Alloy Steel dealers in UAE

EN30B / 835M30 / 30NiCrMo16-6 Alloy Steel | Supplier in UAE & GCC

EN30B / 835M30 (30NiCrMo16-6) — 4% Ni-Cr-Mo air-hardening steel: 1550 MPa min in Condition Z to 150 mm, minimal distortion; critical shafts and gears.

Industries Served

Oil & Gas
Aerospace & Defence
Automotive
Heavy Engineering
Mining
Manufacturing

Overview

EN30B (BS 970 835M30, closely related to EN 30NiCrMo16-6 / 1.6747, French 30NCD16) is a 4% nickel-chromium-molybdenum air-hardening alloy steel, supplied in Europe to EN ISO 683-2 (formerly EN 10083-3). Its 0.26–0.34% carbon, 3.90–4.30% nickel, 1.10–1.40% chromium and 0.20–0.35% molybdenum give the highest hardenability of the BS 970 through-hardening steels — small and medium sections harden fully in still air, and larger sections in oil, so distortion and quench-cracking risk are minimal. Hardened and low-temperature tempered to Condition Z, EN30B reaches 1550 MPa minimum tensile strength, 1125 MPa minimum proof stress and 444 HB minimum through a 150 mm ruling section, while the high nickel content keeps useful toughness at that strength. It is normally supplied annealed (270 HB maximum) so that parts can be machined first and then air hardened. EN30B is chosen for safety-critical, highly stressed parts — aircraft and motorsport gears and shafts, crankshafts, high-strength studs, drill bits and heavy-duty tooling. BS 970 is withdrawn; 30NiCrMo16-6 is the current EN designation.

Nifty Alloys supplies EN30B / 835M30 / 30NiCrMo16-6 alloy steel from stock in Dubai, UAE, in round bar, annealed as standard for machining before heat treatment, with Condition Z hardened and tempered bar on request. Bars are cut to length and dispatched with EN 10204 3.1 Mill Test Certificates as standard, certifying chemistry (835M30 or 30NiCrMo16-6 as supplied), condition and hardness, with tensile and impact results for heat-treated bar; EN 10204 3.2 third-party inspection is available on request. We deliver across the UAE within 24–48 hours, to Saudi Arabia, Kuwait, Qatar, Oman and Bahrain within 3–5 working days, and export to Europe, India and Africa. Send your size list or drawing to request a quote — quotations are turned around the same day.

Chemical Composition

0.3 %
C

Carbon

0.26 – 0.34 %

Si

Silicon

0.1 – 0.35 %

Mn

Manganese

0.45 – 0.7 %

4.1 %
Ni

Nickel

3.9 – 4.3 %

1.25 %
Cr

Chromium

1.1 – 1.4 %

0.28 %
Mo

Molybdenum

0.2 – 0.35 %

P

Phosphorus

≤ 0.025 %

S

Sulfur

≤ 0.025 %

Typical value Range (min–max) Minimum (≥) Maximum (≤) Hover / tap for notes

Standard

EN ISO 683-2

EN

Revision: EN ISO 683-2:2018

Heat-treatable steels, alloy steels and free-cutting steels — Part 2: Alloy steels for quenching and tempering.

European standard governing 25CrMo4 (1.7218). Defines chemical composition, mechanical properties per condition, and delivery requirements. Replaces former EN 10083-1.

Available Forms

Round Bar

20–400 mm. Diameter, annealed; Condition Z guaranteed to 150 mm ruling section. [VERIFY — stock range not confirmed]

Stock & delivery

Stock location
Dubai, UAE
In stock
Annealed (270 HB max) — standard stocked condition. Hardened & Tempered Condition Z on request.
Delivery UAE
24–48 hours
Delivery GCC
3–5 working days — Saudi Arabia, Kuwait, Qatar, Oman, Bahrain
Export
Europe, India, Africa on request
Quotation
Same-day quotation
Minimum order
No minimum order quantity for standard sizes

Key standards

EN ISO 683-2

Designations & Equivalents

StandardDesignationNotes
BSEN30B / EN30BZOriginal BS 970:1955 designation; Z = strength condition
BS835M30 / 835M30ZBS 970 designation (withdrawn standard) — governing chemistry
EN Name30NiCrMo16-6EN ISO 683-2 (formerly EN 10083-3) — closely related; Ni 3.30–4.30, Mo 0.30–0.60
EN / Werkstoff1.674730NiCrMo16-6 material number
Common Name30NCD16 / 35NCD16(AFNOR / AIR) French designations (aerospace AIR 30 NCD 16)
Common NameEN30B round bar / 4% nickel chrome moly steel / air hardening steel / EN30B Condition ZBuyer search terms

Compliance & Certification

StandardStatusNotes
EN 10204 3.1SuitableProvided as standard — chemistry, condition and hardness; tensile and impact for heat-treated bar.
EN 10204 3.2ConditionalAvailable on request with independent third-party inspection — specify at order stage.
NACE MR0175 / ISO 15156Not Applicable — Not acceptable under ISO 15156-2 general requirements: carbon and low-alloy steels must contain < 1% Ni (EN30B has 3.90–4.30%), and hardened conditions far exceed 22 HRC. Not a sour-service grade.

Specifications

Mechanical Properties

Values per EN ISO 683-2. Bar length compares conditions within each row.

PropertyAnnealed (+A) | EN ISO 683-2H&T Condition Z | BS 970-1
Hardness270 HBmaxSoft annealed (+A)EN ISO 683-2 maximum for 30NiCrMo16-6 (835M30 annealed: about 269 HB max).444 HBminCondition ZBS 970 minimum (about 47 HRC).
Tensile Strength (UTS)1080–1230 MPaAfter +QT — 16 to 100 mmPublished 30NiCrMo16-6 +QT range — guidance [VERIFY — size band per EN ISO 683-2 not confirmed].1550 MPaminCondition Z — up to 150 mm LRSBS 970 minimum.
Yield Strength (0.2% Proof Stress)880 MPaminAfter +QT — 16 to 100 mmPublished 30NiCrMo16-6 +QT minimum — guidance.1125 MPaminCondition ZBS 970 minimum (yield point Re: 1235 MPa min).
Impact Energy (Charpy V-notch)35 JminAfter +QT — room tempPublished 30NiCrMo16-6 +QT minimum — guidance.16 JminRoom temp, KCVPublished minimum (some sources: 11 J).
Elongation–7 %minA (5.65√So)BS 970 minimum.

Physical Properties

PropertyAnnealed (+A) | EN ISO 683-2H&T Condition Z | BS 970-1
Densityat 20°C7.85 g/cm³7.85 g/cm³
Modulus of Elasticityat 20°C205 GPa205 GPa
Thermal Conductivityat 20°C30 W/m·K30 W/m·K
Coefficient of Thermal Expansionat 20–100°C11.5 µm/m·°C11.5 µm/m·°C

Service Conditions

Service Temperature

Max 200 °C

Notes

Condition Z is tempered at a low temperature, so service above about 200°C softens it. Material tempered higher for lower strength can serve hotter, but never above its tempering temperature. The 4% nickel content gives good toughness at sub-zero temperatures; specify impact testing at the service temperature.

Corrosion Performance

General corrosion

Corrodes like other low-alloy steels. Condition Z (≥ 1550 MPa) is highly susceptible to hydrogen embrittlement and stress corrosion — avoid acid pickling and electroplating, or bake immediately after plating.

Pitting resistance

No pitting resistance. Store oiled and under cover in the humid, coastal UAE and GCC climate; protect finished parts with coatings or lubricants.

Additional notes

Not applicable — low-alloy steel.

Heat Treatment

HEAT TREATMENT GUIDE — EN30B / 835M30 / 30NiCrMo16-6

Forging: 850–1100°C; cool very slowly (furnace or ash) — the steel air-hardens. Soft annealing: 635–650°C, do not exceed 660°C — slow cool — 270 HB max (+A). A double anneal improves machinability. Normalise / temper / stress relieve: austenitise 850–865°C, air cool; temper about 530°C; stress relieve about 500°C. Hardening: austenitise 840–865°C — cool in still or forced air (small and medium sections) or quench in oil (large sections). Tempering: low-temperature temper for Condition Z (1550 MPa min, 444 HB min); higher tempering temperatures (about 540–630°C) give the EN ISO 683-2 +QT strength ranges. Avoid the temper-embrittlement range [VERIFY — exact range not confirmed]. Conditions (BS 970): Y 1225–1375 MPa (363–429 HB) and Z 1550 MPa min (444 HB min), both to 150 mm limiting ruling section. Distortion: air hardening gives minimal distortion — finish-machine before hardening, leaving grinding allowance only.

ENGINEERING NOTES
Weldability
Poor

Not recommended for welding — carbon equivalent (CEV) is about 1.07, and because the steel air-hardens, the weld and HAZ form hard martensite even with slow cooling. If welding is unavoidable, weld annealed material with high preheat, dry low-hydrogen consumables and controlled interpass temperature [VERIFY — procedure parameters not confirmed], then re-anneal or re-harden and temper. Never weld Condition Z parts.

Filler metals
  • E12018-M · AWS A5.5 / SMAWHighest-strength low-hydrogen electrode — repairs to annealed material only, followed by re-heat treatment
  • ER120S-1 · AWS A5.28 / TIG / MIGHigh-strength wire for repair of annealed material; preheat and re-heat treatment essential
  • E8018-B2 · AWS A5.5 / SMAWUnder-matching electrode for non-load-bearing repairs
Machinability
Fair

Machine in the annealed condition (270 HB max) with carbide tooling, rigid set-ups and generous coolant, then air harden — the low distortion of air hardening allows near-final machining before heat treatment. Condition Z (444 HB min) is practically limited to grinding and hard turning with ceramic or CBN tools. A double anneal at 635–650°C improves machinability.

Applications

  • Aircraft and defence transmission gears, shafts and actuator parts
  • Motorsport crankshafts, camshafts, half-shafts and gearbox components
  • High-strength studs, bolts and tie rods for critical joints
  • Drill bits, rock-drilling components and oilfield tool parts
  • Heavy-duty gears and pinions for mining and industrial gearboxes
  • Press tooling, punches, shear blades and die components
  • Large crankshafts and connecting rods for engines and compressors
  • Heavy shafts for GCC process plant where distortion must be minimal
  • Plastic mould bolsters and high-strength mould components
  • Safety-critical parts needing air hardening after final machining

Related grades in Alloy Steel

Frequently Asked Questions

Quick answers on our grades, certification, supply and lead times.

Still have questions?

Our team responds fast with specifications, certification and stock availability.

Contact our team

EN30B / 835M30 is used for safety-critical, highly stressed parts that need very high strength with minimal heat-treatment distortion: aircraft and motorsport gears and shafts, crankshafts, high-strength studs, drill bits, press tooling and heavy-duty gears. Hardened to Condition Z it reaches 1550 MPa minimum tensile strength through a 150 mm section. In the UAE and GCC it is used for oilfield tooling, heavy machinery and precision engineering parts.

Get in touch

Elevateyourprojectswithoursuperiorsteel