Alloy Steel dealers in UAE

31CrMoV9 / 1.8519 Nitriding Steel | Supplier in UAE & GCC

31CrMoV9 / 1.8519 — Cr-Mo-V nitriding steel to EN 10085: 1100–1300 MPa Q&T core, about 800 HV nitrided case, stable to about 500°C; gears and shafts.

Industries Served

Automotive
Heavy Engineering
Manufacturing
Power Generation
Oil & Gas

Overview

31CrMoV9 (material number 1.8519) is a chromium-molybdenum-vanadium nitriding steel supplied to EN 10085 (also listed in ISO 683-5; formerly DIN 17211). It contains 0.27–0.34% carbon, 2.30–2.70% chromium, 0.15–0.25% molybdenum and 0.10–0.20% vanadium: chromium forms the hard nitrides that give the case its hardness, while vanadium refines the grain and molybdenum resists temper embrittlement during the long nitriding cycle. Supplied quenched and tempered, it offers one of the highest core strengths among nitriding steels — 1100–1300 MPa at 16–40 mm under EN 10085 +QT — so the case is well supported against high contact and bending loads. Gas nitriding produces a surface hardness of about 800 HV (650–800 HV depending on nitriding temperature), with no quench, scale-free surfaces and minimal distortion, and its strength and hardness remain stable in service up to a little over 500°C. Without aluminium, the nitrided case is tougher than that of aluminium-bearing grades. 31CrMoV9 is used for gears, connecting rods, shafts, valves, cylinders and high-load automotive and machine components. No BS or ASTM equivalent exists.

Nifty Alloys supplies 31CrMoV9 / 1.8519 nitriding steel from stock in Dubai, UAE, in round bar, quenched and tempered as standard, with annealed material on request. Bars are cut to length and dispatched with EN 10204 3.1 Mill Test Certificates as standard, certifying EN 10085 chemistry, condition, tensile, impact and hardness results with full traceability to the mill; EN 10204 3.2 third-party inspection is available on request. We deliver across the UAE within 24–48 hours, to Saudi Arabia, Kuwait, Qatar, Oman and Bahrain within 3–5 working days, and export to Europe, India and Africa. Send your size list or drawing to request a quote — quotations are turned around the same day.

Chemical Composition

0.3 %
C

Carbon

0.27 – 0.34 %

Si

Silicon

≤ 0.4 %

0.55 %
Mn

Manganese

0.4 – 0.7 %

2.5 %
Cr

Chromium

2.3 – 2.7 %

0.2 %
Mo

Molybdenum

0.15 – 0.25 %

0.15 %
V

Vanadium

0.1 – 0.2 %

P

Phosphorus

≤ 0.025 %

S

Sulfur

≤ 0.035 %

Typical value Range (min–max) Minimum (≥) Maximum (≤) Hover / tap for notes

Standard

EN 10085

EN

Revision: EN 10085:2001

Nitriding steels — Technical delivery conditions. Covers 31CrMoV9 (1.8519), 41CrAlMo7-10, 31CrMo12, 34CrAlMo5-10 and related grades in the quenched and tempered (+QT) and soft annealed (+A) conditions.

Current European standard for nitriding steels (EN 10085:2001); 31CrMoV9 is also listed in ISO 683-5. Formerly DIN 17211. +QT properties are size-banded from 16 to 250 mm.

Available Forms

Round Bar

16–250 mm. Diameter, Q&T; EN 10085 +QT properties defined to 250 mm; forged bar for larger sizes.

Stock & delivery

Stock location
Dubai, UAE
In stock
Quenched & Tempered (+QT) — standard stocked condition. Annealed (+A) on request. Nitriding by the customer.
Delivery UAE
24–48 hours
Delivery GCC
3–5 working days — Saudi Arabia, Kuwait, Qatar, Oman, Bahrain
Export
Europe, India, Africa on request
Quotation
Same-day quotation
Minimum order
No minimum order quantity for standard sizes

Key standards

EN 10085

Designations & Equivalents

StandardDesignationNotes
EN Name31CrMoV9EN 10085 / ISO 683-5 designation
EN / Werkstoff1.8519Material number
DINDIN 17211 31CrMoV9Superseded German standard
DIN30CrMoV9 / 1.7707 — comparable onlyQuenching-and-tempering steel of directly comparable chemistry — not a nitriding-steel designation
Common NameNo equivalent(BS / ASTM / JIS) No BS, ASTM or JIS equivalent is listed by producers
Common NameCrMoV nitriding steel / 1.8519 round bar / nitriding steelBuyer search terms

Compliance & Certification

StandardStatusNotes
EN 10204 3.1SuitableProvided as standard — EN 10085 chemistry, condition, tensile, impact and hardness.

Specifications

Mechanical Properties

Values per EN 10085. Bar length compares conditions within each row.

PropertyQuenched & Tempered (+QT) | EN 10085Annealed (+A) | EN 10085
Tensile Strength (UTS)1100–1300 MPaOver 16 to 40 mmEN 10085 range.–
Tensile Strength (UTS)1000–1200 MPaOver 40 to 100 mmEN 10085 range; 900–1100 MPa at 100–160 mm, 850–1050 MPa at 160–250 mm.–
Yield Strength (0.2% Proof Stress)900 MPaminOver 16 to 40 mmEN 10085 minimum; 800 at 40–100, 700 at 100–160, 650 at 160–250 mm.–
Elongation9 %minA (5.65√So) — over 16 to 40 mmEN 10085 minimum; 10% at 40–100, 11% at 100–160, 12% at 160–250 mm.–
Impact Energy (Charpy V-notch)25 Jmin+20°C, over 16 to 40 mmEN 10085 minimum; 30 / 35 / 40 J in larger sections.–
Hardness331–380 HBOver 16 to 40 mmFor information; 298–359 HB at 40–100, 271–331 at 100–160, 253–319 at 160–250 mm.248 HBmaxSoft annealed (+A)EN 10085 maximum (255 HB max for +S, treated for cold shearability).
Hardness800 HVminNitrided surfaceGuidance — EN 10085 information value (650–800 HV depending on nitriding temperature).–

Physical Properties

PropertyQuenched & Tempered (+QT) | EN 10085Annealed (+A) | EN 10085
Densityat 20°C7.73 g/cm³7.73 g/cm³
Modulus of Elasticityat 20°C210 GPa210 GPa
Thermal Conductivityat 20°C43 W/m·K43 W/m·K
Coefficient of Thermal Expansionat 20–100°C12.1 µm/m·°C12.1 µm/m·°C
Specific Heat Capacityat 20°C441 J/kg·K441 J/kg·K
Electrical Resistivityat 20°C0.19 µΩ·m0.19 µΩ·m

Service Conditions

Service Temperature

Max 500 °C

Notes

Producer data: strength and hardness remain stable under operating conditions up to a little over 500°C. Keep nitrided parts below the nitriding temperature to preserve the case. Impact values are moderate; specify impact testing for low-temperature service.

Corrosion Performance

General corrosion

Unprotected Q&T bar rusts in humid, coastal UAE and GCC conditions — store oiled. Not for aggressive chemical service without coating.

Pitting resistance

Base metal has no pitting resistance. The nitrided compound layer gives some improvement in atmospheric corrosion resistance compared with bare steel.

Additional notes

Not applicable — low-alloy steel (2.5% Cr is not enough for passivity).

Heat Treatment

HEAT TREATMENT GUIDE — 31CrMoV9 / 1.8519

Hot forming: 1100–850°C, then slow cooling in the furnace. Soft annealing: about 680–720°C, slow cool — 248 HB max (+A); 255 HB max when treated for cold shearability (+S). Hardening: about 870–930°C [VERIFY — range not confirmed] — quench in oil or polymer. Tempering: about 580–700°C, air cool — EN 10085 +QT ranges: 16–40 mm 1100–1300 MPa; 40–100 mm 1000–1200 MPa; 100–160 mm 900–1100 MPa; 160–250 mm 850–1050 MPa. Temper above the planned nitriding temperature. Stress relieving: after rough machining, below the tempering temperature. Nitriding: gas nitriding (or plasma / salt-bath) — surface about 800 HV (650–800 HV depending on nitriding temperature); no quench, minimal distortion. Surface alternatives: flame or induction hardening are also possible where a deeper hardened layer is preferred.

ENGINEERING NOTES
Weldability
Poor

Very difficult to weld and should not be used in welded constructions. If a repair is unavoidable, weld before nitriding with high preheat, low-hydrogen Cr-Mo consumables, controlled interpass temperature and post-weld stress relief below the tempering temperature [VERIFY — procedure parameters not confirmed]. Never weld nitrided surfaces.

Filler metals
  • E9018-B3 · AWS A5.5 / SMAW2.25Cr-1Mo low-hydrogen electrode — nearest Cr-Mo match for repairs before nitriding
  • ER90S-B3 · AWS A5.28 / TIG / MIG2.25Cr-1Mo wire; high preheat and stress relief required
  • E309L-16 · AWS A5.4 / SMAWAustenitic electrode for non-load-bearing attachments
Machinability
Fair

Machine in the Q&T condition (about 331–380 HB at 16–40 mm, for information) with carbide tooling, or annealed (248 HB max) for heavy roughing. Stress relieve after rough machining, finish-machine or grind, then nitride — dimensional change during nitriding is very small. After nitriding only light grinding or lapping is practical.

Applications

  • Nitrided gears and pinions for industrial and marine gearboxes
  • Connecting rods, crankshafts and camshafts for engines
  • Drive shafts and transmission shafts under high bending loads
  • Valves, gate valves and superheated-steam valve components
  • Cylinders and cylinder liners for combustion engines
  • Rotor shafts, discs and rings for gear and power-transmission drives
  • Hydraulic components and pump shafts in GCC process plants
  • Spindles and precision machine-tool parts
  • Extruder and plastics-processing components
  • High-temperature wear parts operating up to about 500°C

Frequently Asked Questions

Quick answers on our grades, certification, supply and lead times.

Still have questions?

Our team responds fast with specifications, certification and stock availability.

Contact our team

31CrMoV9 / 1.8519 is used for nitrided components that combine high surface wear resistance with a very strong core: gears and pinions, connecting rods, crankshafts, drive shafts, valves and gate valves, superheated-steam fittings, engine cylinders and liners, and gearbox rotor shafts. After nitriding the surface reaches about 800 HV. In the UAE and GCC it is used for gearbox, pump and valve components.

Get in touch

Elevateyourprojectswithoursuperiorsteel