080M50 / EN43A / C50 Medium Carbon Steel | Supplier in UAE & GCC

080M50 / EN43A / C50 — 0.50% carbon steel between EN8 and EN9: good strength and wear resistance, flame or induction hardenable; shafts, gears, piston rods.

Industries Served

Manufacturing
Automotive
Heavy Engineering
Construction

Overview

080M50 carbon steel (formerly BS 970 EN43A; EN ISO 683-1 C50E / 1.1206; DIN C50 / Ck50; AISI 1050; JIS S50C) is a medium-carbon non-alloy steel containing 0.47–0.55% carbon (0.45–0.55% to BS 970) and 0.60–0.90% manganese, with residual chromium, molybdenum and nickel held to low limits. It sits between EN8 / 080M40 and EN9 / 070M55, giving higher strength, hardness and wear resistance than EN8 while remaining more ductile than EN9. It is normally supplied normalised — 650 MPa minimum tensile and 355 MPa yield up to 16 mm, falling to 590 / 290 MPa at 100–250 mm under EN ISO 683-1 — and can be quenched and tempered to 650–900 MPa depending on section. Its limited hardenability restricts through-hardening to smaller sections, but it responds well to flame and induction hardening for a hard, wear-resistant surface over a tough core, and is a cost-effective alternative where alloy steel is not justified. Soft-annealed material (217 HB maximum) machines readily. As a carbon steel it needs surface protection. Typical uses are shafts and axles, gears, sprockets and cams, piston rods, crankshafts, spindles, couplings, rollers and wear parts.

Nifty Alloys supplies 080M50 / EN43A / C50 carbon steel from Dubai, UAE, in round bar and flat bar, normalised as standard and quenched and tempered on request. Every supply carries an EN 10204 3.1 Mill Test Certificate as standard; EN 10204 3.2 third-party inspection is available on request. We deliver across the UAE within 24–48 hours, to Saudi Arabia, Kuwait, Qatar, Oman and Bahrain within 3–5 working days, and export to Europe, India and Africa. Send your size list to request a quote — quotations are turned around the same day.

Chemical Composition

0.5 %
C

Carbon

0.47 – 0.55 %

0.25 %
Si

Silicon

≤ 0.4 %

0.75 %
Mn

Manganese

0.6 – 0.9 %

P

Phosphorus

≤ 0.03 %

S

Sulfur

≤ 0.035 %

Cr

Chromium

≤ 0.4 %

Mo

Molybdenum

≤ 0.1 %

Ni

Nickel

≤ 0.4 %

Typical value Range (min–max) Minimum (≥) Maximum (≤) Hover / tap for notes

Standard

EN ISO 683-1

Other

Revision: EN ISO 683-1:2018

Available Forms

Flat Bar

10–100 mm. Thickness; width to order. [VERIFY — stock range not confirmed]

Round Bar

16–300 mm. Diameter, normalised. [VERIFY — stock range not confirmed]

Stock & delivery

Stock location
Dubai, UAE
In stock
Normalised (+N) [VERIFY — stocked sizes]; quenched & tempered on request.
Delivery UAE
24–48 hours
Delivery GCC
3–5 working days — Saudi Arabia, Kuwait, Qatar, Oman, Bahrain
Export
Europe, India, Africa on request
Quotation
Same-day quotation
Minimum order
No minimum order quantity for standard sizes; cut pieces available

Key standards

EN ISO 683-1

Designations & Equivalents

StandardDesignationNotes
BSEN43ABS 970:1955 designation (EN43 family A–J varies in carbon)
Common Name080M50(BS 970 (withdrawn)) BS 970 Part 1 / Part 3 — legacy
BSCS70 (BS 1449)Strip / sheet designation — aliases only
EN NameC50 / C50E / C50REN ISO 683-1 designations (C50E primary)
EN / Werkstoff1.0540 / 1.1206 / 1.1241(EN Number) C50 / C50E / C50R material numbers
AISI / SAE1050Nearest US grade
Common NameDIN Ck50 / JIS S50C / AFNOR XC48H1 / IS 50C8(Other) National equivalents
Common NameCf53 (1.1213)(Related variant) Induction-hardening variant — nearest only
EN NameEN 10083-2(EN (superseded)) Superseded by EN ISO 683-1 — aliases only
Common NameNone(AMS / MIL) No AMS or MIL specification applies (carbon steel)
Common NameEN43 steel / 080M50 / medium carbon steel / C50 round barBuyer search terms

Compliance & Certification

StandardStatusNotes
EN 10204 3.1SuitableProvided as standard — chemistry, condition and mechanical properties.
EN 10204 3.2ConditionalAvailable on request with independent third-party inspection — specify at order stage.

Specifications

Mechanical Properties

Values per EN ISO 683-1. Bar length compares conditions within each row.

PropertyNormalised (+N) | EN ISO 683-1
Tensile Strength (UTS)650 MPamin≤ 16 mmEN ISO 683-1 minimum.
Tensile Strength (UTS)610 MPamin16–100 mmMinimum; Re 320 MPa, A 14%.
Tensile Strength (UTS)590 MPamin100–250 mmMinimum; Re 290 MPa, A 14%.
Yield Strength (ReH)355 MPamin≤ 16 mmEN ISO 683-1 minimum.
Elongation13 %min≤ 16 mmEN ISO 683-1 minimum.
Hardness217 HBmaxSoft annealed (+A)EN ISO 683-1 maximum (+A) — for reference.

Physical Properties

PropertyNormalised (+N) | EN ISO 683-1
Densityat 20°C7.85 g/cm³
Modulus of Elasticityat 20°C210 GPa
Thermal Conductivityat 20°C49 W/m·K
Coefficient of Thermal Expansionat 20–100°C11.1 µm/m·°C
Specific Heat Capacityat 20°C460 J/kg·K

Service Conditions

Service Temperature

Max 300 °C

Notes

General engineering steel for ambient service; Q&T material should not be used above its tempering temperature. No impact requirement in EN ISO 683-1 for C50 [VERIFY].

Corrosion Performance

General corrosion

Rusts in humid and coastal atmospheres — oil, paint or plate finished parts (piston rods are typically hard-chrome plated). Store under cover in the UAE climate.

Pitting resistance

Not applicable — carbon steel.

Additional notes

No corrosion resistance. Surface protection required.

Heat Treatment

HEAT TREATMENT GUIDE — 080M50 / EN43A / C50

Forging / hot rolling: 1100–850°C. Normalising (+N): 830–870°C, air cool. Soft annealing (+A): 680–710°C, slow furnace cool — 217 HB max. Hardening: 800–850°C, quench in oil or water; temper immediately while still hand warm. Tempering: 550–660°C, air cool (+QT: 650–900 MPa by section; for springs, lower tempering after oil hardening). Surface hardening: flame or induction hardening for a hard, wear-resistant surface over a tough core. Flame-cut plate is commonly normalised after cutting to remove the hard edge.

ENGINEERING NOTES
Weldability
Poor

Welding is difficult and generally not recommended for structural joints — the 0.50% carbon content makes the heat-affected zone prone to hardening and cracking. Where unavoidable, preheat to about 200–300°C, use low-hydrogen consumables and stress relieve or temper after welding [VERIFY — procedure].

Filler metals
  • E7018 · AWS A5.1 / SMAWLow-hydrogen electrode — with preheat and post-weld treatment
  • ER70S-6 · AWS A5.18 / MIG (GMAW)Carbon-steel wire — with preheat
  • E312-16 · AWS A5.4 / SMAWAustenitic electrode for repairs / dissimilar joints
Machinability
Fair

Machines best in the soft-annealed (217 HB max) or normalised condition. Slightly lower machinability than EN8; use carbide tooling for Q&T material.

Frequently Asked Questions

Quick answers on our grades, certification, supply and lead times.

Still have questions?

Our team responds fast with specifications, certification and stock availability.

Contact our team

080M50 / EN43A is used for shafts and axles, gears, sprockets and cams, hydraulic piston rods, crankshafts, couplings, spindles, rollers, high-strength bolts, springs and wear parts — often flame or induction hardened. In the UAE and GCC it is common for machined replacement parts and piston rods.

Get in touch

Elevateyourprojectswithoursuperiorsteel