable — Not a sour-service grade in its intended case-hardened condition (about 58–62 HRC surface, far above 22 HRC).

Specifications

Mechanical Properties

Values per EN ISO 683-3. Bar length compares conditions within each row.

PropertyAnnealed (+A) | EN ISO 683-3Normalised (+N / +FP) | EN ISO 683-3
Hardness207 HBmaxSoft annealed (+A)EN ISO 683-3 maximum.138–187 HBNormalised (+N)EN ISO 683-3 range.
Hardness156–207 HBTreated to hardness range (+TH)EN ISO 683-3 range.140–187 HBFerrite-pearlite (+FP)EN ISO 683-3 range.
Hardness58–62 HRCCarburised case after hardening and temperingTypical achievable case hardness — process dependent.–
Tensile Strength (UTS)700 MPatypicalAnnealedTypical — not specified.–
Tensile Strength (UTS)800–1100 MPaCore after case hardening (typical)Typical core strength — guidance, depends on section.–

Physical Properties

PropertyAnnealed (+A) | EN ISO 683-3Normalised (+N / +FP) | EN ISO 683-3
Densityat 20°C7.76 g/cm³7.76 g/cm³
Modulus of Elasticityat 20°C210 GPa210 GPa
Shear Modulusat 20°C80 GPa80 GPa
Thermal Conductivityat 20°C44 W/m·K44 W/m·K
Coefficient of Thermal Expansionat 20–100°C11.5 µm/m·°C11.5 µm/m·°C
Specific Heat Capacityat 20°C431 J/kg·K431 J/kg·K
Electrical Resistivityat 20°C0.12 µΩ·m0.12 µΩ·m

Service Conditions

Service Temperature

Max 150 °C

Notes

Carburised parts are tempered at only 150–200°C, so service above about 150°C softens the case and reduces wear and contact-fatigue resistance. Specify core impact testing for low-temperature service.

Corrosion Performance

General corrosion

Corrodes like other low-alloy steels. Carburised and hardened surfaces are susceptible to hydrogen embrittlement from pickling or plating — bake after electroplating.

Pitting resistance

No pitting resistance. Store oiled and under cover in the humid, coastal UAE and GCC climate; protect finished gears with lubricant or coatings.

Additional notes

Not applicable — low-alloy steel.

Heat Treatment

HEAT TREATMENT GUIDE — 16MnCr5 / 1.7131 / 527M17

Hot forming: 1100–850°C. Normalising: about 870°C, air cool — 138–187 HB (+N). Soft annealing: about 650–710°C, slow cooling (about 15°C/h) to 600°C — 207 HB max (+A). Isothermal / +FP treatment: 140–187 HB for consistent machining. Carburising: about 880–980°C (typically 880–930°C) — time per required case depth. Direct hardening from carburising, or double hardening: core harden 860–900°C, then case harden 780–820°C; quench in oil or polymer. Tempering: 150–200°C, 1 h minimum — case about 58–62 HRC; core typically 800–1100 MPa depending on section. End-quench (Jominy) test: quench from 880°C. Welding: carry out in the annealed state, before carburising.

ENGINEERING NOTES
Weldability
Good

Generally weldable in the annealed or normalised condition before carburising, thanks to its low carbon content. Use low-hydrogen consumables, preheat thicker sections and stress relieve after welding. Never weld carburised or case-hardened parts — the high-carbon case cracks. Mask weld areas from carburising if they must remain soft.

Filler metals
  • E7018 · AWS A5.1 / SMAWLow-hydrogen electrode for joints made before carburising
  • ER70S-6 · AWS A5.18 / MIG (GMAW)Solid wire for general joining in the annealed condition
  • ER80S-B2 · AWS A5.28 / TIG (GTAW)Cr-Mo wire where higher joint strength is needed
Machinability
Good

Machines well in the annealed (207 HB max) or +FP (140–187 HB) condition; +FP gives the most consistent finish for gear hobbing. The controlled-sulphur variant 16MnCrS5 (1.7139) improves chip breaking for high-volume machining. Complete machining before carburising; after case hardening only grinding is practical.

Applications

  • Gears, pinions and gear wheels for automotive and industrial gearboxes
  • Gear shafts, splined shafts and transmission parts
  • Camshafts, cam followers and tappets
  • Gudgeon pins, piston pins, bolts and journals
  • Cardan joints, universal joints and joint parts
  • Spindles and machine-tool components
  • Hole-locking systems and precision wear parts
  • Plastic mould plates and synthetic-resin moulds (carburised)
  • Sprockets and chain wheels for GCC conveyor and handling equipment
  • Case-hardened pins and bushes for construction machinery

Frequently Asked Questions

Quick answers on our grades, certification, supply and lead times.

Still have questions?

Our team responds fast with specifications, certification and stock availability.

Contact our team

16MnCr5 / 1.7131 is used for case-hardened parts that need a hard, wear-resistant surface over a tough core: gears and pinions, gear and splined shafts, camshafts, gudgeon pins, bolts, journals, cardan joints, spindles and carburised mould plates. After carburising it reaches about 58–62 HRC at the surface. In the UAE and GCC it is widely used for gearbox, conveyor and machinery components.

Get in touch

Elevateyourprojectswithoursuperiorsteel