Carbon Steel dealers in UAE

EN9 / 070M55 / C55 Medium Carbon Steel | Supplier in UAE & GCC

EN9 / 070M55 / C55 — 0.55% carbon steel: higher strength and wear resistance than EN8, flame or induction hardenable; gears, sprockets, shafts, cams.

Industries Served

Manufacturing
Automotive
Heavy Engineering
Construction

Overview

EN9 carbon steel (BS 970 070M55; EN ISO 683-1 C55E / 1.1203; DIN C55 / Ck55; AISI 1055; JIS S55C) is a medium-to-high carbon non-alloy steel containing 0.52–0.60% carbon (0.50–0.60% to BS 970) and 0.60–0.90% manganese, with residual chromium, molybdenum and nickel held to low limits. Its higher carbon content gives greater strength, hardness and wear resistance than EN8 / 080M40, at the cost of lower ductility and weldability. It is normally supplied normalised — 680 MPa minimum tensile and 370 MPa yield up to 16 mm, falling to 620 / 300 MPa at 100–250 mm under EN ISO 683-1 — and can be quenched and tempered to 700–950 MPa depending on section. Because of its limited hardenability, through-hardening is restricted to smaller sections, but it responds very well to flame and induction hardening, giving a hard, wear-resistant surface over a tough core. Soft-annealed material (229 HB maximum) machines readily. As a carbon steel it has no corrosion resistance and needs surface protection. Typical uses are gears, sprockets and pinions, cams, shafts and axles, crankshafts, spindles, rollers, machine knives, shear blades, hand tools and wear parts.

Nifty Alloys supplies EN9 / 070M55 / C55 carbon steel from Dubai, UAE, in round bar and flat bar, normalised as standard and quenched and tempered on request. Every supply carries an EN 10204 3.1 Mill Test Certificate as standard; EN 10204 3.2 third-party inspection is available on request. We deliver across the UAE within 24–48 hours, to Saudi Arabia, Kuwait, Qatar, Oman and Bahrain within 3–5 working days, and export to Europe, India and Africa. Send your size list to request a quote — quotations are turned around the same day.

Chemical Composition

0.56 %
C

Carbon

0.52 – 0.6 %

0.25 %
Si

Silicon

≤ 0.4 %

0.75 %
Mn

Manganese

0.6 – 0.9 %

P

Phosphorus

≤ 0.03 %

S

Sulfur

≤ 0.035 %

Cr

Chromium

≤ 0.4 %

Mo

Molybdenum

≤ 0.1 %

Ni

Nickel

≤ 0.4 %

Typical value Range (min–max) Minimum (≥) Maximum (≤) Hover / tap for notes

Standard

EN ISO 683-1

Other

Revision: EN ISO 683-1:2018

Available Forms

Flat Bar

10–100 mm. Thickness; width to order. [VERIFY — stock range not confirmed]

Round Bar

16–300 mm. Diameter, normalised. [VERIFY — stock range not confirmed]

Stock & delivery

Stock location
Dubai, UAE
In stock
Normalised (+N) [VERIFY — stocked sizes]; quenched & tempered (+QT) on request.
Delivery UAE
24–48 hours
Delivery GCC
3–5 working days — Saudi Arabia, Kuwait, Qatar, Oman, Bahrain
Export
Europe, India, Africa on request
Quotation
Same-day quotation
Minimum order
No minimum order quantity for standard sizes; cut pieces available

Key standards

EN ISO 683-1

Designations & Equivalents

StandardDesignationNotes
BSEN9 / EN9KBS 970:1955 designation
Common Name070M55(BS 970 (withdrawn)) BS 970 Part 1 / Part 3 — legacy
EN NameC55 / C55E / C55REN ISO 683-1 designations (C55E primary)
EN / Werkstoff1.0535 / 1.1203 / 1.1209(EN Number) C55 / C55E / C55R material numbers
AISI / SAE1055Nearest US grade
JISS55CJapanese Industrial Standard
DINCk55Former German designation
EN NameEN 10083-2(EN (superseded)) Superseded by EN ISO 683-1 — aliases only
Common NameNone(AMS / MIL) No AMS or MIL specification applies (carbon steel)
Common NameEN9 steel / 070M55 / medium carbon steel / C55 round barBuyer search terms

Compliance & Certification

StandardStatusNotes
EN 10204 3.1SuitableProvided as standard — chemistry, condition and mechanical properties.

Specifications

Mechanical Properties

Values per EN ISO 683-1. Bar length compares conditions within each row.

PropertyNormalised (+N) | EN ISO 683-1Quenched & Tempered (+QT) | EN ISO 683-1
Tensile Strength (UTS)680 MPamin≤ 16 mmEN ISO 683-1 minimum.800–950 MPa≤ 16 mmEN ISO 683-1 range.
Tensile Strength (UTS)640 MPamin16–100 mmMinimum; Re 330 MPa, A 12%.750–900 MPa16–40 mmRange; Re 490 MPa, A 14%.
Tensile Strength (UTS)620 MPamin100–250 mmMinimum; Re 300 MPa, A 12%.700–850 MPa40–100 mmRange; Re 420 MPa, A 15%.
Yield Strength (ReH)370 MPamin≤ 16 mmEN ISO 683-1 minimum.550 MPamin≤ 16 mmEN ISO 683-1 minimum.
Elongation11 %min≤ 16 mmEN ISO 683-1 minimum.12 %min≤ 16 mmEN ISO 683-1 minimum.
Hardness229 HBmaxSoft annealed (+A)EN ISO 683-1 maximum (+A) — for reference.–

Physical Properties

PropertyNormalised (+N) | EN ISO 683-1Quenched & Tempered (+QT) | EN ISO 683-1
Densityat 20°C7.85 g/cm³7.85 g/cm³
Modulus of Elasticityat 20°C210 GPa210 GPa
Thermal Conductivityat 20°C48 W/m·K48 W/m·K
Coefficient of Thermal Expansionat 20–100°C11 µm/m·°C11 µm/m·°C
Specific Heat Capacityat 20°C460 J/kg·K460 J/kg·K

Service Conditions

Service Temperature

Max 300 °C

Notes

General engineering steel for ambient service; Q&T material should not be used above its tempering temperature. Limited low-temperature toughness — no impact requirement in EN ISO 683-1 for C55 [VERIFY].

Corrosion Performance

General corrosion

Rusts in humid and coastal atmospheres — oil, paint or plate finished parts. Store under cover in the UAE climate.

Pitting resistance

Not applicable — carbon steel.

Additional notes

No corrosion resistance. Surface protection required.

Heat Treatment

HEAT TREATMENT GUIDE — EN9 / 070M55 / C55

Forging: heat to 1100°C max; do not forge below 850°C; cool slowly. Normalising (+N): about 790–820°C (some sources 820–860°C), air cool. Soft annealing (+A): 680–710°C, 2–4 h, slow furnace cool (about 15°C/h to 600°C) — 229 HB max. Hardening: 790–820°C, quench in oil or water; temper immediately. Tempering: 550–660°C, air cool (+QT). Surface hardening: flame or induction hardening gives high surface hardness with a tough core. Flame-cut plate is commonly normalised after cutting to remove the hard edge.

ENGINEERING NOTES
Weldability
Poor

Welding is difficult and generally not recommended for structural joints — the 0.55% carbon content makes the heat-affected zone prone to hardening and cracking. Where unavoidable, preheat to about 250–300°C, use low-hydrogen consumables, maintain interpass temperature and stress relieve or temper after welding [VERIFY — procedure].

Filler metals
  • E7018 · AWS A5.1 / SMAWLow-hydrogen electrode — with preheat and post-weld treatment
  • ER70S-6 · AWS A5.18 / MIG (GMAW)Carbon-steel wire — with preheat
  • E312-16 · AWS A5.4 / SMAWAustenitic electrode for repairs / dissimilar joints with reduced preheat
Machinability
Fair

Machines best in the soft-annealed (229 HB max) or normalised condition. Lower machinability than EN8 because of higher carbon and hardness; use carbide tooling for Q&T material.

Frequently Asked Questions

Quick answers on our grades, certification, supply and lead times.

Still have questions?

Our team responds fast with specifications, certification and stock availability.

Contact our team

EN9 / 070M55 is used for gears, sprockets and pinions, cams, shafts and axles, crankshafts, spindles, rollers, machine knives, shear blades, hand tools and wear parts — especially where flame or induction hardening is used to create a hard, wear-resistant surface. In the UAE and GCC it is common for machined replacement parts.

Get in touch