Alloy Steel dealers in UAE

EN36 / 655M13 / 15NiCr13 Case Hardening Steel | Supplier in UAE & GCC

EN36 / 655M13 (15NiCr13) — 3% Ni-Cr case hardening steel: 58–62 HRC carburised case over a tough 850–1230 MPa core for gears, cams and crankshafts.

Industries Served

Automotive
Heavy Engineering
Aerospace & Defence
Mining
Manufacturing

Overview

EN36 (BS 970 655M13, closely related to EN 15NiCr13 / 1.5752, formerly DIN 14NiCr14) is a 3% nickel-chromium case-hardening steel, supplied in Europe to EN ISO 683-3 (formerly EN 10084). Its low carbon of about 0.10–0.16% keeps the core tough and machinable, while 3.0–3.75% nickel and 0.7–1.0% chromium give the hardenability to harden thick sections through the core after carburising. Carburised at 880–980°C and hardened, EN36 develops a hard, wear-resistant case of about 58–62 HRC over a core of roughly 850–1230 MPa, with exceptional resistance to shock and fatigue — nickel is what lets the core stay tough at that strength. Double hardening, core hardening at 840–880°C followed by case hardening at 780–820°C, refines both case and core for the most demanding gears. EN36 is the classic choice for heavy-duty gears, pinions, crankshafts, camshafts, gudgeon pins and aircraft and motorsport transmission parts, where a lean case-hardening steel such as 16MnCr5 or 8620 lacks core strength or toughness.

Nifty Alloys supplies EN36 / 655M13 / 15NiCr13 case-hardening steel from stock in Dubai, UAE, in round bar and flat bar, in the annealed condition for machining before carburising, with normalised and as-rolled bar on request. Bars are cut to length and dispatched with EN 10204 3.1 Mill Test Certificates as standard, reporting chemistry, hardness and, where specified, Jominy hardenability, with full traceability to the mill; EN 10204 3.2 third-party inspection is available on request. We deliver across the UAE within 24–48 hours, to Saudi Arabia, Kuwait, Qatar, Oman and Bahrain within 3–5 working days, and export to Europe, India and Africa for gear makers, automotive and heavy-engineering workshops. Send your size list or drawing to request a quote — quotations are turned around the same day.

Chemical Composition

0.13 %
C

Carbon

0.1 – 0.16 %

Si

Silicon

0.1 – 0.35 %

Mn

Manganese

0.35 – 0.6 %

3.4 %
Ni

Nickel

3 – 3.75 %

0.85 %
Cr

Chromium

0.7 – 1 %

Mo

Molybdenum

≤ 0.15 %

P

Phosphorus

≤ 0.035 %

S

Sulfur

≤ 0.04 %

Typical value Range (min–max) Minimum (≥) Maximum (≤) Hover / tap for notes

Standard

EN ISO 683-3

EN

Revision: EN ISO 683-3 — current edition

Heat-treatable steels, alloy steels and free-cutting steels — Part 3: Case-hardening steels. Covers 16MnCr5 (1.7131) and 16MnCrS5 (1.7139) in delivery conditions +A, +N, +FP, +TH and +AC.

Current European standard for case-hardening steels; replaced EN 10084. Specifies chemistry, delivery-condition hardness and Jominy hardenability bands (+H, +HH, +HL).

Available Forms

Flat Bar

10–100 mm. Thickness; width × thickness to order. [VERIFY — stock range not confirmed]

Round Bar

16–300 mm. Diameter, annealed; bright drawn and ground on request. [VERIFY — stock range not confirmed]

Stock & delivery

Stock location
Dubai, UAE
In stock
Annealed — standard stocked condition. As-rolled and normalised on request. Carburising and hardening by the customer.
Delivery UAE
24–48 hours
Delivery GCC
3–5 working days — Saudi Arabia, Kuwait, Qatar, Oman, Bahrain
Export
Europe, India, Africa on request
Quotation
Same-day quotation
Minimum order
No minimum order quantity for standard sizes

Key standards

EN ISO 683-3

Designations & Equivalents

StandardDesignationNotes
BSEN36 / EN36A / EN36BOriginal BS 970:1955 designations — primary buyer terms (EN36C is a different grade, 832M13)
BS655M13 / 655H13BS 970 designations (withdrawn standard); H = hardenability-band variant
EN Name15NiCr13EN ISO 683-3 (formerly EN 10084) — closely related; 0.14–0.20% C
EN / Werkstoff1.575215NiCr13 material number
DIN14NiCr14Former DIN designation for 1.5752
AISI / SAE3415 — nearest former gradeFormer SAE grade; closest Ni-Cr balance
AISI / SAE3310 / E3310 — nearest former gradeFormer SAE grade with higher chromium — not an exact equivalent
JISSNC815Japanese Industrial Standard
Common Name14NC12(AFNOR) French designation
Common Name12KhN3A(GOST) Russian designation
Common NameEN36 case hardening steel / 3% nickel chrome steel / carburising steel / EN36 round barBuyer search terms

Compliance & Certification

StandardStatusNotes
EN 10204 3.1SuitableProvided as standard — chemistry (655M13 or 15NiCr13 as supplied), hardness and, on request, Jominy hardenability.
EN 10204 3.2ConditionalAvailable on request with independent third-party inspection — specify at order stage.
NACE MR0175 / ISO 15156Not Applicable — Not acceptable under ISO 15156-2 general requirements: carbon and low-alloy steels must contain < 1% Ni (EN36 has 3.0–3.75%), and case-hardened surfaces far exceed 22 HRC. Not a sour-service grade.

Specifications

Mechanical Properties

Values per EN ISO 683-3. Bar length compares conditions within each row.

PropertyAnnealed | EN ISO 683-3Normalised | EN ISO 683-3
Hardness229 HBmaxSoft annealed (+A)EN ISO 683-3 maximum for 15NiCr13.166–217 HBFerrite-pearlite (+FP)EN ISO 683-3 range for 15NiCr13.
Hardness255 HBmaxTreated for cold shearability (+S)EN ISO 683-3 maximum.179–229 HBTreated to hardness range (+TH)EN ISO 683-3 range for 15NiCr13.
Hardness58–62 HRCCarburised case after hardening and temperingTypical achievable case hardness — depends on process.–
Tensile Strength (UTS)1030–1320 MPaCore after case hardening — up to 11 mmEN 10084 guidance for 15NiCr13 — not a supply requirement.–
Yield Strength (0.2% Proof Stress)835 MPaminCore after case hardening — up to 11 mmEN 10084 guidance — not a supply requirement.–
Elongation9 %minCore after case hardening — up to 11 mmEN 10084 guidance.–

Physical Properties

PropertyAnnealed | EN ISO 683-3Normalised | EN ISO 683-3
Densityat 20°C7.85 g/cm³7.85 g/cm³
Modulus of Elasticityat 20°C205 GPa205 GPa
Thermal Conductivityat 20°C35 W/m·K35 W/m·K
Coefficient of Thermal Expansionat 20–100°C11.5 µm/m·°C11.5 µm/m·°C

Service Conditions

Service Temperature

Max 150 °C

Notes

Case-hardened parts are tempered at only 150–200°C, so service above about 150°C softens the carburised case and reduces wear and fatigue resistance. The high-nickel core keeps good toughness at sub-zero temperatures, which suits cold-climate and aerospace transmissions; specify core impact testing if required.

Corrosion Performance

General corrosion

Corrodes like other low-alloy steels. Carburised and hardened surfaces (58–62 HRC) are highly susceptible to hydrogen embrittlement from pickling or plating — bake after any electroplating. Not for sour service in the case-hardened condition.

Pitting resistance

No pitting resistance. Store oiled and under cover in the humid, coastal UAE and GCC climate; protect finished gears with lubricant or coatings.

Additional notes

Not applicable — low-alloy steel.

Heat Treatment

HEAT TREATMENT GUIDE — EN36 / 655M13 / 15NiCr13

Forging: start about 1180–1200°C, finish at about 800–850°C; cool slowly. Soft annealing: 630–660°C — slow cool — max 229 HB (+A) for machining. Carburising: 880–980°C (generally not above 950°C if direct hardening) — time per required case depth — gas, salt or pack. Direct hardening: quench from carburising or from a temperature between core- and case-hardening ranges where distortion is a concern. Double hardening (best properties): core harden 840–880°C, oil quench; then case harden 780–820°C, oil quench. Tempering: 150–200°C, 1 h minimum — case about 58–62 HRC. Core properties after case hardening (EN 10084 guidance, up to 11 mm): 835 MPa min yield, 1030–1320 MPa tensile, 9% min elongation — falling with section size. Sub-zero treatment: optional after quench to reduce retained austenite in the high-nickel case.

ENGINEERING NOTES
Weldability
Fair

Weldable in the annealed or normalised condition before carburising, with preheat and low-hydrogen consumables; nickel and chromium raise hardenability, so control cooling and stress relieve after welding. Do not weld carburised or case-hardened parts — the high-carbon case cracks. Mask weld areas from carburising if a weld must remain soft.

Filler metals
  • E8018-C2 · AWS A5.5 / SMAW3.5% Ni low-hydrogen electrode — matches the nickel steel before carburising
  • ER80S-Ni3 · AWS A5.28 / TIG / MIG3% Ni wire for GTAW / GMAW joining before case hardening
  • E7018 · AWS A5.1 / SMAWGeneral low-hydrogen electrode for non-critical repairs in soft condition
Machinability
Good

Machines well in the annealed condition (max 229 HB) — complete all heavy machining, gear cutting and drilling before carburising. Normalised material gives a consistent finish for gear hobbing. After case hardening, only grinding is practical. Allow grinding stock for distortion and case depth.

Applications

  • Heavy-duty gears, pinions and crown wheels for industrial and mining gearboxes
  • Crankshafts and camshafts needing hard bearing surfaces with a tough core
  • Gudgeon pins, piston pins and connecting rods with case-hardened ends
  • Steering worms, track rod pins and transmission shafts for heavy vehicles
  • Aircraft and motorsport transmission gears and splined shafts
  • Roller and ball bearing races of extra-light section
  • Cams, rollers and followers for heavy machinery in GCC workshops
  • Splined drive shafts and couplings for oilfield and process pumps
  • High-fatigue sprockets and chain wheels
  • Shock-loaded wear parts for mining and quarry equipment

Frequently Asked Questions

Quick answers on our grades, certification, supply and lead times.

Still have questions?

Our team responds fast with specifications, certification and stock availability.

Contact our team

EN36 / 655M13 is used for case-hardened parts that need a very hard surface and a strong, shock-resistant core: heavy-duty gears and pinions, crankshafts, camshafts, gudgeon pins, steering worms and aircraft or motorsport transmission parts. After carburising and hardening it gives a case of about 58–62 HRC over a core of roughly 850–1230 MPa. In the UAE and GCC, gear makers and heavy-equipment workshops use EN36 for mining, oilfield and industrial gearboxes.

Get in touch