Overview

AISI 4140 alloy steel (DIN 42CrMo4, EN 1.7225, BS 970 709M40 / EN19, JIS SCM440, UNS G41400) is a medium-carbon chromium-molybdenum through-hardening steel containing 0.38–0.43% carbon, 0.80–1.10% chromium and 0.15–0.25% molybdenum, used for highly stressed shafts, gears, oilfield tools and pressure-containing components. Chromium gives a deep, predictable hardening response in oil, which is why EN 10083-3 specifies quenched and tempered properties up to a 250 mm ruling section. Molybdenum strengthens the tempered martensite, slows softening at high tempering temperatures and suppresses temper embrittlement. Quenched and tempered to EN 10083-3, 42CrMo4 develops 900–1100 MPa tensile strength and at least 650 MPa 0.2% proof stress at 40–100 mm, while BS 970 709M40 Condition T (EN19T) bar is supplied at 850–1000 MPa and 248–302 HB. For H2S service the grade is tempered to 80 ksi (552 MPa) minimum yield at a maximum of 22 HRC per NACE MR0175 / ISO 15156-2; for sweet-service downhole tools it is tempered to 110 ksi (758 MPa) minimum yield.

Nifty Alloys supplies AISI 4140 / 42CrMo4 from stock in Dubai, UAE, in quenched and tempered round bar, with flat bar, square bar, plate and block, open-die forgings, rings and hollow forgings to order. Material is available in the EN 10083-3 +QT / 709M40T condition, annealed or normalised for customer heat treatment, and in 80K NACE MR0175 and 110K yield conditions for oil and gas tools. Every delivery is certified to EN 10204 3.1 with full heat traceability; EN 10204 3.2 third-party inspection and ultrasonic testing are available on request. We deliver within the UAE in 24–48 hours and across the GCC to Saudi Arabia, Kuwait, Qatar, Oman and Bahrain, and export to Europe, India and Africa. As an alloy steel supplier in the UAE, we issue same-day quotations — contact our team to request a quote.

Chemical Composition

0.41 %
C

Carbon

0.38 – 0.43 %

0.25 %
Si

Silicon

0.15 – 0.35 %

0.8 %
Mn

Manganese

0.75 – 1 %

1 %
Cr

Chromium

0.8 – 1.1 %

0.2 %
Mo

Molybdenum

0.15 – 0.25 %

P

Phosphorus

≤ 0.035 %

S

Sulfur

≤ 0.04 %

Ni

Nickel

≤ 0.25 %

Cu

Copper

≤ 0.35 %

Typical value Range (min–max) Minimum (≥) Maximum (≤) Hover / tap for notes

Standard

EN 10083-3

EN

Revision: EN 10083-3:2006

Steels for quenching and tempering — Part 3: Technical delivery conditions for alloy steels. Defines 25CrMo4 (1.7218) chemistry and +QT properties by ruling section.

European reference for 25CrMo4; supersedes DIN 17200. Chemistry differs from AISI 4130 (C 0.22–0.29%, Mn 0.60–0.90%, Cr 0.90–1.20%, Mo 0.15–0.30%) — dual certification requires a heat inside the overlap.

Available Forms

Round Bar

10–500 mm. Diameter. Q&T to EN 10083-3 up to 250 mm; above 250 mm as forged and Q&T bar to EN 10250-3. Cut to length in Dubai. [VERIFY against stock list]

Flat Bar

10–200 mm. Thickness; widths to 600 mm, larger cut from plate. [VERIFY against stock list]

Square Bar

20–300 mm. Across flats. [VERIFY against stock list]

Plate / Block

20–400 mm. Thickness; length and width cut to size. [VERIFY against stock list]

Forging / Ring Forging

100–1500 mm. Forging OD / ring OD; to drawing. Hollow forgings by bore size. [VERIFY against forge capacity]

Stock & delivery

Stock location
Dubai, UAE
In stock
Q&T round bar to EN 10083-3 +QT / 709M40T (EN19T) — stock. 80K NACE and 110K Q&T round bar, annealed and normalised bar, flat bar, square bar, plate / block and forgings — stock or to order. [VERIFY — confirm against current stock list]
Delivery UAE
24–48 hours
Delivery GCC
3–5 working days — Saudi Arabia, Kuwait, Qatar, Oman, Bahrain
Export
Europe, India, Africa on request
Quotation
Same-day quotation
Minimum order
No minimum order quantity for standard sizes

Key standards

EN 10083-3

Designations & Equivalents

StandardDesignationNotes
AISI / SAE4140Primary designation
UNSG41400Unified Numbering System; H41400 = 4140H hardenability-band variant
EN / Werkstoff1.7225European material number
DIN42CrMo4German standard designation — primary DIN/EN used throughout this page
EN Name42CrMo4EN 10083-3 steel name
BS709M40BS 970 designation; EN19 in BS 970:1955. Condition T = "EN19T" (850–1000 MPa)
BSEN19 / EN19TLegacy BS 970:1955 name — highest search volume in UAE, GCC and India
BS708M40EN19A. Mo 0.15–0.25%, the BS chemistry closest to ASTM 4140. Has its own approved page — /alloy-steel/708m40-en19a-alloy-steel
JISSCM440Japanese Industrial Standard JIS G4053
ISO42CrMo4ISO 683-2 designation
ASTMA29 / A322ASTM bar standards defining 4140 chemistry
Common Name42CrMoS4 (1.7227)Controlled-sulphur (0.020–0.040% S) free-machining variant to EN 10083-3
Common Name42CD4 / SS 2244 / 40HM / 42CrMoFrench AFNOR (legacy), Swedish SS, Polish PN and Chinese GB equivalents
Common NameChromoly / CrMo steel / 4140 HTTrade and shop-floor names; "4140 HT" = pre-hardened Q&T bar

Compliance & Certification

StandardStatusNotes
EN 10204 3.1SuitableMill Test Certificate provided as standard with every delivery — heat chemistry, tensile, yield, elongation, reduction of area, hardness and, where ordered, Charpy results.
EN 10204 3.2ConditionalAvailable on request — specify at order stage. Third-party inspector witnesses testing; additional lead time applies.
NACE MR0175 / ISO 15156ConditionalCompliant ONLY in SpecSheet 4 (Q&T 80K): quenched and tempered, hardness ≤22 HRC (≤237 HBW) across the section, Ni <1%. Welds PWHT to ≤250 HV10. NOT compliant: 110K (28–36 HRC) and EN 10083-3 +QT in sections where hardness exceeds 22 HRC. The 26 HRC allowance in ISO 15156-2 Table A.3 applies to qualified tubulars, not solid bar.
NACE MR0103Requires ConfirmationRefinery sour service: the 80K ≤22 HRC condition normally satisfies MR0103 / ISO 17945 hardness limits — confirm against the refinery material specification at order stage.
API 6ARequires Confirmation80K material exceeds the 75K material designation minimums (517 MPa YS, 655 MPa UTS). PSL, QTC size, impact temperature class and NDE must be stated on the order.
ASTM A388 / EN 10228-3ConditionalUltrasonic testing of bar and forgings on request; acceptance class to be agreed at order.

Specifications

Mechanical Properties

Values per EN 10083-3. Bar length compares conditions within each row.

PropertyQuenched & Tempered | EN 10083-3 +QT / BS 970 709M40TAnnealed | EN 10083-3 +ANormalised | ASTM A29 / A29MQ&T 110K Yield (Non-Sour) | ASTM A29 / A29MQ&T 80K Yield, NACE MR0175 (≤22 HRC) | ASTM A29 / A29M
Tensile Strength (UTS)1100–1300 MPaRoom temp, longitudinal, d ≤16 mmEN 10083-3 +QT655 MPatypicalRoom temp, longitudinalTypical — not specified1020 MPatypicalRoom temp, longitudinal, ~25 mm sectionTypical — not specified [VERIFY — handbook typical value]862 MPaminTypical 950 MPaRoom temp, longitudinal, T/4 or mid-radius125 ksi min (purchase-spec minimum) [VERIFY vs customer spec]655 MPaminTypical 760 MPaRoom temp, longitudinal, T/4 or mid-radius95 ksi min (purchase-spec minimum); typical value indicative
Tensile Strength (UTS)1000–1200 MPaRoom temp, longitudinal, 16 < d ≤ 40 mmEN 10083-3 +QT––––
Tensile Strength (UTS)900–1100 MPaRoom temp, longitudinal, 40 < d ≤ 100 mmEN 10083-3 +QT — website headline band––––
Tensile Strength (UTS)800–950 MPaRoom temp, longitudinal, 100 < d ≤ 160 mmEN 10083-3 +QT––––
Tensile Strength (UTS)750–900 MPaRoom temp, longitudinal, 160 < d ≤ 250 mmEN 10083-3 +QT––––
Tensile Strength (UTS)850–1000 MPaRoom temp, longitudinal, BS 970 709M40 Condition TEN19T — within limiting ruling section––––
Yield Strength (0.2% Proof Stress)900 MPaminRoom temp, longitudinal, d ≤16 mmEN 10083-3 +QT415 MPatypicalRoom temp, longitudinalTypical — not specified655 MPatypicalRoom temp, longitudinal, ~25 mm sectionTypical — not specified [VERIFY — handbook typical value]758 MPaminTypical 820 MPaRoom temp, longitudinal, T/4 or mid-radius110 ksi min552 MPaminTypical 620 MPaRoom temp, longitudinal, T/4 or mid-radius80 ksi min; exceeds API 6A 75K (517 MPa)
Yield Strength (0.2% Proof Stress)750 MPaminRoom temp, longitudinal, 16 < d ≤ 40 mmEN 10083-3 +QT––––
Yield Strength (0.2% Proof Stress)650 MPaminRoom temp, longitudinal, 40 < d ≤ 100 mmEN 10083-3 +QT––––
Yield Strength (0.2% Proof Stress)550 MPaminRoom temp, longitudinal, 100 < d ≤ 160 mmEN 10083-3 +QT––––
Yield Strength (0.2% Proof Stress)500 MPaminRoom temp, longitudinal, 160 < d ≤ 250 mmEN 10083-3 +QT––––
Yield Strength (0.2% Proof Stress)680 MPaminRoom temp, longitudinal, BS 970 709M40 Condition TEN19T [VERIFY — published stockist values range 650–680 MPa]––––
Elongation12 %minA5 (5.65√S0), 40 < d ≤ 100 mmEN 10083-3: 10 / 11 / 12 / 13 / 14% min for the five bands ≤16 to 250 mm25 %typical50 mm gauge lengthTypical — not specified17.7 %typical50 mm gauge lengthTypical — not specified [VERIFY — handbook typical value]15 %minTypical 18 %50 mm gauge lengthPurchase-spec minimum [VERIFY vs customer spec]18 %minTypical 22 %50 mm gauge lengthPurchase-spec minimum; API 6A 75K requires 17% [VERIFY vs customer spec]
Elongation13 %minBS 970 709M40 Condition TEN19T––––
Reduction of Area50 %minRoom temp, longitudinal, 40 < d ≤ 100 mmEN 10083-3: 40 / 45 / 50 / 50 / 55% min for the five bands56 %typicalLongitudinalTypical — not specified46.8 %typicalLongitudinalTypical — not specified [VERIFY — handbook typical value]45 %minTypical 55 %LongitudinalPurchase-spec minimum [VERIFY vs customer spec]35 %minTypical 55 %LongitudinalAPI 6A 75K minimum; typical value indicative
Impact Energy (Charpy)35 JminKV, +20°C, 16 < d ≤ 250 mmEN 10083-3: 30 J min for d ≤16 mm–––V-notch, per ordered temperaturePer customer spec (commonly −20°C) [VERIFY — enter value when PO specifies]–V-notch, per ordered temperature classPer customer spec / API 6A temperature class (typically −29°C or −46°C) [VERIFY — enter value when PO specifies]
Impact Energy (Charpy)50 JminKCV / Izod, BS 970 709M40 Condition TEN19T [VERIFY — source not confirmed against BS 970-1]––––
Hardness271–331 HBtypical40 < d ≤ 100 mmInformative only in EN 10083-3 (not a specified requirement)241 HBmaxTypical 197 HBSurfaceEN 10083-3 +A max (specified); 197 HB typical full anneal302 HBtypicalSurface, ~25 mm sectionTypical; heavier sections ~270 HB285–341 HBTypical 311 HBSurface and section survey≈30–36 HRC. Not sour-service compliant22 HRCmaxTypical 20 HRCSurface and section surveyNACE MR0175 / ISO 15156-2 maximum; ≤237 HBW
Hardness248–302 HBSurface, BS 970 709M40 Condition TEN19T specified hardness range––––

Physical Properties

PropertyQuenched & Tempered | EN 10083-3 +QT / BS 970 709M40TAnnealed | EN 10083-3 +ANormalised | ASTM A29 / A29MQ&T 110K Yield (Non-Sour) | ASTM A29 / A29MQ&T 80K Yield, NACE MR0175 (≤22 HRC) | ASTM A29 / A29M
Densityat 20°C7.85 g/cm³7.85 g/cm³7.85 g/cm³–7.85 g/cm³
Modulus of Elasticityat 25°C205 GPa205 GPa205 GPa–205 GPa
Thermal Conductivityat 100°C42.6 W/m·K42.6 W/m·K42.6 W/m·K–42.6 W/m·K
Coefficient of Thermal Expansionat 20–100°C12.2 µm/m·°C12.2 µm/m·°C12.2 µm/m·°C–12.2 µm/m·°C
Specific Heat Capacityat 20°C473 J/kg·K473 J/kg·K473 J/kg·K–473 J/kg·K
Melting Point / Rangeat Solidus1416 °C1416 °C1416 °C–1416 °C
ISO 9001:2015at Quality Management System — procurement, stock management, supply.–––2026 Check current certificate–
AEO (Authorised Economic Operator)at Customs compliance for UAE and GCC trade.––––UAE Federal Customs Authority–
1–––709 Locked decision kept — EN19 stays in slug, name and H1 (highest search volume). 708M40 is listed in aliases with a pointer to its own page, and FAQ #11 explains the difference. Confirm whether the separate 708M40 page is still wanted.–
2–––62 Cosmetic — update the character count in both reference files.–
3–––4140 Replace it with this document as the 4140 master so the sample and live data do not diverge.–
4–––193 No action unless a B7 SpecSheet is wanted here.–
5–––7.7 Confirm against the current stock list before publishing.–

Service Conditions

Service Temperature

Min -29 °CMax 400 °C

Notes

Lower limit applies only to Q&T material Charpy-tested at or below the design minimum temperature (−29°C corresponds to API 6A temperature class L). Without impact testing at temperature, do not assume toughness below 0°C; lower temperatures (e.g. −46°C) require qualification on the order [VERIFY per project]. Upper limit: above about 400°C Q&T 4140 loses strength progressively and service approaching the tempering temperature (540–680°C) over-tempers the structure. 4140 is not a creep-resistant grade — use 1¼Cr-½Mo or 2¼Cr-1Mo pressure-vessel steels for sustained elevated-temperature duty.

Corrosion Performance

General corrosion

Protect with oil, VCI wrapping or primer during storage. Service protection: zinc-nickel or zinc plating, phosphate and oil, black oxide, or hard chrome for piston rods. At hardness above about 31 HRC, bake electroplated parts at 190–220°C for at least 4 h to relieve hydrogen embrittlement. In H2S-containing environments, hardness above 22 HRC risks sulphide stress cracking — specify the 80K NACE condition. High-strength conditions (110K and above) are also susceptible to hydrogen embrittlement from cathodic protection; avoid over-protection.

Pitting resistance

No meaningful pitting resistance. Corrodes readily in seawater, splash zones, chloride-bearing humidity and condensing coastal atmospheres typical of the GCC. Unprotected bar rusts within days in coastal storage.

Additional notes

Not applicable — alloy steel. ~1% Cr is far below the ~10.5% needed for passivity.

Heat Treatment

HEAT TREATMENT GUIDE — AISI 4140 / 42CrMo4 / EN19

Forging: 1150–850°C — Do not forge below 850°C; slow cool in sand or furnace — Follow with normalising or annealing before machining or hardening Soft annealing (+A): 680–720°C — 2–4 h; furnace cool to ~600°C, then air — ≤241 HB per EN 10083-3; best machinability Normalising (+N): 840–880°C — ~1 h per 25 mm section; still-air cool — Refined, uniform structure; typical 270–320 HB. Temper at 600–650°C if machining follows Hardening: 820–860°C (EN 10083-3) — ~30 min per 25 mm at temperature; oil quench (water or polymer only for simple shapes — crack risk) — As-quenched hardness ~54–59 HRC in small sections [typical] Tempering (+QT): 540–680°C (EN 10083-3) — Temper immediately after quench; minimum 2 h; air cool — Sets final strength. Avoid 250–400°C (tempered-martensite embrittlement) Tempering — 80K NACE: ≥620°C, typically 650–700°C — Minimum 2 h; air cool — ≤22 HRC; 552 MPa min yield. Minimum 620°C is standard sour-service practice [VERIFY against project specification] Tempering — 110K: 560–620°C [typical] — Minimum 2 h; air cool — ~285–341 HB; 758 MPa min yield Stress relieving: 550–650°C — 1–2 h; furnace or still-air cool — At least 30°C below the last tempering temperature Induction / flame hardening: 850–880°C surface — Water or polymer spray quench; temper 150–200°C — Surface ~50–55 HRC on Q&T core [typical] Gas nitriding: 500–530°C — 20–70 h depending on case depth — Case ~500–650 HV [typical]. Pre-temper at least 30°C above nitriding temperature

ENGINEERING NOTES
Weldability
Fair

AISI 4140 is weldable only under a qualified procedure: its carbon equivalent (CEV IIW) is typically 0.80–0.90, so the HAZ forms hard martensite and is prone to hydrogen cracking. Use low-hydrogen consumables (H4) baked per manufacturer. Preheat 250–350°C, using the upper end above 25 mm section, and hold interpass at or above preheat (max 400°C). If PWHT cannot follow immediately, post-heat at 250–300°C for 2–4 h to diffuse hydrogen. PWHT at 550–650°C, at least 30°C below the original tempering temperature so base-metal properties are not lost. For NACE MR0175 service, PWHT at 620°C minimum and verify weld metal and HAZ hardness ≤250 HV10 per ISO 15156-2. Austenitic or nickel-base fillers allow preheat to be reduced by roughly 50–75°C but give non-matching strength. Do not weld in the fully hardened condition.

Filler metals
  • E8018-B2 H4R · AWS A5.5 / SMAW1¼Cr-½Mo low-hydrogen electrode; matching chemistry, recommended where PWHT follows
  • E10018-D2 H4R · AWS A5.5 / SMAWMn-Mo higher-strength electrode for 110K repair and joint welding
  • ER80S-D2 · AWS A5.28 / GMAW-GTAWMn-Mo wire; widely used for 4130/4140 oilfield fabrications, root and fill passes
  • ER80S-B2 · AWS A5.28 / GMAW-GTAW1¼Cr-½Mo wire; matches base Cr-Mo where weld response to PWHT must track base metal
  • E7018-1 H4R · AWS A5.1 / SMAWNon-matching strength; buttering layers and low-stress attachments only
  • ERNiCr-3 · AWS A5.14 / GTAWNickel-base for dissimilar joints or repairs where full PWHT is not possible; non-matching strength — confirm design
Machinability
Good

Best machined annealed (≤241 HB), where machinability is about 65% of AISI 1212 [typical]. Q&T bar at 248–330 HB (EN19T / +QT) machines well with coated carbide (ISO P20–P35 grades); this is the usual route for finished parts that are not re-hardened. Above about 35 HRC use CBN or ceramic for finish turning and rigid set-ups. For heavy-volume turning, 42CrMoS4 (1.7227, 0.020–0.040% S) improves chip breaking. Rough-machine before hardening and leave grinding allowance for distortion; stress relieve at 550–650°C after heavy roughing of Q&T stock.

Applications

  • Drill string subs, crossovers, pup joints and stabiliser bodies for oilfield drilling
  • Wellhead, Christmas tree and valve body components in 80K NACE condition for sour service
  • Mandrels, packer components and downhole tool housings in 110K condition for sweet wells
  • Hydraulic cylinder piston rods, rams and gland nuts for heavy plant and offshore equipment
  • Drive shafts, axles, spindles and torsion bars for automotive and industrial machinery
  • Gears, pinions, sprockets and couplings, often induction hardened on tooth flanks
  • Pump and compressor shafts for petrochemical plants and GCC desalination facilities
  • Crane hooks, lifting pins, shackles and clevis components for construction and port handling
  • Die holders, bolsters, back-up plates and mould frames in pre-hardened Q&T condition
  • Excavator pins, bushings and track components for mining and earthmoving equipment
  • Nitrided spindles, cams and wear-critical shafts needing a hard case on a tough core

Related grades in Alloy Steel

Frequently Asked Questions

Quick answers on our grades, certification, supply and lead times.

Still have questions?

Our team responds fast with specifications, certification and stock availability.

Contact our team

AISI 4140 is used for highly stressed shafts, gears, axles, hydraulic rods and oil and gas tools that need high strength with good toughness. In oil and gas it is machined into drill string subs, crossovers, mandrels, valve bodies and wellhead components, using the 80K NACE condition for sour service and 110K for sweet wells. In automotive and heavy engineering it is used for crankshafts, drive shafts, spindles, couplings and induction-hardened gears. It is also used for crane hooks, lifting pins, excavator pins, die holders and mould frames. Across the UAE and GCC, 4140 is one of the most commonly specified alloy steels for oilfield and plant maintenance parts.